Journals / Hittite Journal of Science and Engineering / 2026 / Volume: 12 Issue: 2

Performance Analysis of Environmental Conditioning Effect on Crush Character of Hybrid Composite Pipes with Different Winding Angles

Pages
—
Publication Date
2025-06-30
🏛️Bibliographic metadata and full text access for this article are provided via DergiPark.
DergiPark Record ↗
✨

AI Summary & Key Takeaways

AI Insight
⚡ TL;DR(Too Long; Didn't Read)

Notably, hybrid pipes with 55° winding angles exhibited superior energy absorption (30.44 J/g for U55), emphasizing the role of fiber orientation in load distribution.

📌 3 Key Takeaways

🎯
Objective & Hypothesis:The effects of hydrothermal aging in distilled water (DW) and seawater (SW) environments on the water absorption behavior and crush characteristics of hybrid glass/carbon fiber-reinforced composite pipes with ±55° and ±70° winding angles were evaluated.
📊
Key Findings & Data:Specimens were kept for 120 days at 30°C, and water absorption was analyzed experimentally and theoretically.
💡
Conclusion & Impact:Notably, hybrid pipes with 55° winding angles exhibited superior energy absorption (30.44 J/g for U55), emphasizing the role of fiber orientation in load distribution.
🔬Design:Research Article
📍Scope:Comprehensive Sample
⚙️Variables:Hybrid composites · hydrothermal aging · winding angle

Abstract

The effects of hydrothermal aging in distilled water (DW) and seawater (SW) environments on the water absorption behavior and crush characteristics of hybrid glass/carbon fiber-reinforced composite pipes with ±55° and ±70° winding angles were evaluated. Specimens were kept for 120 days at 30°C, and water absorption was analyzed experimentally and theoretically. Results revealed that distilled water-aged samples exhibited higher maximum water absorption rates (2.5% for DW55 and 2.62% for DW70) compared to seawater-aged samples (2.37% for SW55 and 2.44% for SW70), attributed to the inhibitory role of ionic components in seawater. Lower winding angles consistently showed greater water absorption due to increased microstructural voids, facilitating water diffusion. Quasi-static axial compression tests demonstrated significant degradation in crush performance after aging. Unconditioned samples with 70° winding angles achieved the highest initial peak load (56.9 kN) and specific energy absorption (28.89 J/g). However, aging reduced these values, with seawater-aged samples (SW55) showing a 12.32% decrease in specific energy absorption compared to unconditioned counterparts. Crushing force efficiency (CFE) also declined, correlating with matrix plasticization and fiber/matrix interface weakening. Notably, hybrid pipes with 55° winding angles exhibited superior energy absorption (30.44 J/g for U55), emphasizing the role of fiber orientation in load distribution.

🔖

Cite This Article

Özbek, Ö., Oğuz, Z. A., Erkliğ, A., Bozkurt, Ö. Y. (2025). Performance Analysis of Environmental Conditioning Effect on Crush Character of Hybrid Composite Pipes with Different Winding Angles. Hittite Journal of Science and Engineering, Volume: 12 Issue: 2. https://doi.org/10.17350/HJSE19030000352

📄 Full Text PDF Viewer

📄

PDF görüntüleyici hazırlanıyor...

References (22)

  1. Kosedag E. Effect of artificial aging on 3-point bending behavior of glass fiber/epoxy composites. J Reinf Plast Compos. 2023; 42(21-22):1147-53.
  2. Demircan G, Kisa M, Ozen M, Acikgoz A, Işıker Y, Aytar E. Nano-gelcoat application of glass fiber reinforced polymer composites for marine application: Structural, mechanical, and thermal analysis. Mar Pollut Bull. 2023; 194:115412.
  3. Kosedag E, Caliskan U, Ekici R. The effect of artificial aging on the impact behavior of SiC nanoparticle-glass fiber-reinforced polymer matrix composites. Polym Compos. 2022; 43(2):964-76.
  4. Doğan NF, Oğuz ZA, Erkliğ A. An experimental study on the hydrothermal aging effect on the free vibration properties of hybrid aramid/glass/epoxy composites: Comparison of sea water and distilled water. Polym Compos. 2023; 44(10):6902-12.
  5. Zuo W, Luo Q, Li Q, Sun G. Effect of thermal and hydrothermal aging on the crashworthiness of carbon fiber reinforced plastic composite tubes. Compos Struct. 2023; 303:116136.
  6. Krishnan P, Majid MA, Afendi M, Yaacob S, Gibson AG. Effects of hydrothermal ageing on the behaviour of composite tubes under multiaxial stress ratios. Compos Struct. 2016; 148:1-11.
  7. Fitriah SN, Majid MA, Ridzuan MJM, Daud R, Gibson AG, Assaleh TA. Influence of hydrothermal ageing on the compressive behaviour of glass fibre/epoxy composite pipes. Compos Struct. 2017; 159:350-60.
  8. Sepetcioglu H, Gunoz A, Kara M. Effect of hydrothermal ageing on the mechanical behaviour of graphene nanoplatelets reinforced basalt fibre epoxy composite pipes. Polym Polym Compos. 2021;29(9_suppl): S166-77.
  9. Kara M, Ak S, Uyaner M, Gunoz A, Kepir Y. The effect of hydrothermal aging on the low-velocity impact behavior of multi-walled carbon nanotubes reinforced carbon fiber/epoxy composite pipes. Appl Compos Mater. 2021; 28:1567-87.
  10. Oğuz ZA, Özbek Ö, Erkliğ A, Bozkurt ÖY. Hydrothermal aging effect on crushing characteristics of intraply hybrid composite pipes. Eng Struct. 2023; 297:117011.
  11. Özbek Ö, Oğuz ZA, Bozkurt ÖY, Erkliğ A. Crashworthiness characteristics of hydrothermally aged intraply glass/basalt composite pipes. Mar Struct. 2024; 97:103656.
  12. Oguz ZA, Erklig A, Bozkurt ÖY. Degradation of hybrid aramid/glass/epoxy composites hydrothermally aged in distilled water. J Compos Mater. 2021;55(15):2043-60.
  13. Oğuz ZA, Erkliğ A, Bozkurt ÖY. Effects of hydrothermal seawater aging on the mechanical properties and water absorption of glass/aramid/epoxy hybrid composites. Int Polym Process. 2021; 36(1):79-93.
  14. Quaresimin M, Ricotta M, Martello L, Mian S. Energy absorption in composite laminates under impact loading. Compos Part B Eng. 2013; 44(1):133-40.
  15. Fitriah SN, Majid MA, Ridzuan MJM, Daud R, Gibson AG, Assaleh TA. Influence of hydrothermal ageing on the compressive behaviour of glass fibre/epoxy composite pipes. Compos Struct. 2017; 159:350-60.
  16. Sebaey TA. Crashworthiness of GFRP composite tubes after aggressive environmental aging in seawater and soil. Compos Struct. 2022; 284:115105.
  17. Özbek Ö, Bozkurt ÖY, Erkliğ A. An experimental study on intraply fiber hybridization of filament wound composite pipes subjected to quasi-static compression loading. Polym Test. 2019; 79:106082.
  18. Miki M, Murotsu Y, Tanaka T. Optimum fiber angle of unidirectional composites for load with variations. AIAA J. 1992; 30(1):189-96.
  19. Wang HW, Zhou HW, Gui LL, Ji HW, Zhang XC. Analysis of effect of fiber orientation on Young’s modulus for unidirectional fiber reinforced composites. Compos Part B Eng. 2014; 56:733-9.
  20. Özbek Ö, Oğuz ZA. Crushing behaviors of intraply carbon/basalt hybrid composite pipes under seawater and distilled water aging environments. In: International Scientific Research and Innovation Congress -II; 2024. p. 2509-23.
  21. https://www.dostkimya.com/tr/urunler/epoksi-sistemler//mgs-laminasyon-epoksi-recine-l160 (Date of visit: 08.04.2025)
  22. Özbek, Ö., Bozkurt, Ö. Y., & Erkliğ, A. (2022). Development of a trigger mechanism with circular cut-outs to improve crashworthiness characteristics of glass fiber-reinforced composite pipes. Journal of the Brazilian Society of Mechanical Sciences and Engineering, 44, 1-14.