Fiber addition significantly affected biodegradation in a complicated way: by decelerating mass loss but accelerating deterioration of mechanical properties.

📌 3 Maddede Bu Makale

🎯
Amaç & Hipotez:This paper focuses on preparation of poly(vinyl alcohol) (PVA)-based composites reinforced with okra bast fibers at different percentages of 5, 10, 20% via solution casting method.
📊
Temel Bulgular & Veri:Fibers obtained from different sections of okra plants were biologically degummed and scoured with Na2CO3.
💡
Sonuç & Katkı:Fiber addition significantly affected biodegradation in a complicated way: by decelerating mass loss but accelerating deterioration of mechanical properties.
🔬Tür:Araştırma Makalesi
📍Kapsam:Genişletilmiş Akademik Örneklem
⚙️Değişkenler:Agroresidue · agrowaste · biodegradation

Abstract

This paper focuses on preparation of poly(vinyl alcohol) (PVA)-based composites reinforced with okra bast fibers at different percentages of 5, 10, 20% via solution casting method. Fibers obtained from different sections of okra plants were biologically degummed and scoured with Na2CO3. Selected fibers were bleached, treated with maleic anhydride or grafted with vinyl acetate. Mechanical, physical and biodegradational properties of the composites were investigated. The tensile strength of the produced composites ranges between 33.8 and 55.1 MPa, elasticity modulus from 1.8 to 2.6 GPa, elongation rate at break varies in 2.8-10%. Chemical treatments led to improved mechanical performance whereas increased fiber content reduces tensile strength, stiffness and elongation, as well as water absorption. Fiber addition significantly affected biodegradation in a complicated way: by decelerating mass loss but accelerating deterioration of mechanical properties.

🔖

Bu Makaleye Atıf Yap

KHAN, G. M. A., YİLMAZ, N. D. (2022). Biologically Degummed and Chemically Treated Okra Bast Fibers-Reinforced Poly(Vinyl Alcohol) Composites. Textile and Apparel, Cilt: 32 Sayı: 4, 366–375. https://ajindex.com/articles/943413

📄 Tam Metin PDF Okuyucu

📄

PDF görüntüleyici hazırlanıyor...

Kaynakça (4)

  1. N. Jain, V. K. Singh, and S. Chauhan, “A review on mechanical and water absorption properties of polyvinyl alcohol based composites/films,” J. Mech. Behav. Mater., vol. 26, no. 5–6, pp. 213–222, 2017, doi: 10.1515/jmbm-2017-0027. C. M. Hassan and N. A. Peppas, “Structure and Applications of Poly(vinyl alcohol) Hydrogels Produced by Conventional Crosslinking or by Freezing/Thawing Methods,” Biopolym. · PVA Hydrogels, Anionic Polym. Nanocomposites, vol. 153, pp. 37–65, 2000, doi: 10.1007/3-540-46414-X_2. F. Cengi̇z Çallioğlu, “The effect of glyoxal cross-linker and NaCl salt addition on the roller electrospinning of poly(vinyl) nanofibers,” Tekst. ve Konfeksiyon, vol. 24, no. 1, pp. 15–20, 2014.
  2. L. Wang, G. Periyasami, A. Aldalbahi, and V. Fogliano, “The antimicrobial activity of silver nanoparticles biocomposite films depends on the silver ions release behaviour,” Food Chem., vol. 359, p. 129859, 2021, doi: https://doi.org/10.1016/j.foodchem.2021.129859. S. Xu et al., “Properties of Polyvinyl Alcohol Films Composited With Hemicellulose and Nanocellulose Extracted From Artemisia selengensis Straw,” Front. Bioeng. Biotechnol., vol. 8, no. August, pp. 1–11, 2020, doi: 10.3389/fbioe.2020.00980. G. M. A. Khan, N. D. Yilmaz, and K. Yilmaz, “Effects of Alkalization on Physical and Mechanical Properties of Biologically Degummed Okra Bast and Corn Husk Fibers,” J. Nat. Fibers, 2020, doi: 10.1080/15440478.2020.1798840. S. Biswas, Q. Ahsan, A. Cenna, M. Hasan, and A. Hassan, “Physical and mechanical properties of jute, bamboo and coir natural fiber,” Fibers Polym., vol. 14, no. 10, pp. 1762–1767, 2013, doi: 10.1007/s12221-013-1762-3.
  3. G. M. A. Khan, M. S. Alam Shams, M. R. Kabir, M. A. Gafur, M. Terano, and M. S. Alam, “Influence of chemical treatment on the properties of banana stem fiber and banana stem fiber/coir hybrid fiber reinforced maleic anhydride grafted polypropylene/low-density polyethylene composites,” J. Appl. Polym. Sci., vol. 128, pp. 1020–1029, 2013, doi: 10.1002/app.38197. G. M. A. Khan, N. D. Yilmaz, and K. Yilmaz, “Effects of chemical treatments and degumming methods on physical and mechanical properties of okra bast and corn husk fibers,” J. Text. Inst., vol. 111, no. 10, pp. 1418–1435, 2020, doi: 10.1080/00405000.2019.1702492. L. Li, G. Sheng, and Q. Wang, “Parameters optimization for degumming of cotton-straw bast fiber,” Tekst. ve Konfeksiyon, vol. 25, no. 2, pp. 135–139, 2015.
  4. M. S. Alam, G. M. A. Khan, and S. M. A. Razzaque, “Estimation of Mai