Dergiler / Türkiye Ormancılık Dergisi / 2021 / Cilt: 22 Sayı: 1

Farklı mol oranlarıyla sentezlenen üre reçinelerinin yüksek yoğunlukta lif levhaların (HDF) fiziksel özelliklerine ve formaldehit emisyonuna etkisi

The effect of urea resins synthesized with different mole ratios on physical properties of high density fiberboards (HDF) and formaldehyde emission

Sayfa
49–55
Yayın Tarihi
2021-03-26
DOI
—
🏛️Bu makalenin bibliyografik verileri ve tam metin bağlantısı DergiPark üzerinden sağlanmıştır.
DergiPark Kaydı ↗
✨

Yapay Zeka Hızlı Bakış & Çıkarımlar

AI Insight
⚡ TL;DR(1 Cümlede Hızlı Çıkarım)

Çalışmanın sonucunda (R;1.17, X;0.98 ve Y;0.88) mol üre formaldehit kullanarak üretilen HDF levhalarına hem fiziksel test sonuçları hemde formaldehit gaz emisyonu sonuçlarına göre farklılıklar ortaya konulmuştur.

📌 3 Maddede Bu Makale

🎯
Amaç & Hipotez:Yaşam alanlarının vazgeçilmez ürünü yüksek yoğunlukta lif levha (HDF) bazlı ve türevi ürünlerin (laminant parke türevleri vb.) hammaddesi HDF levhalarıdır.
📊
Temel Bulgular & Veri:HDF levhalarının fiziksel test değerleri ilgili standart değerlerde ve formaldehit emisyonun E1 veya E0 olması hedeflenmiştir.
💡
Sonuç & Katkı:Çalışmanın sonucunda (R;1.17, X;0.98 ve Y;0.88) mol üre formaldehit kullanarak üretilen HDF levhalarına hem fiziksel test sonuçları hemde formaldehit gaz emisyonu sonuçlarına göre farklılıklar ortaya konulmuştur.
🔬Tür:Araştırma Makalesi
📍Kapsam:Genişletilmiş Akademik Örneklem
⚙️Değişkenler:HDF · Fiziksel özellikler · Üre formaldehit

Özet

Yaşam alanlarının vazgeçilmez ürünü yüksek yoğunlukta lif levha (HDF) bazlı ve türevi ürünlerin (laminant parke türevleri vb.) hammaddesi HDF levhalarıdır. HDF levhalarının fiziksel test değerleri ilgili standart değerlerde ve formaldehit emisyonun E1 veya E0 olması hedeflenmiştir. Bu çalışmada, yüksek yoğunlukta lif levha üretim hattında %50 sarıçam (Pinus sylvestres L.), %30 göknar (Abies nordmanniana L.), %20 kayın (Fagus orientalis L.). Üretim hattında üç farklı mol üre-formaldehit reçinesi (R; 1.17, X; 0.98 ve Y; 0.88) kullanılarak 7.7mmx2100mmx2440mm HDF levhalar üretildi. Proseste üretim parametreleri sabit kalmıştır. Tek değişken üç farklı mol oranlarında kullanılan üre formaldehit tutkalı olmuştur. Sıcak pres parametrelerinden pres hızını 950 mm/sn ve pres sıcaklığını 215ºC ve 60 saniye presleme süresi parametrelerinde üretim gerçekleşmiştir. Üretilen R, X, Y HDF levhaların; fiziksel testlerine (kalınlığına, yoğunluğu, levha rutubetine, 24 saat suda kalınlığına şişme ve 24 saat su alma) ve formaldehit gaz emisyonuna bakılmıştır. Her bir test grubundan beş levha ölçülmüştür. HDF levhalarının fiziksel özellikleri, özgül ağırlığı R;874 kg/m³, X;881 kg/m³ ve Y;860 kg/m³, kalınlığına suda şişmesi 24 saat R; %17.79, X; %19.65 ve Y; %19.08, 24 saat su alma R; %19.65, X; %19.09 VE Y; %22.42 ölçülmüştür. Formaldehit gaz emisyon değerleri R; 14.96, mg/100g. X; 8.28 mg/100g ve Y; 6.79 mg/100g analiz edilmiştir. Çalışmanın sonucunda (R;1.17, X;0.98 ve Y;0.88) mol üre formaldehit kullanarak üretilen HDF levhalarına hem fiziksel test sonuçları hemde formaldehit gaz emisyonu sonuçlarına göre farklılıklar ortaya konulmuştur.

Abstract

The indispensable product of living spaces, the raw material of high density fiberboard (HDF) based derivative products (laminate flooring derivatives, etc.) are HDF boards. The test values (physical and formaldehyde emission properties ) of HDF boards are targeted both physical properties and formaldehyde emission E1 or E0 standard. In this study, 50% yellow pine (Pinus sylvestres L), 30% fir (Abies nordmanniana L), 20% beech (Fagus orientalis L) were used biomass. HDF boards of 7.7mmx2100mmx2440mm were produced on the production line which using three different moles of urea-formaldehyde resins (R; 1.17, X; 0.98 and Y; 0.88). Production parameters remained constant in the HDF line process and the only variable were urea formaldehyde resins used in three different molar ratios. The productions were manufactured in pressing speed of 950 mm/second and pressing temperature 215ºC and 60 seconds pressing time in the continue hot press. R, X, Y HDF boards produced; physical tests (thickness, density, board moisture, 24 hours Thickness-swelling and 24 hours water absorption) and formaldehyde gas emissions were analysed which was five boards were measured from each test group. Physical properties of HDF boards were measured which was the density of boards (R; 874 kg/m³, X; 881 kg/m³ and Y; 860 kg/m³) Thickness swelling of boards at 24 hours (R; 17.79%, X; 19.65% and Y; 19.08%) water absorption of boards at 24 hours (R; 19.65%, X; 19.09% and Y; 22.42%). Formaldehyde gas emission result of HDF boards were analysed (R; 14.96, mg/100g. X; 8.28 mg/100g and Y; 6.79 mg/100g). As a result of the study, differences were determined according to both physical test results and formaldehyde gas emission results for HDF boards produced.

🔖

Bu Makaleye Atıf Yap

ÇAMLIBEL, O. (2021). Farklı mol oranlarıyla sentezlenen üre reçinelerinin yüksek yoğunlukta lif levhaların (HDF) fiziksel özelliklerine ve formaldehit emisyonuna etkisi. Türkiye Ormancılık Dergisi, Cilt: 22 Sayı: 1, 49–55. https://ajindex.com/articles/914428

📄 Tam Metin PDF Okuyucu

📄

PDF görüntüleyici hazırlanıyor...

Kaynakça (6)

  1. Alpar, T., Faczan, T., Racz, I., Katoli, G., 2010. MDF/HDF production from plantation wood species. Drvna Industrıja, 61(3): 183-191.
  2. Angelatos, A.S., 2004. NMR structural elucidation of amino resins. Journal of Applied Polymer Science, 91(6): 3504–3512. DOI:10.1002/app.13538. ASTM D 6007–02, 2002. Standard test method for determining formaldehyde concentration in air from wood products using a small–scale chamber. ASTM Standarts, USA. Boran, S., Usta, M., 2010. Odun esaslı panellerde açığa çıkan formaldehit ve formaldehit sınırları hakkında bilgiler. III. Ulusal Karadeniz Ormancılık Kongresi, 20-22
  3. Mayıs, Artvin, s. 1968-1975.
  4. Boran, S., Usta, M., Gümüşkaya, E., 2011. Decreasing formaldehyde emission from medium density fiberboard panels produced by adding different amine compounds to urea formaldehyde resin. International Journal of Adhesion&Adhesive, 31: 674-678. CARB, 2007. Proposed Airborne Toxic Control Measure (ATCM) to reduce formaldehyde emission from composite wood products. http://www.arb.ca.gov/sites/default/files/classic //toxics/compwood/consumer_faq.pdf. Accesed: 30.09.2020.
  5. Costa, N., Pereira, J., Ferra, J., Cruz, P., Martins, J., Magalhaes, F., Mendes, A., Carvalho, L., 2013. Soduium metabisülfite as scavenger of air pollutions in wood based building materials. International Wood Products Journal, 4(4): 242-247. doi:10.1179/2042645313Y.0000000037. Dazmiri, M,K., Kiamahalleh, M,V., Dorieh, A., Pizzi, A., 2019. Effect of the initial F/U molar ratio in urea-formaldehyde resins synthesis and its ınfluence on the performance of medium density fiberboard bonded with them. International Journal of Adhesion and Adhesives, 95: 102440. DOI: 10.1016/j.ijadhadh. Despres, A., Pizzi, A., Vu, C., Delmotte, L., 2010. Colourless formaldehyde-free urea resin adhesives for wood panels. Eurepean Journal Wood Product, 68(1): 13–20. EN 717–1, 2004. Wood based panels–determination of formaldehyde release–Part 1: formaldehyde emission by the chamber method. European Standard. EN 717–2, 1994. Wood based panels–determination of formaldehyde release–Part 2: formaldehyde release by the gas analysis method. European Standard. Eroğlu, H., Usta, M., 2000. Lif Levha Üretim Teknolojisi. Karadeniz Teknik Üniversitesi, Orman Fakültesi, Genel Yayın No: 200, Fakülte Yayın No: 30, Trabzon. Faostat, 2020. Forestry production and trade. Food and Agriculture Organization of the United, Nations, http://www.fao.org/ faostat/en/#data/FO, Accessed: 24.01.2020.
  6. Grigsby, W., Mc