Dergiler / International Journal of Chemistry and Technology / 2017 / Cilt: 1 - Sayı: 1

Investigation of leaching conditions of chalcopyrite by chlorine gas in aqueous medium

Sayfa
67–73
Yayın Tarihi
2017-12-15
DOI
—
🏛️Bu makalenin bibliyografik verileri ve tam metin bağlantısı DergiPark üzerinden sağlanmıştır.
DergiPark Kaydı ↗
✨

Yapay Zeka Hızlı Bakış & Çıkarımlar

AI Insight
⚡ TL;DR(1 Cümlede Hızlı Çıkarım)

Under these conditions, 68.44% of copper in chalcopyrite dissolved.

📌 3 Maddede Bu Makale

🎯
Amaç & Hipotez:Generally, copper is obtained by pyrometallurgical methods from sulphide ores and SO2, a dangerous gas is emitted to environment.
📊
Temel Bulgular & Veri:Thus, both Cl2, a by-product of chlor-alkali industry, is removed using as a reagent, and emission of SO2 from copper sulphide prometallurgy is prevented.
💡
Sonuç & Katkı:Under these conditions, 68.44% of copper in chalcopyrite dissolved.
🔬Tür:Araştırma Makalesi
📍Kapsam:Genişletilmiş Akademik Örneklem
⚙️Değişkenler:Chalcopyrite · optimization · Taguchi method

Abstract

Generally, copper is obtained by pyrometallurgical methods from sulphide ores and SO2, a dangerous gas is emitted to environment. Hydrometallurgical processes is preferred over pyrometallurgical processes in recent years. The present work aims to optimize leaching of chalcopyrite with chlorine gas in aqueous medium by an experimental design using Taguchi method. Thus, both Cl2, a by-product of chlor-alkali industry, is removed using as a reagent, and emission of SO2 from copper sulphide prometallurgy is prevented. In this study, experimental parameters and their values were 16-45°C for reaction temperature, 0.05-0.20 g ml-1 for solid-to-liquid ratio, 30-120 min for reaction time, 0.027-0.4 mol l-1 for [Fe3+] and 0.025-0.4 mol l-1 for [Cu2+ ]. The optimum conditions were 45°C for reaction temperature, 0.05 g ml-1 for solid-to-liquid ratio, 0.2 mol l-1 for [Fe3+], 0.025 mol l-1 for [Cu2+ ] and 120 min for reaction time. Under these conditions, 68.44% of copper in chalcopyrite dissolved.

🔖

Bu Makaleye Atıf Yap

TEMUR, H., YARTAŞI, A., KOCAKERİM, M. M. (2017). Investigation of leaching conditions of chalcopyrite by chlorine gas in aqueous medium. International Journal of Chemistry and Technology, Cilt: 1 - Sayı: 1, 67–73. https://ajindex.com/articles/765731

📄 Tam Metin PDF Okuyucu

📄

PDF görüntüleyici hazırlanıyor...

Kaynakça (29)

  1. Çolak, S.; Alkan, M.; Kocakerim, M.M. Hydrometallurgy 1987, 18, 183-193
  2. Mukherjee, T.K.; Gupta, C.K. Miner. Process. Technol. Rev. 1, 1983, 111-153
  3. Bayrakçeken, S.; Yaşar, Y.; Çolak, C. Hydrometallurgy 1990, 25, 27-36
  4. Groves, R.D.; Smith, P.B. Reactions of copper sulp-hide minerals with chlorine in an aqueous system. Bureau of Mines, Report of Investigation, 7801, 1973
  5. Flett, D.S. Chloride Hydrometallurgy for Complex Sulphides: a Review, Chloride Hydrometallurgy, International Conference on the Practice and Theory of Chloride/Metal Interaction, Montreal, Quebec, Canada, October 19-23, 2002
  6. Lu, Z.Y.; Jeffrey, M.I.; Lawson, F. Hydrometallurgy 2000, 56(2), 189-202
  7. Bonan, M.; Demarthe, J.M.; Renon, H.; Baratin, F. Metall. Trans. B, 1981, 12B, 269-274
  8. Wilson, J.P.; Fisher, W.W. J. Met, 1981 33(2), 52-57
  9. Scrobian, M.; Havlik, T.; Ukasik, M. Hydrometallurgy 2005, 77, 109-114
  10. Lundström,M.; Aromaa, J.; Forsén, O.; Hyvarinen, O.; Barker, M.H. Hydrometallurgy 2005, 77, 89-95
  11. Havlik, T.; Skrobian, M.; Balaz, P.; Kammel, R. Int. J. Miner. Process 1995, 43, 61-72
  12. Dutrizac, J.E. Hydrometallurgy 1990, 23, 153-176
  13. Habashi, F.; Toor, T. Metall. Trans. B. 1979, 10B, 49-56
  14. Puvvada, G.V.K.; Murthy, D.S.R. Hydrometallurgy 2000, 58, 185-191
  15. Maurice, D.; Hawk, J.A. Hydrometallurgy 1999, 51, 371-377
  16. Saraç, H.; Kocakerim, M.M.; Çolak, S. Chim. Acta Turcica 1994, 22 (3), 259-370
  17. Padilla, R.; Zambrano, P.; Ruiz, M.C., Metall. Mater. Trans. B, 2002, 34B, 153-159
  18. Abalı, Y.; Çolak, S.; Yapici, S. Hydrometallurgy 1997, 46, 27
  19. Ata, O.N.; Çolak, S.; Çopur, M.; Çelik, C. Ind. Eng. Chem. Res. 2000, 39, 488-493
  20. Ata, O. N.; Çolak, S.; Ekinci, Z.; Çopur, M. Chem. Eng. Technol. 2001, 24, 409
  21. Beşe, A.V.; Ata, O.N.; Çelik, C.; Çolak, S. Chem. Eng. Process. 2003, 42, 291-298
  22. Çopur, M.; Pekdemir, T.; Çelik, C.; Çolak, S. Ind. Eng. Chem. Res. 1997, 36, 682
  23. Çopur, M. Chem. Biochem. Eng. Q. 2002, 15(4), 191-197
  24. Dönmez, B.; Çelik, Ç.; Çolak, S.; Yartaşı, A. Ind. Eng. Chem. Res. 1998, 37, 3382-3387
  25. Dönmez, B.; Ekinci, Z.; Çelik, C.; Çolak, S. Hydrometallurgy 1999, 52, 81-90
  26. Antonijevic, M.M.; Bogdanovic, G.D. Hydrometallurgy 2004, 73, 245-256
  27. Aydoğan, S.; Uçar, G.; Cambazoğlu, G., Hydrometallurgy 2006, 81, 45-51
  28. Cordoba, E.M., Munoz, J.A., Blazquez, M.L., Gonzales, F., Ballester, A., Miner. Eng. 2009, 22, 229-235
  29. Li, Y., Qian, G., Li, J., Gerson, A.R., Geochim. Cosmochi