Graft copolymerization of N- vinylimidazole on poly (ethylene terephthalate) fibers in a swelling solvent using azobisiobuthyronitrile as initiator

Sayfa
403–415
Yayın Tarihi
2022-11-05
DOI
—
🏛️Bu makalenin bibliyografik verileri ve tam metin bağlantısı DergiPark üzerinden sağlanmıştır.
DergiPark Kaydı ↗
✨

Yapay Zeka Hızlı Bakış & Çıkarımlar

AI Insight
⚡ TL;DR(1 Cümlede Hızlı Çıkarım)

Grafted fibers were characterized by FTIR spectroscopy and scanning electron microscopy.

📌 3 Maddede Bu Makale

🎯
Amaç & Hipotez:In this study, poly(ethylene terephthalate) (PET) fibers were grafted in dimethylformamide (DMF) with n-vinylimidazole (n-VI) using azobisisobutyronitrile (AIBN) as an initiator.
📊
Temel Bulgular & Veri:Variations of percentage grafting with time, temperature, monomer and initiator concentrations as well as monomer and initiator diffusions were investigated.
💡
Sonuç & Katkı:Grafted fibers were characterized by FTIR spectroscopy and scanning electron microscopy.
🔬Tür:Araştırma Makalesi
📍Kapsam:Genişletilmiş Akademik Örneklem
⚙️Değişkenler:Alan Parametreleri

Abstract

In this study, poly(ethylene terephthalate) (PET) fibers were grafted in dimethylformamide (DMF) with n-vinylimidazole (n-VI) using azobisisobutyronitrile (AIBN) as an initiator. Variations of percentage grafting with time, temperature, monomer and initiator concentrations as well as monomer and initiator diffusions were investigated. It was observed that the percentage of grafting and grafting efficiency increased as time and temperature rose up to a certain value, and then they levelled off. The percentage of grafting was found to rise with increasing monomer and initiator concentrations, and then decrease. Monomer and initiator diffusions into PET fibers were shown to follow a similar trend and increased the percentage of grafting. Optimum conditions for grafting were found to be [n-VI] = 0.5 M, [AIBN] = 1.5 x $10^{-3}$ M, T = 70 °C and t = 3 days. The rate of grafting was found to be proportional to 1.4 and 0.7 powers of monomer and initiator concentrations, respectively. The overall activation energy for grafting was 22.2 kcal/mol. Further changes in the properties of grafted PET fibers such as intrinsic viscosity, water absorption capacity, fiber diameter and elongation percentage were determined. Grafted fibers were characterized by FTIR spectroscopy and scanning electron microscopy.

🔖

Bu Makaleye Atıf Yap

ÜNAL, H. İ., İNEGÖLLÜ, C., ŞANLI, O. (2022). Graft copolymerization of N- vinylimidazole on poly (ethylene terephthalate) fibers in a swelling solvent using azobisiobuthyronitrile as initiator. Turkish Journal of Chemistry, Cilt: 27 - Sayı: 3, 403–415. https://ajindex.com/articles/602258

📄 Tam Metin PDF Okuyucu

📄

PDF görüntüleyici hazırlanıyor...

Kaynakça (32)

  1. Y. Hsieh, C. Pugh and M.S. Ellison, J. Appl. Polym. Sci., 29, 3547 (1984)
  2. I.F. Osipenko and V.I. Martinovich, J. Appl. Polym. Sci., 39, 935 (1990)
  3. A.K. Pradhan, N.C. Pati and P.L. Nayak, J. Appl. Polym. Sci., 27, 1873 (1982)
  4. E.M. Abdel-bary, A.A. Sarhan and H.H. Abdel-Razik, J. Appl. Polym. Sci., 35, 439 (1988)
  5. S.E. Shalaby, A.M. Bayazeed and A. Hebeish, J. Appl. Polym. Sci., 22, 1359 (1978)
  6. S. Lenka, P.L. Nayak, M.K. Mishra and A.K. Tripathy, J. Appl. Polym. Sci., 26, 2773 (1981)
  7. S. Mishra, P.L. Nayak and G. Sahu, J. Appl. Polym Sci., 27, 3867 (1982)
  8. S. Lenka, J. Polym. Sci. Polym. Let. Ed., 21, 281 (1983)
  9. S. Lenka, P.L. Nayak and A.K. Tripathy, J. Macromol. Sci. Pure and Appl. Chem., A18(6), 987 (1982)
  10. A.K. Pradhan, N.C. Pati and P.L. Nayak. J. Appl. Polym. Sci., 27, 2131 (1982)
  11. A. Hebeish, S.E. Shalaby and A.M. Bayazeed, J. Appl. Polym. Sci., 26, 3253 (1981)
  12. M. Sacak and E. Pulat, J. Appl. Polym. Sci., 33, 539 (1989)
  13. R. Anbarasan, T. Vasudevan and A. Gopalan, Eur. Polym. J., 36, 1725 (2000)
  14. P. Dokolas, G.G. Qiao and D.H. Solomon, J. Appl. Polym. Sci., 83, 898 (2002)
  15. E. Uchida, Y. Uyama and Y. Ikada, J. Polym. Sci., A27, 527 (1989)
  16. J. Xue and C.A. Wilkie, J. Appl. Polym. Sci., 33, 1019 (1995)
  17. H.I. Ünal, M. Rostamlou and O. Sanli, J. Macromol. Sci. Pure and Appl. Chem., A35(9), 1541 (1995)
  18. O. Sanli, S. Aytemiz and H.I. Ünal, J. Macromol Sci. Pure and Appl. Chem., A34(6), 1003 (1997)
  19. O. Sanli and E. Pulat, J. Appl. Polym. Sci., 47, 1 (1993)
  20. H.I. Ünal, R. Coskun, O. Sanli and M. Yigitoglu, J. Appl. Polym. Sci., 64, 1437 (1997)
  21. H.I. Ünal and O. Sanli, J. Appl. Polym. Sci., 62, 1161 (1996)
  22. B.B. Dambatta and J.R. Ebdon, Eur. Polym. J., 22, 783 (1986)
  23. C.H. Bamford and E. Schoffeld, Polymer, 22, 1227 (1981)
  24. B.B. Dambatta, J.R. Ebdon and T.N. Huckerby, Eur. Polym. J., 20, 645 (1984)
  25. H.T. Grampel, G. Tuin, Y.Y. Tan and G. Challa, Macromolecules, 25, 1049 (1992)
  26. H.T. Grampel, Y.Y. Tan and G. Challa, Macromolecules, 23, 5209 (1990)
  27. H.T. Grampel, A.G.M. Santing, Y.Y. Tan and G. Challa, J. Polym. Sci., A30, 787 (1992)
  28. H.T. Grampel, Y.Y. Tan and G. Challa, Macromolecules, 25, 1041 (1992)
  29. N. Inagaki, S. Tasaka and M. Masumoto, Macromolecules, 29, 1642 (1996)
  30. N. Inagaki, S. Tasaka and M. Masumoto, J. Appl. Polym. Sci., 56, 135 (1995)
  31. Xu. Zhilli, A. Chapiro and N. Schmitt, Eur. Polym. J., 29, 301 (1993)
  32. H. Kubota, Eur. Polym