Dergiler / Research on Engineering Structures and Materials / 2017 / Cilt: 3 - Sayı: 1

Physico-mechanical and corrosion behavior of acid resistant bricks developed from quarry waste silicate residues using powder metallurgy

Sayfa
55–64
DOI
—
🏛️Bu makalenin bibliyografik verileri ve tam metin bağlantısı DergiPark üzerinden sağlanmıştır.
DergiPark Kaydı ↗
✨

Yapay Zeka Hızlı Bakış & Çıkarımlar

AI Insight
⚡ TL;DR(1 Cümlede Hızlı Çıkarım)

It was observed that most of the developed brick samples showed excellent results in both HCl and H 2 SO 4 media in accordance with IS: 4860-1968 and ESS:41-1986.

📌 3 Maddede Bu Makale

🎯
Amaç & Hipotez:The disposal of industrial wastes comprises one of the major worldwide environmental problems as these wastes render the environment unfriendly.
📊
Temel Bulgular & Veri:In order to investigate the possibility of producing acid resistant bricks, nine suggested batches, namely, A1, A2, A3, A4, A5, B1, B2, B3 and B4, were composed for this present study.
💡
Sonuç & Katkı:It was observed that most of the developed brick samples showed excellent results in both HCl and H 2 SO 4 media in accordance with IS: 4860-1968 and ESS:41-1986.
🔬Tür:Araştırma Makalesi
📍Kapsam:Genişletilmiş Akademik Örneklem
⚙️Değişkenler:Alan Parametreleri

Özet

The disposal of industrial wastes comprises one of the major worldwide environmental problems as these wastes render the environment unfriendly. The growing demand for waste utilization has made solid wastes- like materials from granite processing industry, and sand to be absorbed into the ceramic composition of bricks. The possibility of reduction in production costs provides a strong logic for use of these wastes. In this work, attempt was made to develop acid resistant bricks from quarry fine waste residues (stone dust, kaolin and sand). In order to investigate the possibility of producing acid resistant bricks, nine suggested batches, namely, A1, A2, A3, A4, A5, B1, B2, B3 and B4, were composed for this present study. These mixtures were composed of 40 wt% of Kaolin fine residue with 10-50 wt% of stone dust and silica sand; and 50 wt% of Kaolin fine residue with 10-40 wt% of stone dust and silica sand respectively. The bodies made with the variation of raw materials were sintered at 970 0 C and their behaviors with respect to apparent porosity, water absorption, bulk density, firing volume changes, compressive strength and acid resistance as a function of temperature, stone dust and sand was studied. It was observed that most of the developed brick samples showed excellent results in both HCl and H 2 SO 4 media in accordance with IS: 4860-1968 and ESS:41-1986.

🔖

Bu Makaleye Atıf Yap

OWOEYE, S. S., LAMIDI, Y. D., AJAYI, O. J. (2017). Physico-mechanical and corrosion behavior of acid resistant bricks developed from quarry waste silicate residues using powder metallurgy. Research on Engineering Structures and Materials, Cilt: 3 - Sayı: 1, 55–64. https://ajindex.com/articles/302630

📄 Tam Metin PDF Okuyucu

📄

PDF görüntüleyici hazırlanıyor...

Kaynakça (8)

  1. Ferreira JMF, Torres PMC, Silva MS, Labrincha JA. Recycling of sludges generated from natural stones cutting processes in ceramic formulations. Proceedings of the TMS Fall Meeting on Recycling and Waste Treatment in Mineral and Metal Processing: Technical and Economic Aspects, 2002; 2:389-395.
  2. Pereira DA, Couto DM, Labrincha J.A. Incorporation of aluminum-rich residues in refractory bricks. Ceram. Forum Int., 2000; 77:21-25.
  3. Ribeiro MJ, Ferreira,JMF., Labrincha JA. Clay-based ceramic formulations containing different solid wastes. Euro Ceram. Newslett., 2002; 14:4-7.
  4. Menezesa R, Ferreirab HS, Neves GA, Lirab H, Ferreirab HC. Use of granite sawing wastes in the production of ceramics bricks and tiles. J. European Ceramic Society, 2005; 25:1149-1158. http://dx.doi.org/10.1016/j.jeurceramsoc.2004.04.020
  5. Youssef NF, Osman TA, El-Shimy E. Utilization of granite-basalt fine quarry waste in a ceramics floor tile mixture. J. Silicate Industry, 2004; 69:7-13.
  6. El-Alfi EA, Radwan AM, Ail MH. Physico-mechanical properties of basalt bricks. J. Inter. Ceram., 2004; 53:178-181. Williams TP. Waste treatment and disposal, 2nd ed. New York: John Wiley & Sons, 2005. http://dx.doi.org/10.1002/0470012668
  7. Ibrahim DM, Mostafa AA, Nour WMN. Granite processing waste as a source of flux for the production of acid resistant sewage bricks. International Ceramic Review, 2006; 55:186-190. Medhat SE. Characterization of acid resisting bricks made from quarry residues and waste steel slag. Construction and Building Materials, 2008; 22:1887–1896. http://dx.doi.org/10.1016/j.conbuildmat.2007.04.007
  8. Eliche-Quesada D, Martínez-García C, Martínez-Cartas ML, Cotes-Palomino MT, Pérez- Villarejo L, Cruz-Pérez N, Corpas-Iglesias, FA. The use of different forms of waste in the manufacture of ceramic bricks. Applied Clay Science, 2011; 52:270–276. http://dx.doi.org/10.1016/j.clay.2011.03.003 Hassan SB. Modern refractories: production, properties, testing and applications, 1st ed. Zaria: Timo Commercial Printers, 2005. Omowumi OJ. Characterization of some Nigerian clay as refractory materials for furnace lining, Nigerian Foundry of Engineering Management, 2000; 1-4. Prateik M. Development of acid resistant bricks using waste materials. Department of Ceramic Engineering, National Institute of Technology, Rourkela, Thesis (Unpublished), 2013. Egyptian Standard Specification. Acid-resisting brick of lining sewages tunnels, 1986; 41:1-5. IS 4860: 1968 (R 2001). Specification for Acid Resistant Bricks.