IMPROVEMENT OF MAGNETIC PROPERTIES OF MELT-SPUN PRODUCED Nd2Fe14B PARTICLES DURING SURFACTANT-ASSISTED BALL MILLING

Pages
25–35
Publication Date
2016-04-01
DOI
—
🏛️Bibliographic metadata and full text access for this article are provided via DergiPark.
DergiPark Record ↗
✨

AI Summary & Key Takeaways

AI Insight
⚡ TL;DR(Too Long; Didn't Read)

The experiments were performed to optimize the milling parameters regarding the particle size and magnetic properties of the powders

📌 3 Key Takeaways

🎯
Objective & Hypothesis:NdFeB permanent magnets are used for variety of applications such as electronics, automotive and clean technology industries.
📊
Key Findings & Data:The sintered NdFeB magnets represent about 90% of the total rare earth permanent magnet market.
💡
Conclusion & Impact:The experiments were performed to optimize the milling parameters regarding the particle size and magnetic properties of the powders
🔬Design:Research Article
📍Scope:Comprehensive Sample
⚙️Variables:Nd15Fe77B8 magnetic alloy · Melt spinning · Surfactant-assisted

Abstract

NdFeB permanent magnets are used for variety of applications such as electronics, automotive and clean technology industries. The majority of commercial NdFeB permanent magnets are produced by melt-spinning techniques and sintering. The sintered NdFeB magnets represent about 90% of the total rare earth permanent magnet market. Sintered melt-spin NdFeB magnets exhibit the highest magnetic performance due to their strong crystallographic alignment. These magnets have enabled their applications to operate with the highest energy efficiencies and to be fabricated in the most compact form. In this study, the flaky shaped Nd15Fe77B8 magnetic alloy powders were produced by melt-spinning technique. In this process, the powders were produced by using a single roller melt spinning apparatus with high vacuum atmosphere (10-7 mbar). The flaky shaped Nd15Fe77B6 powders were milled by using the high energy ball milling under vacuum atmosphere with surfactant-assisted material. The experiments were performed to optimize the milling parameters regarding the particle size and magnetic properties of the powders

🔖

Cite This Article

ÖZTÜRK, S., İCİN, K., ÖZTÜRK, B., TOPAL, U., KAFTELEN, H. (2016). IMPROVEMENT OF MAGNETIC PROPERTIES OF MELT-SPUN PRODUCED Nd2Fe14B PARTICLES DURING SURFACTANT-ASSISTED BALL MILLING. The International Journal of Energy and Engineering Sciences, Cilt: 1 - Sayı: 2, 25–35. https://ajindex.com/articles/806019

📄 Full Text PDF Viewer

📄

PDF görüntüleyici hazırlanıyor...

References (10)

  1. Brown, D. N., Wu, Z., He, F., Miller, D. J., & Herchenroeder, J. W. (2014). Dysprosium-free melt-spun permanent magnets. Journal of Physics: Condensed Matter, 26(6), 64202. http://doi.org/10.1088/0953-8984/26/6/064202
  2. Chandrasekaran, P. S. and R. G. and N. V. R. R. and M. M. R. and V. (2007). SmCo 5 /Fe nanocomposite magnetic powders processed by magnetic field-assisted ball milling with and without surfactant. Journal of Physics D: Applied Physics, 40(17), 5021. http://doi.org/10.1088/0022-3727/40/17/002
  3. Lewis, L. H., Panchanathan, V., & Wang, J. Y. (1997). Technical magnetic properties of melt-spun (Nd1-xPrx)(2)Fe14B at low temperature. Journal of Magnetism and Magnetic Materials, 176(2–3), 288–296. http://doi.org/10.1016/S0304-8853(97)00648-3
  4. Neu, V., & Schultz, L. (2001). Two-phase high-performance Nd-Fe-B powders prepared by mechanical milling. Journal of Applied Physics, 90(3), 1540–1544. http://doi.org/10.1063/1.1380223
  5. Ono, K., Kakefuda, Y., Okuda, R., Ishii, Y., Kamimura, S., Kitamura, a., & Oshima, M. (2002). Organometallic synthesis and magnetic properties of ferromagnetic SmCo nanoclusters. Journal of Applied Physics, 91(10 I), 8480–8482. http://doi.org/10.1063/1.1456407
  6. Ozawa, S., Saito, T., & Motegi, T. (2004). Effects of cooling rate on microstructures and magnetic properties of Nd-Fe-B alloys. Journal of Alloys and Compounds, 363(1–2), 263–270. http://doi.org/10.1016/S0925-8388(03)00461-4
  7. Rong, C., Poudyal, N., & Liu, J. P. (2010). Size-dependent spin-reorientation transition in Nd2Fe14B nanoparticles. Physics Letters A, 374(38), 3967–3970. http://doi.org/10.1016/j.physleta.2010.07.061
  8. Simeonidis, K., Sarafidis, C., Papastergiadis, E., Angelakeris, M., Tsiaoussis, I., & Kalogirou, O. (2011). Evolution of Nd2Fe14B nanoparticles magnetism during surfactant-assisted ball-milling. Intermetallics, 19(4), 589–595. http://doi.org/10.1016/j.intermet.2010.12.012
  9. Su, K. P., Liu, Z. W., Zeng, D. C., Huo, D. X., Li, L. W., & Zhang, G. Q. (2013). Structure and size-dependent properties of NdFeB nanoparticles and textured nano-flakes prepared from nanocrystalline ribbons. Journal of Physics D: Applied Physics, 46(24), 245003. http://doi.org/10.1088/0022-3727/46/24/245003
  10. Szymura, S., Wyslicki, J., Rabinovich, Y., & Bala, H. (1994). Domain structure, magnetic and mechanical properties of Nd-Fe-B magnets with different grain size. Phys. Stat. Sol. (a), 141, 435. Tian, Z., Li, S., Peng, K., Gu, B., Zhang, J., Lu, M., & Du, Y. (2004). The microstructure and