Journals / Teknik Dergi / 2022 / Cilt: 33 - Sayı: 4

The Effect of Hydrated Lime Mixing Forms and Ratios on Performance in Asphalt Pavements

Pages
12243–12263
Publication Date
2022-10-18
DOI
—
🏛️Bibliographic metadata and full text access for this article are provided via DergiPark.
DergiPark Record ↗
✨

AI Summary & Key Takeaways

AI Insight
⚡ TL;DR(Too Long; Didn't Read)

However, if the HL content is increased to medium and high levels, mixing HL to AC creates higher water damage resistance than adding it as filler.

📌 3 Key Takeaways

🎯
Objective & Hypothesis:In this study; the water damage problem and indirect tensile strengths (ITS) were investigated for different hydrated lime (HL) additive ratios and adding methods.
📊
Key Findings & Data:In this regard, identical briquettes modified with hydrated lime have been produced.
💡
Conclusion & Impact:However, if the HL content is increased to medium and high levels, mixing HL to AC creates higher water damage resistance than adding it as filler.
🔬Design:Research Article
📍Scope:Comprehensive Sample
⚙️Variables:Asphalt pavements · hydrated lime · HL mixing forms

Abstract

In this study; the water damage problem and indirect tensile strengths (ITS) were investigated for different hydrated lime (HL) additive ratios and adding methods. In this regard, identical briquettes modified with hydrated lime have been produced. HL was used both in the bituminous binder (wet method) and as part of the filler aggregate. The hydrated lime was added in two different ways to form the defined equivalent ratios. By producing nine identical briquettes in each option, the values of water damage and ITS in both unconditioned and modified mixtures were compared, and the level of significance differences between the identical briquettes and mixtures was questioned. Increasing the HL content increases the standard deviation between identical samples in terms of ITS. The workability of the mixture is adversely affected by the increase in the hydrated lime ratio. When HL is mixed into the asphalt cement (AC), the standard deviations of ITS values among identical samples remain lower due to the increase in mixing rates. Increasing the ratio of adding HL to the asphalt cement reduces the ITS ratios compared to the option of adding filler to aggregate. If HL is added to the mixture in low HL content, the water damage ratios show, on average, higher water damage resistance (15% higher) than the HL being added to the AC. However, if the HL content is increased to medium and high levels, mixing HL to AC creates higher water damage resistance than adding it as filler.

Özet

In this study; the water damage problem and indirect tensile strengths (ITS) were investigated for different hydrated lime (HL) additive ratios and adding methods. In this regard, identical briquettes modified with hydrated lime have been produced. HL was used both in the bituminous binder (wet method) and as part of the filler aggregate. The hydrated lime was added in two different ways to form the defined equivalent ratios. By producing nine identical briquettes in each option, the values of water damage and ITS in both unconditioned and modified mixtures were compared, and the level of significance differences between the identical briquettes and mixtures was questioned. Increasing the HL content increases the standard deviation between identical samples in terms of ITS. The workability of the mixture is adversely affected by the increase in the hydrated lime ratio. When HL is mixed into the asphalt cement (AC), the standard deviations of ITS values among identical samples remain lower due to the increase in mixing rates. Increasing the ratio of adding HL to the asphalt cement reduces the ITS ratios compared to the option of adding filler to aggregate. If HL is added to the mixture in low HL content, the water damage ratios show, on average, higher water damage resistance (15% higher) than the HL being added to the AC. However, if the HL content is increased to medium and high levels, mixing HL to AC creates higher water damage resistance than adding it as filler.

🔖

Cite This Article

AKSOY, A., İSKENDER, E., ŞENGÜL, C. E., AYYILDIZ, D. (2022). The Effect of Hydrated Lime Mixing Forms and Ratios on Performance in Asphalt Pavements. Teknik Dergi, Cilt: 33 - Sayı: 4, 12243–12263. https://ajindex.com/articles/596536

📄 Full Text PDF Viewer

📄

PDF görüntüleyici hazırlanıyor...

References (10)

  1. Preti, F., Accardo, C., Gouveia, B. C. S., Romeo, E., Tebaldi, G. (2020). Influence of high-surface-area hydrated lime on cracking performance of open-graded asphalt mixtures. Road Materials and Pavement Design, 1-7.
  2. Lesueur, D., Denayer, C., Ritter, H.-J., Kunesch, C., Gasiorowski, S., d'Alto, A. (2016). The use of hydrated lime in the formulation of asphalt mixtures: European case studies. E&E Congress 2016, 6th Eurasphalt & Eurobitume Congress, Prague, Czech Republic Roberto, A., Romeo, E., Montepara, A., & Roncella, R. (2020). Effect of fillers and their fractional voids on fundamental fracture properties of asphalt mixtures and mastics. Road Materials and Pavement Design, 21(1), 25-41.
  3. Peterson, J.C. (1998). Lime-treated pavements offer increased durability. Roads and Bridges Journal 26(1), 85-87.
  4. Wang, H., Al-Qadi, I. L., Faheem, A. F., Bahia, H. U., Yang, S. H., Reinke, G. H. (2011). Effect of mineral filler characteristics on asphalt mastic and mixture rutting potential. Transportation Research Record, 2208(1), 33-39.
  5. Rashwan, N.K. (2016). Hot Mix Asphalt (HMA) performance as affected by limestone powder filler content. World Applied Sciences Journal 34 (2), 237-244.
  6. Han, S., Dong, S., Yin, Y., Liu, M., Liu, Y. (2020). Study on the effect of hydrated lime content and fineness on asphalt properties, Construction and Building Materials, 244, 118379. Sebaaly, P. E., Little, D. N., Epps, J. A. (2006). The benefits of hydrated lime in hot mix asphalt. Prepared for the National Lime Association, April 2006
  7. Lesueur, D. (2010). Hydrated lime: A proven additive for durable asphalt pavements–Critical literature review. Brussels: European Lime Association (EuLA) Ed. 2010.
  8. Little, D. N., Petersen, J. C. (2005). Unique effects of hydrated lime filler on the performance-related properties of asphalt cements: Physical and chemical interactions revisited. Journal of Materials in Civil Engineering, 17(2), 207-218.
  9. Han, S., Dong, S., Liu, M., Han, X., Liu, Y. (2019). Study on improvement of asphalt adhesion by hydrated lime based on surface free energy method. Construction and Building Materials, 227, 116794. Huang, S. C., Robertson, R. E., Branthaver, J. F., Petersen, J. C. (2005). Impact of lime modification of asphalt and freeze–thaw cycling on the asphalt–aggregate interaction and moisture resistance to moisture damage. Journal of Materials in Civil Engineering, 17(6), 711–718.
  10. Hicks, R. G., Scholz, T. V. (2003). Life Cycle Costs for Lime in Hot Mix Asphalt, Rep