Journals / International Journal of Automotive Science and Technology / 2020 / Cilt: 4 - Sayı: 4

Effect of Ultrasonic Treatment Parameters on Microstructural and Mechanical Properties of A356 Aluminum Alloy

Pages
234–243
Publication Date
2022-10-19
DOI
—
🏛️Bibliographic metadata and full text access for this article are provided via DergiPark.
DergiPark Record ↗
✨

AI Summary & Key Takeaways

AI Insight
⚡ TL;DR(Too Long; Didn't Read)

According to the results, the amount of liquid metal directly affects the the ultrasonic intensity that is produced during the treatment.

📌 3 Key Takeaways

🎯
Objective & Hypothesis:The aim of this study is to investigate the effect of ultrasonic treatment on the microstructural and mechanical properties of A356 aluminum al-loy.
📊
Key Findings & Data:Ultrasonic treatment was applied to 2 kg and 4 kg molten metals at different melting temperatures (700 oC, 720 oC and 740 oC) for different durations (0, 60, 180 and 300 seconds).
💡
Conclusion & Impact:According to the results, the amount of liquid metal directly affects the the ultrasonic intensity that is produced during the treatment.
🔬Design:Research Article
📍Scope:Comprehensive Sample
⚙️Variables:Ultrasonic treatment · Aluminum alloy · Bifilm index

Abstract

The aim of this study is to investigate the effect of ultrasonic treatment on the microstructural and mechanical properties of A356 aluminum al-loy. Ultrasonic treatment was applied to 2 kg and 4 kg molten metals at different melting temperatures (700 oC, 720 oC and 740 oC) for different durations (0, 60, 180 and 300 seconds). Bifilm indices of the samples were also measured after all parameters were tested. The ultimate tensile strength (UTS) and elongation values were used to calculate the Quality Index (QI) of the samples. According to the results, the amount of liquid metal directly affects the the ultrasonic intensity that is produced during the treatment. Maximum UTS and elongation results were determined at 720 oC during 300 seconds for 4 kg casting. Minimum bifilm density val-ue was measured at the same ultrasonic temperature and time.

🔖

Cite This Article

DOKUMACI, E., ÖNEL, K., AYBARÇ, U. (2022). Effect of Ultrasonic Treatment Parameters on Microstructural and Mechanical Properties of A356 Aluminum Alloy. International Journal of Automotive Science and Technology, Cilt: 4 - Sayı: 4, 234–243. https://ajindex.com/articles/540495

📄 Full Text PDF Viewer

📄

PDF görüntüleyici hazırlanıyor...

References (13)

  1. H. Puga, M. Prokic, N. Van Donge: MMM Ultrasonic Metallurgy. http://mastersonics.com/documents/mmm_applications/ultrasonic_metallurgy/MMM-Ultrasonic-Metallurgy-Aluminium-International.pdf. Accessed 08 May 2018
  2. Birol, Y. (2013). Impact of grain size on mechanical properties of AlSi7Mg0.3 alloy: Materials Science and Engineering A, 559, 394–400.
  3. Nikanorov, S.P., Volkov, M. P., Gurin, V.N., Burenkov, Y. A., Derkachenko, L.I., Kardashev, B.K., Regel, L.L., Wilcox, W.R. (2005). Structural and mechanical properties of Al-Si alloys obtained by fast cooling of a levitated melt: Materials Science and Engineering:A, 390(1–2), 63–69.
  4. YE, H. (2003). An overview of the development of Al-Si-Alloy based material for engine applications: JMEPEG, 12(3), 288–297.
  5. Hawari, A. A., Khader, M., Hasan, W. E., Alijla, M., Manawi, A., Benamour, A. (2014). A life cycle assessment (LCA) of aluminum production process: International Journal of Mechanical, Aerospace, Industrial, Mechatronic and Manufacturing Engineering, 8(4), 704–710.
  6. Xu, H., Meek, T., Han, Q. (2007). Effects of ultrasonic field and vacuum on degassing of molten aluminum alloy: Materials Letters, 61(4–5), 1246–1250.
  7. Xu, H., Jian, X., Meek, T. T., Han, Q. (2004). Degassing of molten aluminum A356 alloy using ultrasonic vibration: Materials letters, 58(29), 3669–3673.
  8. Felberbaum, M., Landry-Désy, E., Weber, L., Rappaz, M. (2011). Effective hydrogen diffusion coefficient for solidifying aluminium alloys: Acta Materialia, 59(6), 2302–2308.
  9. Dispinar, D., Akhtar, S., Nordmark, A., Sabatino, M.D., Arnberg, L. (2010). Degassing, hydrogen and porosity phenomena in A356: Materials Science and Engineering: A, 527(16–17), 3719–3725.
  10. Dispinar, D., Campbell, J. (2004). Critical assessment of reduced pressure test. Part 1: Porosity phenomena: International Journal of Cast Metals Research, 17(5), 280–286.
  11. Dispinar, D., Campbell, J. (2011). Porosity, hydrogen and bifilm content in: Materials Science and Engineering: A, 528(10–11), 3860–3865.
  12. Dispinar, D., Akhtar, S., Nordmark, A., Syvertsen, F., Sabatino, M.D., Arnberg, L. (2012). Correlation between mechanical properties and porosity distribution of A356 in gravity die casting and low pressure die casting: Advanced Materials Research. Trans Tech Publ, 445, 283–288.
  13. Eskin, D.G., Atamanenko, T.V., Zhang, L., Katgerman, L. (2010). On the mechanism of grain refinement by ultrasonic melt treatment in the presence of transition metals: Essential Readings in Light Metals. 415–419. Eskin,