AI Summary & Key Takeaways

AI Insight
⚡ TL;DR(Too Long; Didn't Read)

As a result, a lead concentrate of 55.13% Pb was obtained and it was found that this concentrate contained 2489 ppm of Ag.

📌 3 Key Takeaways

🎯
Objective & Hypothesis:In this study, grinding + flotation experiments were performed on the sample of complex Pb-Zn sulphide ore taken from Niğde (Ulukışla-Madenköy) region in Turkey.
📊
Key Findings & Data:The experiments were carried out at a solid ratio of 30%, a flow rate of 10 L/min, a stirring rate of 1250 rpm and pH = 9.
💡
Conclusion & Impact:As a result, a lead concentrate of 55.13% Pb was obtained and it was found that this concentrate contained 2489 ppm of Ag.
🔬Design:Research Article
📍Scope:Comprehensive Sample
⚙️Variables:Domain Parameters

Özet

In this study, grinding + flotation experiments were performed on the sample of complex Pb-Zn sulphide ore taken from Niğde (Ulukışla-Madenköy) region in Turkey. According to the mineralogical analysis of the ore sample used in experimental studies, it was determined that the ore composition contains calcite, quartz, pyrite, chalcopyrite, hematite, goethite, limonite, gypsum, galena, sphalerite, jarosite, arsenopyrite and marcasite minerals. In addition, Au and Ag grains were found to be inclusions in hematite, goethite and jarosite minerals. The experiments were carried out at a solid ratio of 30%, a flow rate of 10 L/min, a stirring rate of 1250 rpm and pH = 9. In flotation tests, lime is used as the pH regulator, zinc sulphate, sodium silicate as the depressant, sodium isobutyl dithiophosphine as the collector and methyl isobutyl carbinol as the frother. In the flotation studies, the effect of Aerophine 3418A collector dosage on flotation was investigated. As a result, a lead concentrate of 55.13% Pb was obtained and it was found that this concentrate contained 2489 ppm of Ag. The amount of Aerophine 3418A collector was determined as 10 g/t.

🔖

Cite This Article

AGACAYAK, T., YİLMAZ, N. B. (2021). The Effect of Aerophine 3418A Collector Dosage on Niğde (Ulukışla-Madenköy) Complex Pb-Zn Sulphide Ore Flotation. ACADEMIC PLATFORM-JOURNAL OF ENGINEERING AND SCIENCE, Cilt: 9 - Sayı: 2, 309–313. https://ajindex.com/articles/354819

📄 Full Text PDF Viewer

📄

PDF görüntüleyici hazırlanıyor...

References (18)

  1. S. Temur, “Bolkardağı yöresi (Ulukışla/Niğde) çinkokurşun yataklarının jeokimyasal incelemesi”. Türkiye Jeoloji Bülteni, Sayı: 35, s: 101–114, 1990
  2. N. Şişman, M.H. Şenocak, S. Dilek, M. Yazgaç, “Bolkardağ yöresinin jeolojisi ve maden yatakları”, MTA Genel Müdürlüğü, Rapor No: 7202, Ankara, (1981)
  3. S. Atak, Flotasyon ilkeleri ve uygulaması, İstanbul, 1990
  4. A. M. Gaudin, Flotation, McGraw Hill, New York, 1957
  5. J. S. Laskowski, Frothing in Flotation II, G&B Science,1998
  6. B.K. Parekh, J. D. Miller, Advances in flotation technology, Soc. for Mining Metallurgy, New York, 1999
  7. L. Leja, Surface Chemistry of Froth Flotation. New York, 1982
  8. N. Arbiter, SME Mineral Processing Handbook, Volume I, New York, 1985
  9. B.A. Wills, Mineral Processing Technology. Fourth Edition,1988
  10. M. Cao, Q. Liu, “Re-examining the functions of zinc sulphate as a selective depressant in differential sulphide flotation the role of coagulation”, Journal of Colloid and Interface Science, vol. 301, pp. 523– 531, 2006
  11. S.M. Bulatovic, Handbook of flotation reagents, chemistry. theory and practice, flotation of sulfide ores, Elsevier, Amsterdam, 2007
  12. S.R. Grano, M. Sollaart, W. Skinner, C.A. Prestidge, J. Ralston, “Surface modifications in the chalcopyrite-sulphite ion system. I. collectorless flotation, XPS and dissolution study” International Journal of Mineral Processing, vol. 50(2), pp. 1-26, 1997
  13. S.R. Grano, N.W. Johnson, J. Ralston, “Control of the solution interaction of meta bisulphite and ethyl xanthate in the flotation of the Hilton ore of Mount Isa Mines Limited, Australia”, Miner. Eng., vol. 10 (1), pp. 17, 1997a
  14. S.R. Grano, C.A. Prestidge, J. Ralston, “Solution interaction of ethyl xanthate and sulphite and its effect on galena flotation and xanthate adsorption”, Int. J. of Miner. Process. Vol. 52, pp. 161-186, 1997b
  15. T.N. Khmeleva, J.K. Chapelet, W.M. Skinner, D.A. Beattie, “Depression mechanisms of sodium bisulphite in the xanthate-induced flotation of copper activated sphalerite”, International Journal of Mineral Processing. Vol.79, pp. 61-75, 2006
  16. N. Acarkan, G. Bulut, A. Gül, O. Kangal, F. Karakaş, O. Kökkılıç, G. Önal, “The effect of collector's type on gold and silver flotation in a complex ore”, Sep. Sci. Technol. Vol. 46, pp. 283–289, 2011
  17. C. Durmaz, “Kuyumculuk kökenli curüflardan fiziksel zenginleştirme yöntemleri ile altının geri kazanımı”, Yüksek Lisans Tezi, İstanbul, 2012
  18. Cytec Min