Journals / El-Cezeri / 2020 / Cilt: 7 - Sayı: 2

Hot Corrosion Resistance of ZrO2-5%CaO Thermal Barrier Coating (TBC) System

ZrO2-5%CaO TERMAL BARİYER KAPLAMA (TBC) SİSTEMİNİN SICAK KOROZYON DİRENCİ

Journal
El-Cezeri
Pages
628–638
Publication Date
2020-05-31
DOI
—
🏛️Bibliographic metadata and full text access for this article are provided via DergiPark.
DergiPark Record ↗
✨

AI Summary & Key Takeaways

AI Insight
⚡ TL;DR(Too Long; Didn't Read)

It has been found that the molten corrosion salts penetrate through the top coating, but have not yet seriously damaged the coating under these test conditions.

📌 3 Key Takeaways

🎯
Objective & Hypothesis:Thermal barrier coatings (TBCs) provide thermal and corrosive protection to metallic substrate materials under high temperature conditions.
📊
Key Findings & Data:In this study, NiCoCrAlY powders were sprayed on 316L stainless steel substrate material using High Velocity Oxygen Fuel (HVOF) technique.
💡
Conclusion & Impact:It has been found that the molten corrosion salts penetrate through the top coating, but have not yet seriously damaged the coating under these test conditions.
🔬Design:Research Article
📍Scope:Comprehensive Sample
⚙️Variables:Sıcak korozyon · Termal bariyer kaplama · CaO-ZrO2

Abstract

Thermal barrier coatings (TBCs) provide thermal and corrosive protection to metallic substrate materials under high temperature conditions. TBC systems applied to hot part components of workpieces are exposed to oxidation and hot corrosion damage. Hot corrosion, in particular, causes destructive damage earlier than oxidation. In this study, NiCoCrAlY powders were sprayed on 316L stainless steel substrate material using High Velocity Oxygen Fuel (HVOF) technique. Calcia-stabilized zirconia (ZrO2-5% CaO, CSZ) was deposited as a top coating material by the atmospheric plasma spray technique (APS) on the substrate with the bond coat. The produced TBC system was subjected to 25 hours cyclic hot corrosion tests with a mixture of 50% V2O5- 50% Na2SO4 at 900 °C. At the end of the hot corrosion tests, as a result of the reaction of CaO with hot corrosion salts, phase transformation has occurred in the top coating. It has been found that the molten corrosion salts penetrate through the top coating, but have not yet seriously damaged the coating under these test conditions.

Özet

Termal bariyer kaplamalar (TBCs), yüksek sıcaklık koşullarında metalik altlık malzemeleri termal ve korozif koruma sağlamaktadır. TBC sistemleri, iş parçalarının sıcak bölüm komponentlerinde oksidasyon ve sıcak korozyon hasarlara maruz kalmaktadır. Özellikle sıcak korozyon, oksidasyona nazaran daha erken yıpratıcı hasarlara neden olmaktadır. Bu çalışmada, NiCoCrAlY tozları, yüksek hız oksi yakıt (HVOF) tekniği kullanılarak 316L paslanmaz çelik altlık malzeme üzerine püskürtülmüştür. Kalsiya ile stabilize zirkonya (ZrO2-5% CaO, CSZ), bağ kaplaması üretilmiş altlıklar üzerine üst kaplama malzemesi olarak atmosferik plazma sprey tekniği (APS) ile biriktirilmiştir. Üretilen TBC sistemi, 900 ° C' de % 50 V2O5-50 Na2SO4 karışımı ile 25 saatlik çevrimli sıcak korozyon testlerine tabi tutulmuştur. Sıcak korozyon testlerinin sonunda TBC sistemlerinde korozyon etkisi ve faz analizi stereo mikroskop, taramalı elektron mikroskobu (SEM), SEM - Enerji Dağılımlı X-Ray (EDX), SEM Haritalama ve XRD analizi kullanılarak incelenmiştir.

🔖

Cite This Article

DÖLEKER, K. M. (2020). Hot Corrosion Resistance of ZrO2-5%CaO Thermal Barrier Coating (TBC) System. El-Cezeri, Cilt: 7 - Sayı: 2, 628–638. https://ajindex.com/articles/252557

📄 Full Text PDF Viewer

📄

PDF görüntüleyici hazırlanıyor...

References (14)

  1. Doleker, K. M., Ozgurluk, Y., Ahlatci, H., Karaoglanli, A. C., Evaluation of oxidation and thermal cyclic behavior of YSZ, Gd2Zr2O7 and YSZ/Gd2Zr2O7 TBCs, Surface And Coatings Technology, 2019, 371, 262–275.
  2. Padture, N. P., Thermal Barrier Coatings for Gas-Turbine Engine Applications, Science, 2002, 296 (5566), 280–284.
  3. Karaoglanli, A. C., Doleker, K. M., Ozgurluk, Y., "State of the art thermal barrier coating (TBC) materials and tbc failure mechanisms", Advanced Structured Materials, Springer, Singapore, 2017, 441–452.
  4. Wortman, D. J., Fryxell, R. E., Luthra, K. L., Bergman, P. A., Mechanism of low temperature hot corrosion: Burner rig studies, Thin Solid Films, 1979, 64(2), 281–288.
  5. Eliaz, N., Shemesh, G., Latanision, R. M., Hot corrosion in gas turbine components, Engineering Failure Analysis, 2002, 9(1), 31–43.
  6. Hui, Y., Zhao, S., Xu, J., Zou, B., Wang, Y., Cai, X., Zhu, L., Cao, X., High-temperature corrosion behavior of zirconia ceramic in molten Na2SO4+NaVO3 salt mixture, Ceramics International, 2016, 42(1), 341–350.
  7. Habibi, M. H., Wang, L., Guo, S. M., Evolution of hot corrosion resistance of YSZ, Gd2Zr2O7, and Gd2Zr2O7+YSZ composite thermal barrier coatings in Na2SO4+V2O5 at 1050°C, Journal of The European Ceramic Society, 2012, 32(8), 1635–1642.
  8. Ozgurluk, Y., Doleker, K. M., Karaoglanli, A. C., Hot corrosion behavior of YSZ, Gd2Zr2O7 and YSZ/Gd2Zr2O7 thermal barrier coatings exposed to molten sulfate and vanadate salt, Applied Surface Science, 2018, 438, 96–113.
  9. Ozgurluk, Y., Doleker, K. M., Karaoglanli, A. C., Investigation of the effect of V2O5 and Na2SO4 melted salts on thermal barrier coatings under cyclic conditions, Anti-Corrosion Methods And Materials, 2019, 66(5), 644–650.
  10. Keyvani, A., Saremi, M., Heydarzadeh Sohi, M., Microstructural stability of zirconia-alumina composite coatings during hot corrosion test at 1050 °C, Journal of Alloys and Compounds, 2010, 506(1), 103–108.
  11. Wang, P., Deng, S., He, Y., Liu, C., and Zhang, J., Oxidation and hot corrosion behavior of Al2O3/YSZ coatings prepared by cathode plasma electrolytic deposition, Corrosion Science, 2016, 109, 13–21.
  12. Worrel, W. L., Solid Electrolytes, Springer-Verlag, New York, 2006, 143–166.
  13. Evans, H. E., Oxidation failure of TBC systems: An assessment of mechanisms, Surface and Coatings Technology, 2011, 206(7), 1512–1521.
  14. Toscano, J., Naumenko, D., Gil, A., Singheiser, L., Quadakkers, W. J., Parameters affecting TGO growth rate and the lifetime of TBC systems with MCrAIY-bondcoats, M