AI Summary & Key Takeaways

AI Insight
⚡ TL;DR(Too Long; Didn't Read)

Choosing the surface treatment method occording to the type and microstructure of the ceramic material is important for providing durable and stable bonding.

📌 3 Key Takeaways

🎯
Objective & Hypothesis:In prosthetic dentistry, increasing sensivity an esthetics and biocompatibilty have moved both the patients’ and dentists’ demands to metal-free tooth colored restorations.
📊
Key Findings & Data:The surface treatments that applied to the all-ceramic materials increase the BS between the all-ceramic restoration and cement, BS between two ceramic layers, and BS between the all-ceramic restoration and the repair material.
💡
Conclusion & Impact:Choosing the surface treatment method occording to the type and microstructure of the ceramic material is important for providing durable and stable bonding.
🔬Design:Research Article
📍Scope:Comprehensive Sample
⚙️Variables:Domain Parameters

Abstract

In prosthetic dentistry, increasing sensivity an esthetics and biocompatibilty have moved both the patients’ and dentists’ demands to metal-free tooth colored restorations. For this reason, the use all-ceramic systems have became widely used. High bonding strength (BS) is crucial for long-term clinical success of all-ceramic restorations. The surface treatments that applied to the all-ceramic materials increase the BS between the all-ceramic restoration and cement, BS between two ceramic layers, and BS between the all-ceramic restoration and the repair material. Mechanical, chemical, or combination of these two methods can be applied to the ceramic surface for a realible bonding. Choosing the surface treatment method occording to the type and microstructure of the ceramic material is important for providing durable and stable bonding.

Özet

Protetik diş hekimliğinde, estetik ve doku uyumluluğuna karşı gösterilen hassasiyet, diş hekimlerini ve hastaları, metal desteksiz protez arayışına yönlendirmiştir. Bu nedenle tam seramiklerin kullanımları yaygınlaşmıştır. Tam seramik restorasyonların uzun dönem klinik başarısı için güçlü bağlanma dayanımı önemlidir. Tam seramik restorasyonlara uygulanan yüzey işlemleri, siman bağlanma dayanımını, iki seramik tabakası arasındaki bağlanma dayanımını ve tamir işlemlerinde tamir materyali ile seramik arasındaki bağlanma dayanımını artırmaktadır. Güvenilir bir bağlantı için seramik yüzeyine mekanik, kimyasal veya her ikisinin kombinasyonu olan yüzey işlemleri uygulanmaktadır. Kullanılan tam seramik materyalinin çeşidini ve mikro yapısını bilmek ve bu özelliklere göre yüzey işlemlerini seçerek uygulamak dayanıklı ve stabil bağlantı dayanımı için önemlidir.

🔖

Cite This Article

SEVMEZ, H., GÜNGÖR, M. B., YILMAZ, H. (2018). Surface Treatments of All Ceramic Restorations. Ege Üniversitesi Diş Hekimliği Fakültesi, Cilt: 39 - Sayı: 3, 148–159. https://ajindex.com/articles/153481

📄 Full Text PDF Viewer

📄

PDF görüntüleyici hazırlanıyor...

References (6)

  1. Leung BT, Tsoi JK, Matinlinna JP, Pow EH. Comparison of mechanical properties of three machinable ceramics with an experimental fluorophlogopite glass ceramic. J Prosthet Dent 2015;114(3):440-6.
  2. Kelly JR, Nishimura I, Campbell SD. Ceramics in dentistry: historical roots and current perspectives. J Prosthet Dent 1996;75(1):18-32.
  3. Wong ACH, Tian T, Tsoi JKH, Burrow MF, Matinlinna JP. Aspects of adhesion tests on resin– glass ceramic bonding. Dent Mater 2017;33(9):1045- 55. Vargas MA, Bergeron C, Diaz-Arnold A. Cementing all-ceramic restorations: recommendations for success. J Am Dent Assoc 2011;142 Suppl 2:20S-4S. Awad M, Alqahtani H, Al-Mudahi A, Murayshed M, Alrahlah A, Bhandi S. Adhesive bonding to computer-aided design/computer-aided manufacturing esthetic dental materials: An overview. J Contemp Dent Pract 2017;18(7):622-6.
  4. Spitznagel FA, Horvath SD, Guess PC, Blatz MB. Resin bond to indirect composite and new ceramic/polymer materials: a review of the literature. J Esthet Restor Dent 2014;26(6):382-93. de Lucena Pereiraa L, Camposb F, Dal Pivac AMdO, Gondimd LD, e Souzae ROdA, Özcanf M. Can application of universal primers alone be a substitute for airborne-particle abrasion to improve adhesion of resin cement to zirconia? J Adhes Dent 2015;17:169- 74. Mello CC, Bitencourt SB, dos Santos DM, Pesqueira AA, Pellizzer EP, Goiato MC. The effect of surface treatment on shear bond strength between Y ‐TZP and veneer ceramic: A systematic review and meta ‐ analysis. J Prosthodont 2017;doi: 10.1111/jopr.12727. Dutra D, Pereira G, Kantorski K, Exterkate R, Kleverlaan C, Valandro L, et al. Grinding with diamond burs and hydrothermal aging of a Y-TZP material: Effect on the material surface characteristics and bacterial adhesion. Oper Dent 2017;42(6):669- 78. Papia E, Larsson C, du Toit M, von Steyern PV. Bonding between oxide ceramics and adhesive cement systems: A systematic review. J Biomed Mater Res B Appl Biomater 2014;102(2):395-413.
  5. Külünk Ş, Külünk T, Kavut İ, Saraç D, Kunt GE. Fracture strength of surface treated zirconia based multilayer CAD/CAM ceramic crowns. Turkiye Klinikleri J Dental Sci 2017;23(3):174-83.
  6. Addison O, Cao X, Sunnar P, Fleming GJ. Machining variability impacts on the strength of a ‘chairside’CAD–CAM ceramic. Dent Mater 2012;28(8):880-7. Pradíes G, Godoy ‐Ruiz L, Özcan M, Moreno‐ Hay I, Martínez ‐Rus F. Analysis of surface roughness, fracture toughness, and weibull characteristics of different framework—veneer dental ceramic assemblies