⚡ TL;DR(1 Cümlede Hızlı Çıkarım)

The differences between the E00-values among the aging tests in the all-ceramic types and the all-ceramic thicknesses were significant.

📌 3 Maddede Bu Makale

🎯
Amaç & Hipotez:The aim of the study is to test the effects of three different aging methods on colour change (E00) in three different all-ceramic systems prepared in two thicknesses (0.5 and 1.0 mm).
📊
Temel Bulgular & Veri:Zirconia Katana UTML (ZK), Prettau Anterior (PA) and IPS-e.max press (EP) prepared in two thicknesses were tested using in vitro artificial accelerated aging (AAA), thermocycling (TC) and autoclave aging (AA) methods.
💡
Sonuç & Katkı:The differences between the E00-values among the aging tests in the all-ceramic types and the all-ceramic thicknesses were significant.
🔬Tür:Araştırma Makalesi
📍Kapsam:Genişletilmiş Akademik Örneklem
⚙️Değişkenler:Accelerated aging · Autoclave aging · Thermocycling

Abstract

Objective. The aim of the study is to test the effects of three different aging methods on colour change (E00) in three different all-ceramic systems prepared in two thicknesses (0.5 and 1.0 mm). Materials and methods. Zirconia Katana UTML (ZK), Prettau Anterior (PA) and IPS-e.max press (EP) prepared in two thicknesses were tested using in vitro artificial accelerated aging (AAA), thermocycling (TC) and autoclave aging (AA) methods. The effects on the colour (CIE L*a*b*) differences were determined using a spectrophotometer and evaluated by analysis of variance (ANOVA). Results. The aging protocols affected the E00-values of the ceramic systems at different levels (0.64–2.69), and the ceramic thicknesses were statistically significant (P <0.5). Generally (excluding the 0.5-mm EP group), the highest E00 value among the methods of aging was in the AAA applied samples, followed by those in the TC and the AA. Also, the ceramic thickness was found to be significant in testing aging protocols. In addition, the E00-values of the ceramic materials tested were below the clinically accepted level. Conclusions. Three ceramic types – prepared in two different thicknesses and applied for three 1-year in vitro aging protocols – were affected at different levels by the aging methods tested, and significant colour differences were determined among all the ceramic samples. Clinical Significance: One-year applications of three aging protocols (AAA, TC and AA) resulted in significant differences in the E00-values of ceramic systems (ZK, PA and EP). The differences between the E00-values among the aging tests in the all-ceramic types and the all-ceramic thicknesses were significant.

🔖

Bu Makaleye Atıf Yap

TEMIZCI, T., TUNÇDEMİR, A. R. (2020). Effects of Three Aging Methods on Colour Differences of All-Ceramic Materials. Karamanoğlu Mehmetbey Üniversitesi Mühendislik ve Doğa Bilimleri Dergisi, Cilt: 2 - Sayı: 1, 1–17. https://ajindex.com/articles/784102

📄 Tam Metin PDF Okuyucu

📄

PDF görüntüleyici hazırlanıyor...

Kaynakça (13)

  1. Conrad HJ, Seong WJ, Pesun IJ. Current ceramic materials and systems with clinical recommendations: a systematic review. J Prosthet Dent 2007; 98(5):389-404
  2. Douglas RD, Brewer JD. Acceptability of shade differences in metal ceramic crowns. J Prosthet Dent 1998; 79(3):254-260
  3. Kelly J, Benetti P. Ceramic materials in dentistry: historical evolution and current practice. Aust Dent J 2011; 56(s1):84-96
  4. Haselton DR, Diaz-Arnold AM, Hillis SL. Clinical assessment of high-strength all-ceramic crowns. J Prosthet Dent 2000; 83(4):396-401
  5. Türkcan İ, Nalbant AD. Dental protetik materyallerin biyolojik uyumluluğu ve test yöntemleri. AOT 2016; 33(3):145-152
  6. Schulze KA, Marshall SJ, Gansky SA, Marshall GW: Color stability and hardness in dental composites after accelerated aging. Dental materials 2003; 19(7):612-619
  7. Sundh A, Kou W, Sjögren G. Effects of Pretreatment, Specimen Thickness, and Artificial Aging on Biaxial Flexural Strength of Two Types of Y-TZP Ceramics. Operative dentistry 2019; 44(6):615-624
  8. Walczak K, Meißner H, Range U, Sakkas A, Boening K, Wieckiewicz M, Konstantinidis I. Translucency of zirconia ceramics before and after artificial aging. Journal of Prosthodontics 2019; 28(1):e319-e324
  9. Hatanaka GR, Polli GS, Adabo GL. The mechanical behavior of high-translucent monolithic zirconia after adjustment and finishing procedures and artificial aging. The Journal of Prosthetic Dentistry 2020; 123(2):330-337
  10. Kurt M, Bal BT. Effects of accelerated artificial aging on the translucency and color stability of monolithic ceramics with different surface treatments. The Journal of prosthetic dentistry 2019; 121(4):712. e711-712. e718. [11] da Rocha JFS, de Avila ED, Rigolin MSM, Barbugli PA, Marin DO, Junior FAM, Jorge JH. Biological and physicochemical implications of the aging process on titanium and zirconia implant material surfaces. The Journal of Prosthetic Dentistry 2020
  11. Yazigi C, Schneider H, Chaar MS, Rüger C, Haak R, Kern M. Effects of artificial aging and progression of cracks on thin occlusal veneers using SD-OCT. Journal of the mechanical behavior of biomedical materials 2018; 88:231-237
  12. Wei C, Gong X, Xie C, Chen Z, Li S, Gremillard L. In vitro cyclic fatigue and hydrothermal aging lifetime assessment of yttria-stabilized zirconia dental ceramics. Journal of the European Ceramic Society 2020
  13. Ustun S, Ayaz EA. Effect of different cement systems and aging on the bond strength of chairside