Dergiler / European Annals of Dental Sciences / 2021 / Cilt: 48 - Sayı: 1

Color Stability and Surface Roughness of Resin Based Direct and Indirect Restorative Materials

Sayfa
1–6
Yayın Tarihi
2021-04-30
DOI
—
🏛️Bu makalenin bibliyografik verileri ve tam metin bağlantısı DergiPark üzerinden sağlanmıştır.
DergiPark Kaydı ↗
✨

Yapay Zeka Hızlı Bakış & Çıkarımlar

AI Insight
⚡ TL;DR(1 Cümlede Hızlı Çıkarım)

Direct composite resins have a higher discoloration potential over resin-based CAD/CAM blocks, whereas they are less prone to discoloration than indirect composite resins.

📌 3 Maddede Bu Makale

🎯
Amaç & Hipotez:This study investigated discoloration and surface roughness (Ra) in resin-based computer aided design (CAD)/computer aided manufacturing (CAM) blocks and direct and indirect composite resins.
📊
Temel Bulgular & Veri:Using a Teflon mold, disc shaped specimens (8×2 mm2) were fabricated from direct (Estelite Asteria and GrandioSO) and indirect (Gradia Plus) composite resins, and specimens (12×14×2 mm3) were prepared from composite resin CAD/CAM blocks (Vita Enamic, Brilliant Crios, and Cerasmart) (n=10).
💡
Sonuç & Katkı:Direct composite resins have a higher discoloration potential over resin-based CAD/CAM blocks, whereas they are less prone to discoloration than indirect composite resins.
🔬Tür:Araştırma Makalesi
📍Kapsam:Genişletilmiş Akademik Örneklem
⚙️Değişkenler:Resin based CAD/CAM materials · Discoloration · Roughness

Abstract

This study investigated discoloration and surface roughness (Ra) in resin-based computer aided design (CAD)/computer aided manufacturing (CAM) blocks and direct and indirect composite resins. Using a Teflon mold, disc shaped specimens (8×2 mm2) were fabricated from direct (Estelite Asteria and GrandioSO) and indirect (Gradia Plus) composite resins, and specimens (12×14×2 mm3) were prepared from composite resin CAD/CAM blocks (Vita Enamic, Brilliant Crios, and Cerasmart) (n=10). A profilometer was used to determine the Ra values of all 60 polished samples. These specimens were thermocycled between 5 and 55°C for 3,000 cycles, and they were immersed in coffee solution (37°C) for 1 and 7 days. A spectrophotometer was used to determine the color change (∆E00) with the CIEDE2000 formula after the specimens were polished. ANOVA TUKEY test was performed to analyze the data. The lowest degree of discoloration among the materials tested was found in Vita Enamic (<0.05), whereas the highest degree of discoloration was found in the Gradia Plus indirect composite (<0.05). Direct composite resins have a higher discoloration potential over resin-based CAD/CAM blocks, whereas they are less prone to discoloration than indirect composite resins.

🔖

Bu Makaleye Atıf Yap

ERSÖZ, B., KARAOĞLANOĞLU, S., OKTAY, E. A., AYDIN, N. (2021). Color Stability and Surface Roughness of Resin Based Direct and Indirect Restorative Materials. European Annals of Dental Sciences, Cilt: 48 - Sayı: 1, 1–6. https://ajindex.com/articles/757245

📄 Tam Metin PDF Okuyucu

📄

PDF görüntüleyici hazırlanıyor...

Kaynakça (13)

  1. JefferiesSR.Abrasivefinishingandpolishinginrestorative dentistry: a state-of-the-art review. Dent Clin North Am. 2007;51(2):379–397, ix. doi:10.1016/j.cden.2006.12.002
  2. Stawarczyk B, Sener B, Trottmann A, Roos M, Ozcan M, Hämmerle CH. Discoloration of manually fabricated resins and industrially fabricated CAD/CAM blocks ver- sus glass-ceramic: effect of storage media, duration, and subsequent polishing. Dent Mater J. 2012;31(3):377–383. doi:10.4012/dmj.2011-238
  3. Spitznagel FA, Vuck A, Gierthmühlen PC, Blatz MB, Hor- vath SD. Adhesive Bonding to Hybrid Materials: An Overview of Materials and Recommendations. Compend Contin Educ Dent. 2016;37(9):630–637
  4. Stawarczyk B, Awad D, Ilie N. Blue-Light Transmittance of Esthetic Monolithic CAD/CAM Materials With Respect to Their Composition, Thickness, and Curing Conditions. Oper Dent. 2016;41(5):531–540. doi:10.2341/15-252-l
  5. Lawson NC, Burgess JO. Gloss and Stain Resis- tance of Ceramic-Polymer CAD/CAM Restorative Blocks. J Esthet Restor Dent. 2016;28 Suppl 1:S40–45. doi:10.1111/jerd.12166
  6. Spitznagel FA, Horvath SD, Guess PC, Blatz MB. Resin bond to indirect composite and new ceramic/polymer ma- terials: a review of the literature. J Esthet Restor Dent. 2014;26(6):382–393. doi:10.1111/jerd.12100
  7. Giordano R. Materials for chairside CAD/CAM-produced restorations. J Am Dent Assoc. 2006;137 Suppl:14s–21s. doi:10.14219/jada.archive.2006.0397
  8. PapadopoulosT,SarafianouA,HatzikyriakosA.Coloursta- bility of veneering composites after accelerated aging. Eur J Dent. 2010;4(2):137–142
  9. Arocha MA, Basilio J, Llopis J, Di Bella E, Roig M, Ardu S, et al. Colour stainability of indirect CAD-CAM pro- cessed composites vs. conventionally laboratory processed composites after immersion in staining solutions. J Dent. 2014;42(7):831–838. doi:10.1016/j.jdent.2014.04.002
  10. Koc-VuralU,BaltaciogluI,AltinciP.Colorstabilityofbulk- fill and incremental-fill resin-based composites polished with aluminum-oxide impregnated disks. Restor Dent En- dod. 2017;42(2):118–124. doi:10.5395/rde.2017.42.2.118
  11. Luo MR, Cui G, Rigg B. The development of the CIE 2000 colour-difference formula: CIEDE2000. Color Research & Application. 2001;26(5):340–350. doi:10.1002/col.1049
  12. Paravina RD, Ghinea R, Herrera LJ, Bona AD, Igiel C, Linninger M, et al. Color difference thresholds in den- tistry. J Esthet Restor Dent. 2015;27 Suppl 1:S1–9. doi:10.1111/jerd.12149
  13. Rueggeberg FA, Margeson DH. The effect of oxygen inhibition