Dergiler / Turkish Journal of Physics / 2007 / Cilt: 31 - Sayı: 6

Optical Properties and Determination of Thermal Transformation Parameters for Se0.65Te0.35 High Reflectance Thin Films

Sayfa
331–340
Yayın Tarihi
2007-06-01
DOI
—
🏛️Bu makalenin bibliyografik verileri ve tam metin bağlantısı DergiPark üzerinden sağlanmıştır.
DergiPark Kaydı ↗
✨

Yapay Zeka Hızlı Bakış & Çıkarımlar

AI Insight
⚡ TL;DR(1 Cümlede Hızlı Çıkarım)

The activation energies for the glass transition and crystallization were calculated.

📌 3 Maddede Bu Makale

🎯
Amaç & Hipotez:Chalcogenide glasses Se-Te have been prepared from the high purity constituent elements.
📊
Temel Bulgular & Veri:The reflectance and transmittance spectra were measured for the mentioned films and analyzed in the incident photon energy range from 1.16 to 2.47 eV.
💡
Sonuç & Katkı:The activation energies for the glass transition and crystallization were calculated.
🔬Tür:Araştırma Makalesi
📍Kapsam:Genişletilmiş Akademik Örneklem
⚙️Değişkenler:Optical Properties and Parameters · High Reflectance Chalcogenide Semiconductors · Thermal Transformation Parameters

Özet

Chalcogenide glasses Se-Te have been prepared from the high purity constituent elements. Thin films of these materials have been deposited by vacuum evaporation. The thickness effects on the optical properties have been performed for the as-deposited films. The impact of varying thickness on the value of the optical gap is also reported and discussed. The resultant films were in amorphous nature. The reflectance and transmittance spectra were measured for the mentioned films and analyzed in the incident photon energy range from 1.16 to 2.47 eV. The refractive indices were determined as a function of wavelength via the transmittance analysis in the incident photon energy range from 1.16 to 1.38 eV. Also, the dispersion energy, oscillator energy, static refractive index and static dielectric constant were calculated for the thicknesses under investigation. The results of differential scanning calorimetry (DSC) at different heating rates are reported and analyzed. The activation energies for the glass transition and crystallization were calculated.

Abstract

Chalcogenide glasses Se-Te have been prepared from the high purity constituent elements. Thin films of these materials have been deposited by vacuum evaporation. The thickness effects on the optical properties have been performed for the as-deposited films. The impact of varying thickness on the value of the optical gap is also reported and discussed. The resultant films were in amorphous nature. The reflectance and transmittance spectra were measured for the mentioned films and analyzed in the incident photon energy range from 1.16 to 2.47 eV. The refractive indices were determined as a function of wavelength via the transmittance analysis in the incident photon energy range from 1.16 to 1.38 eV. Also, the dispersion energy, oscillator energy, static refractive index and static dielectric constant were calculated for the thicknesses under investigation. The results of differential scanning calorimetry (DSC) at different heating rates are reported and analyzed. The activation energies for the glass transition and crystallization were calculated.

🔖

Bu Makaleye Atıf Yap

EL-AMIN, A. A., BADR, A. M., ABDEL-WAHAAB, F. (2007). Optical Properties and Determination of Thermal Transformation Parameters for Se0.65Te0.35 High Reflectance Thin Films. Turkish Journal of Physics, Cilt: 31 - Sayı: 6, 331–340. https://ajindex.com/articles/724072

📄 Tam Metin PDF Okuyucu

📄

PDF görüntüleyici hazırlanıyor...

Kaynakça (2)

  1. A. R. Hilton, D. J. Hayes and M. D. Rechitin, J. Non-Cryst. Solids, 17, (1975), 319. A. Vasko, in: Proceedings of the 11thinternational congress on glass, 5, (1977), Prague, 533. J. S. Sanghara and I. D. Agarwal, J. Non-Cryst. Solids, 6, (1999), 256. K. Schwarts, The Physics of Optical Recording, (Berlin, Springer-Verlag. 1993).
  2. A. Pradley, Optical Storage for Computers Technology and Applications, (Ellis Horwood Limited, New York. ). K. L. Tai, E. Ong and R. G. Vadimsky, Proc. Electro. Chem. Sci., 9, (1982), 82. Pathinettan Padiyan, A. Marikani and K. R. Murali, Cryst. Res. Technol., 35, (2000), 949. A. H. Mo harram, Thin Solid Films, 392, (2001), 34. V. Pandey, N. Mehta, S. K. Tripathi and A. Kumer, Chalcogenide Letters, 2, (2005), 39. V. Pandey, N. Mehta, S. K. Tripathi and A. Kumar, Chalcogenide Letters, 2, (2005), 39. J. Tauc, Amorphous and Liquid Semiconductors, (New York, Plenum. 1974), Ch. 4. V. N. Chernyaev and V. F. Korzo, Thin Solid Films, 37, (1976), L61. J. I. Pankove, Optical processes in Semiconductors, (New Jersey, Prentice-Hall. 1971), p. 93. A. F. Qasrawi, Cryst. Res. Technol., 40, (2005), 610. J. I. Pankove, Optical process in semiconductors, (Prentice Hall Inc., 1971), p. 45. C. Baban, G. I. Rusu and P. Prepelita, Journal of Optoelectronics and Advanced Materials, 7, (2005), 817. P. Sharma and S. C. Katyal, Mater. Lett., 61, (2007), 4516. M. Lasocka, Mater. Sci. Eng., 23, (1976), 173. H. E. Kissinger, J. Res. Natl Bur. Stand., 57, (1956), 217. T. Ozawa, J. Therm. Anal., 2, (1970), 301. J. A. Augis, J. E. Bennett, J. Them. Anal., 13, (1978), 283. N. AŞfy, A. Gaber, I. Abdalla and H. Talaat, Physica B, 229, (1997), 167.