Dergiler / Cumhuriyet Science Journal / 2021 / Cilt: 42 - Sayı: 4

Effects of various heat treatments on microstructure and mechanical properties of investment cast Co-Cr-Mo implants

Sayfa
965–976
Yayın Tarihi
2022-10-12
DOI
—
🏛️Bu makalenin bibliyografik verileri ve tam metin bağlantısı DergiPark üzerinden sağlanmıştır.
DergiPark Kaydı ↗
✨

Yapay Zeka Hızlı Bakış & Çıkarımlar

AI Insight
⚡ TL;DR(1 Cümlede Hızlı Çıkarım)

Moreover, hardness values increased with the subsequent aging, yet do not change significantly with the solutionizing temperature.

📌 3 Maddede Bu Makale

🎯
Amaç & Hipotez:In this study, the effects of various heat treatments (solutionizing, solutionizing + aging) on the microstructure and mechanical properties of the Co-Cr-Mo based hip implants produced by investment casting were investigated.
📊
Temel Bulgular & Veri:The solution treatments were carried out at 1125°C, 1175°C and 1225°C for 3 hours under argon atmosphere.
💡
Sonuç & Katkı:Moreover, hardness values increased with the subsequent aging, yet do not change significantly with the solutionizing temperature.
🔬Tür:Araştırma Makalesi
📍Kapsam:Genişletilmiş Akademik Örneklem
⚙️Değişkenler:Alan Parametreleri

Abstract

In this study, the effects of various heat treatments (solutionizing, solutionizing + aging) on the microstructure and mechanical properties of the Co-Cr-Mo based hip implants produced by investment casting were investigated. The solution treatments were carried out at 1125°C, 1175°C and 1225°C for 3 hours under argon atmosphere. The aging treatments were carried at 850°C for 4 hours. The samples were examined under scanning electron microscope (SEM) and optical microscope (OM). Room temperature tensile tests and hardness tests were applied. The results showed that, the process of solutionizing at 1175°C and subsequent aging resulted in the formation of the smallest size precipitates with more homogeneous distribution in the interdendritic space of the as-cast structure compared to other treatments. According to tensile test results of the aged samples, as the solutionizing temperature increased to 1175°C both strength and elongation values increased. However, with the increase of solutionizing temperature to 1225°C, strength and elongation values decreased again. Solutionizing temperature of 1175°C gave the best microstructure-mechanical property relationship. Moreover, hardness values increased with the subsequent aging, yet do not change significantly with the solutionizing temperature.

🔖

Bu Makaleye Atıf Yap

ÖZTÜRK, K., ERTUĞRUL, O., ÖZCAN, M. (2022). Effects of various heat treatments on microstructure and mechanical properties of investment cast Co-Cr-Mo implants. Cumhuriyet Science Journal, Cilt: 42 - Sayı: 4, 965–976. https://ajindex.com/articles/477541

📄 Tam Metin PDF Okuyucu

📄

PDF görüntüleyici hazırlanıyor...

Kaynakça (13)

  1. Giacchi J., V, Morando C.N., Fornaro O., Palacio H.A., Microstructural characterization of as-cast biocompatible Co–Cr–Mo alloys, Materials Characterization, 62(1) (2011) 53-61
  2. Zangeneh S.H., Lashgari H.R., Saghafİ M., Karshenas M., Effect of isothermal aging on the microstructural evolution of Co–Cr–Mo–C alloy, Materials Science and Engineering, 527(24-25) (2010) 6494–6500
  3. Montero O.C., Talavera M., Lopez H., Effect of alloy preheating on the mechanical properties of as-cast CoCrMoC alloys, Metallurgical Materials Transactions, 30 (1999) 611–20
  4. Dobbs H.S., Robertson J.L.M., Heat treatment of cast Co–Cr–Mo for orthopaedic implant use, J Mater Sci., 18 (1983) 391–401
  5. Yamanaka K., Mori M., Chiba A., Influence of carbon addition on mechanical properties and microstructures of Ni-free Co–28Cr–9 W–1Si–C alloys subjected to thermomechanical processing, J. Mech. Behav. Biomed. Mater., 37 (2014) 274– 85
  6. Youdelis W.V., Kwon O., Carbide phases in cobalt of subsize tensile test specimens and the traditional base superalloy: Role of nucleation entropy in refine- method of measuring % elongation to fracture by joinment, Metal Sci., 17(8) (1983) 379–384
  7. Lee S.H., Nomura N., Chiba A., Significant improvement in mechanical properties of biomedical Co-Cr-Mo alloys with combination of N addition and Cr enrichment, Mater. Trans., 49(2) (2008) 260–264
  8. Yamanaka K., Mori M., Chiba A., Assessment of precipitation behavior in dental castings of a Co– Cr–Mo alloy, Mechanical Behavior Biomedical Materials, 50 (2015) 268–27
  9. Li S.J., Niinomi M., Akahori T., Kasuga T., Yang R., Hao Y.O., Fatigue characteristics of bioactive glass-ceramic-coated Ti–29Nb–13Ta– 4.6Zr for biomedical application, Biomaterials, 25(17) (2004) 3369-3378
  10. Gomez M., Mancha H., Salinas A., Rodryguez J.L., Escobedo J., Castro M., Mendez M., Relationship between microstructure and ductility of investment cast ASTM F-75 implant alloy, Journal of Biomedical Materials Research, 34(2) (1997), 157–163
  11. Sims C.T, Hagel W., Stoloff N., The Superalloys II: High temperature materials for aerospace and industrial power, 2nd ed. New York: Wiley & Sons, (1987)
  12. Ramírez V.L.E., Castro R.M., Herrera T.M., García L.C.V., Almanza C.E., Cooling rate and carbon content effect on the fraction of secondary phases precipitate in as-cast microstructure of ASTM F75 alloy, J Material Process Technology, 209(4) (2009) 1681–1687
  13. Rosenthal R., Cardoso B.R., Bott I.S., Paranhos