Effect of tungsten disilicide addition on tungsten boride based composites produced by milling-assisted pressureless sintering

Sayfa
42–50
Yayın Tarihi
2018-03-26
DOI
—
🏛️Bu makalenin bibliyografik verileri ve tam metin bağlantısı DergiPark üzerinden sağlanmıştır.
DergiPark Kaydı ↗
✨

Yapay Zeka Hızlı Bakış & Çıkarımlar

AI Insight
⚡ TL;DR(1 Cümlede Hızlı Çıkarım)

The results showed that the highest density, microhardness and oxidation stability values amongst the fabricated composites were obtained for the dry milled and sintered WB-20 wt.% WSi2 sample.

📌 3 Maddede Bu Makale

🎯
Amaç & Hipotez:In this study, tungsten boride (WB and W2B) based composites with various amounts of tungsten disilicide (WSi2) addition were fabricated by using a combined method of mechanical milling (MM), cold isostatic pressing (CIP) and pressureless sintering (PS).
📊
Temel Bulgular & Veri:MM was conducted for 4 h in ethanol (wet milling) and Argon atmosphere (dry milling) using a high-energy ball mill.
💡
Sonuç & Katkı:The results showed that the highest density, microhardness and oxidation stability values amongst the fabricated composites were obtained for the dry milled and sintered WB-20 wt.% WSi2 sample.
🔬Tür:Araştırma Makalesi
📍Kapsam:2 sample
⚙️Değişkenler:Tungsten boride · tungsten disilicide · pressureless sintering

Abstract

In this study, tungsten boride (WB and W2B) based composites with various amounts of tungsten disilicide (WSi2) addition were fabricated by using a combined method of mechanical milling (MM), cold isostatic pressing (CIP) and pressureless sintering (PS). MM was conducted for 4 h in ethanol (wet milling) and Argon atmosphere (dry milling) using a high-energy ball mill. WSi2 was used with different amounts (0, 5, 10 and 20 wt.%) in order to investigate its effect on the resultant products. MM’d powders were compacted using CIP under a pressure of 450 MPa, and were consecutively sintered at 1600 °C for 2 h and 1770 °C for 2 h under Ar atmosphere. Compositional, physical and microstructural characterizations of the samples were performed using stereo and optical microscopes, X-ray diffractometer, TOPAS software, scanning electron microscope coupled with an energy-dispersive spectrometer, particle size analyzer and gas pycnometer. Sintered products were also characterized in terms of Archimedes density and Vickers microhardness. Moreover, the oxidation studies of the samples were performed at 500 and 1000 °C via thermogravimetric analyzer. The results showed that the highest density, microhardness and oxidation stability values amongst the fabricated composites were obtained for the dry milled and sintered WB-20 wt.% WSi2 sample.

🔖

Bu Makaleye Atıf Yap

Ovalı, D., Ağaoğulları, D., Gökçe, H., Öveçoğlu, M. L. (2018). Effect of tungsten disilicide addition on tungsten boride based composites produced by milling-assisted pressureless sintering. Bor Dergisi, Cilt: 3 - Sayı: 1, 42–50. https://ajindex.com/articles/252076

📄 Tam Metin PDF Okuyucu

📄

PDF görüntüleyici hazırlanıyor...

Kaynakça (14)

  1. Weimer A.W., ed., Carbide, Nitride and Boride Materials Synthesis and Processing, 1st edition, Chapman & Hall, London, 1996. doi:10.1007/978-94-009-0071-4
  2. Ramberg C.E., Beatrice P., Kurokawa K., Worrell W.K., High temperature oxidation behavior of structural silicides, 21st Annual Cocoa Beach Conference And Exposition on Composites, Advanced Ceramics, Materials and Structures, 12-16 January, 1993
  3. Suryanarayana C., Mechanical alloying and milling, Prog. Mater. Sci., 46, 1–184, 2001. doi:10.1016/S0079-6425(99)00010-9
  4. Guo S.Q., Densification of ZrB2-based composites and their mechanical and physical properties: A review, J. Eur. Ceram. Soc., 29, 995–1011, 2009. doi:10.1016/j.jeurceramsoc.2008.11.008
  5. Murthy T.S.R.C., Sonber J.K., Sairam K., Bedse R.D., Chakarvartty J.K., Development of refractory and rare earth metal borides & carbides for high temperature applications, Mater. Today Proc., 3, 3104–3113, 2016. doi:10.1016/j.matpr.2016.09.026
  6. Kainer K.U., High temperature ceramic matrix composites, 1st edition, Wiley-VCH Verlag GmbH & Co. KGaA, Weinheim, 2006. doi:10.1002/3527605622.fmatter
  7. Silvestroni L., Meriggi G., Sciti D., Oxidation behavior of ZrB2 composites doped with various transition metal silicides, Corros. Sci., 83, 281–291, 2014. doi:10.1016/j.corsci.2014.02.026
  8. Predel B., B-W (Boron-Tungsten), B-Ba–C-Zr, Springer-Verlag, Berlin/Heidelberg, 1992. doi:10.1007/10040476_402
  9. Itoh H., Matsudaira T., Naka S., Hamamoto H., Obayashi M., Formation process of tungsten borides by solid state reaction between tungsten and amorphous boron, J. Mater. Sci., 22, 2811–2815, 1987. doi:10.1007/BF01086475
  10. Li Q., Zhou D., Zheng W., Ma Y., Chen C., Global structural optimization of tungsten borides, Phys. Rev. Lett., 110, 136-403, 2013. doi:10.1103/PhysRevLett.110.136403
  11. Kiessling R., The borides of some transition elements, J. Electrochem. Soc., 98 166–170, 1951. doi:10.1149/1.2778125
  12. Brewer L., Sawyer D.L., Templeton D.H., Dauben C.H., A study of the refractory borides, J. Am. Ceram. Soc., 34 173–179, 1951. doi:10.1111/j.1151-2916.1951.tb11631.x
  13. Barış M., Şimşek T., Gökmeşe H., Akkurt A., Characterization of W2B nanocrystals synthesized by mechanochemical method, J. Boron., 1, 45–51, 2016
  14. Petrovic J.J., High temperature structural silicides, 21st Annual Cocoa Beach Conference and Exposition on Compo