AI InsightConclusion The compositional structure of the composite material and the photoinitiator mechanism used are directly related to the formation of its mechanical properties.
📌 3 Maddede Bu Makale
Abstract
Aim This study aims to comparatively investigate the color stability and microhardness values of dental composites with different photoinitiators. Material and method In the study, Ivoclar Tetric N-Ceram, Dentac Parion, and FGM Llis composites were used. A total of 30 composite discs were evenly divided for surface microhardness and ΔE measurements. Each subgroup contained 5 composite discs (Diameter: 5 mm, Thickness: 2 mm). Before the experimental procedures, all composite discs were aged in a coffee solution for one week. Surface microhardness was measured using the Vickers Hardness Test device, while color stability was assessed with a spectrophotometer. One-way ANOVA and Two-Way Repeated Measures ANOVA with Bonferroni-adjusted pairwise comparisons were applied. Results No statistically significant difference was observed among the three dental composite groups in terms of color stability (p > 0.05). However, their color stability performance ranked from highest to lowest as follows: Llis (3.13 ± 0.42) > Parion (2.76 ± 0.57) > Tetric N-Ceram (2.70 ± 0.76). In contrast, a statistically significant difference was detected among the groups regarding surface microhardness (p < 0.05). Llis exhibited significantly higher values compared to Tetric N-Ceram and Parion (p < 0.05). Conclusion The compositional structure of the composite material and the photoinitiator mechanism used are directly related to the formation of its mechanical properties.