The effect of relative humidity and moisture to the durability of spruce and laminated timber

Sayfa
103–110
DOI
—
🏛️Bu makalenin bibliyografik verileri ve tam metin bağlantısı DergiPark üzerinden sağlanmıştır.
DergiPark Kaydı ↗
✨

Yapay Zeka Hızlı Bakış & Çıkarımlar

AI Insight
⚡ TL;DR(1 Cümlede Hızlı Çıkarım)

The paper presents experimentally and theoretically approach to the effect of relative humidity and moisture to the durability of massive spruce and spruce laminated timber during to drying and wetting exposure.

📌 3 Maddede Bu Makale

🎯
Amaç & Hipotez:Wood is a hygroscopic material.
📊
Temel Bulgular & Veri:Material properties are affected by the hygro-scopicity of wood; for example, the strength value decreases with increasing mois-ture content of wood.
💡
Sonuç & Katkı:The paper presents experimentally and theoretically approach to the effect of relative humidity and moisture to the durability of massive spruce and spruce laminated timber during to drying and wetting exposure.
🔬Tür:Araştırma Makalesi
📍Kapsam:Genişletilmiş Akademik Örneklem
⚙️Değişkenler:Alan Parametreleri

Özet

Wood is a hygroscopic material. Material properties are affected by the hygro-scopicity of wood; for example, the strength value decreases with increasing mois-ture content of wood. Wood in the living tree generally has a moisture content (MC) of 30% or greater. The cell wall is fully saturated. After the tree is felled, the green wood is exposed to atmospheric conditions. It loses water until it comes to an adequately low moisture content to be at equilibrium with the surrounding atmosphere. This is called equilibrium moisture content (EMC) which is approxi-mately proportional to the relative atmospheric humidity (RH). Also, EMC varies with the kind and distribution of cell-wall constituents, different wood species, af-fected by temperature, between heartwood and sapwood, extractives, previous ex-posure history and mechanical stress. The EMC decreases with decreasing relative humidity, also, increases with the increasing relative humidity of the surrounding air at a constant temperature. The important point that the EMC at a given rel-ative humidity is not constant. It is increased or decreased to reach equilibrium depends on the level of moisture in the timber. The paper presents experimentally and theoretically approach to the effect of relative humidity and moisture to the durability of massive spruce and spruce laminated timber during to drying and wetting exposure.

🔖

Bu Makaleye Atıf Yap

KARAGÜLER, M. E., KAYA, G. (2017). The effect of relative humidity and moisture to the durability of spruce and laminated timber. A|Z ITU Mimarlık Fakültesi Dergisi, Cilt: 14 - Sayı: 1, 103–110. https://ajindex.com/articles/145556

📄 Tam Metin PDF Okuyucu

📄

PDF görüntüleyici hazırlanıyor...

Kaynakça (13)

  1. Aicher, S., Langer, G. L. (2005). Ef-fect of Lamination Anisotropy and Lay up in Glued Laminated Timber. Journal of Structural Engineering, 131, 1095-1103.
  2. Angst, V. (2012). Moisture Induced Stresses in Glulam; Effect of Cross Sec-tion Geometry and Screw Reinforce-ment. Norwegian University of Science and Technology Faculty of Engineering Science and Technology Department of Structural Engineering. Norway. Angst, V., Malo, K. A. (2010). Mois-ture Induced Stresses Perpendicular to the Grain Glulam: Review and Eval-uation of the Relative Importance of Models and Parameters. Department of Structural Engineering, NTNU Nor-wegian University of Science and Tech-nology. Holzforschung, 64(5), 609-617.
  3. Angst, V., Malo, K. A. (2012). The Effect of Climate Variations on Glu-lam –An Experimental Study. Europe-an Journal of Wood and Wood Prod-ucts,70(5), 603-613.
  4. Astrup, T., Clorius, C. O., Damkilde, L., Hoyfmeyer, P. (2006). Size effect of Glulam Beams in Tension Perpendicu-lar to Grain. Wood Science Technolo-gy, 41, 361-372.
  5. Breyer, D. E., Fridley, K. J., Cobeen, K. E., Pollock, D. G. (2005).
  6. Design of Wood Structures, ASS/LRFD. United States of America: McGraw-Hill. Fragiacomo, M., Fortino, S., Tononi, D., Usardi, I., Toratti, T. (2011). Mois-ture Induced Stresses Perpendicular to Grain in Cross-Section of Timber Members Exposed To Different Cli-mates. Elsevier, 33(11), 3071-3078.
  7. Frese, M., Blab, H. J. (2009). Bending Strength of Spruce Glulam.European Journal of Wood and Wood Products, 67(3), 277-286.
  8. Frese, M., Camberg, M. E., Blab, H. J., Glos, P.(2012). Compressive Strength of Spruce Glulam. European Journal of Wood and Wood Products, 70(6), 801-809.
  9. Gereke, T., Niemz, P. (2009). Mois-ture-Induced Stresses in Spruce Cross-Laminated. Engineering Struc-tures, 32(2), 600-606.
  10. Haglund, M. (2010). Parameter Influence on Moisture Induced Ei-gen-stresses in Timber. European Jour-nal of Wood and Wood Products, 68 (4), 397-406.
  11. Issa, C. A., Kmeid, Z. (2005). Ad-vanced Wood Engineering: Glulam Beams. Construction and Building Materials,Elsevier, 19 (2), 99-106.
  12. Jönsson, J., Thelandersson, S. (2003). The Effect of Moisture Gradients on Tensile Strength Perpendicular to Grain in Glulam. European Journal of Wood and Wood Products, 61(5), 342-348.
  13. Kollmann, F. P., Kuenzi, E. W., Stamm, A. J. (1975). Principles of Wood Science and Technology II, Wood-Based Materials. Berlin: Spring-er-Verlag. Pecenkol, R., Hozjan, T., Pazlar, T., Turk, G. (2012). Experimental and Nu-merical A