Dergiler / Tekstil ve Konfeksiyon / 2017 / Volume: 27 Issue: 4

EXTRACTION OF DISCARDED CORN HUSK FIBERS AND ITS FLAME RETARDED COMPOSITES

Sayfa
—
Yayın Tarihi
2017-12-27
DOI
—
🏛️Bu makalenin bibliyografik verileri ve tam metin bağlantısı DergiPark üzerinden sağlanmıştır.
DergiPark Kaydı ↗
✨

Yapay Zeka Hızlı Bakış & Çıkarımlar

AI Insight
⚡ TL;DR(1 Cümlede Hızlı Çıkarım)

Discarded corn husk fibers/ polylactic acid composites containing ammonium polyphosphate and pentaerythritol as flame

📌 3 Maddede Bu Makale

🎯
Amaç & Hipotez:Discarded corn husk fibers/ polylactic acid composites containing ammonium polyphosphate and pentaerythritol as flame
📊
Temel Bulgular & Veri:Discarded corn husk fibers/ polylactic acid composites containing ammonium polyphosphate and pentaerythritol as flame
💡
Sonuç & Katkı:Discarded corn husk fibers/ polylactic acid composites containing ammonium polyphosphate and pentaerythritol as flame
🔬Tür:Research Article
📍Kapsam:Genişletilmiş Akademik Örneklem
⚙️Değişkenler:Discarded corn husk · flame retardant treatment · polylactic acid

Özet

Discarded corn husk fibers/ polylactic acid composites containing ammonium polyphosphate and pentaerythritol as flame

Abstract

Discarded corn husk fibers/ polylactic acid composites containing ammonium polyphosphate and pentaerythritol as flame

🔖

Bu Makaleye Atıf Yap

Lv, L., Bi, J., Ye, F., Qıan, Y., Zhao, Y., Chen, R., Su, X. (2017). EXTRACTION OF DISCARDED CORN HUSK FIBERS AND ITS FLAME RETARDED COMPOSITES. Tekstil ve Konfeksiyon, Volume: 27 Issue: 4. https://ajindex.com/articles/1111386

📄 Tam Metin PDF Okuyucu

📄

PDF görüntüleyici hazırlanıyor...

Kaynakça (38)

  1. Ren, Z.J., Gu. M.D., 2005, "Comprehensive utilization of crop straw and circular economy.", Journal of Anhui agricultural science, Vol. 33, pp: 2105- 2106
  2. Liang, C.Q., Li, L.,2003, "Preparation of carboxymethyl cellulose with shuck of corn.", Technology and development of chemical industry, Vol.32, pp:8-9
  3. Hu,Y.B., Wang, Z., 2006, "Effects of different bio-preparations on the composition and functional properties of corn bran dietary fibers.", Food science, Vol.27, pp:96-99
  4. Cui,L.F., Wang, S., 2002, "Corn skin pigment extraction and its stability study.", Food science, Vol.23, pp:66-70
  5. Ma, B.X., 2003, "Fabrication of carpet made by corn husk.", Popular business, Vol.6, pp:49
  6. Xue, Z.Y., 2003, "Starch extraction of corn byproducts.", Farm products prcessing, Vol.8, pp:19
  7. Zhao, J.Q., 2011,"The study of the cellulose fiber extracted from corn husk.", Journal of textile dyeing and finishing, Vol.2, pp:12-16
  8. Wang, S.Y., 2004,"The development trend of comprehensive utilization of maize straw.", Jilin Journal of animal husbandry and veterinary medicine, Vol.1, pp:26-27
  9. Zhang, M., Cui, C.N., 2008,"Analysis of the factors influencing degradability and degradation mechanism of polylactic acid.", Packaging engineering, Vol.29, pp:16-46
  10. Zhang, J., Li, G.P., 2006,"Research on manufacturing environmentally friendly and fire-retardant medium-density fiberboard.", China wood-based panels, Vol.13, pp:26-28
  11. Feng,X.W., Wu, X.Q., Qiu, G.X., 2002,"Research on the shaping process and flame retardant property of the recycled waste textile material.", Journal of Tianjin institute of textile science and technology, Vol.21, pp:18-21
  12. Liang, S.J., Xu, H.S., 2009,"Halogen-free flame retardant polypropylene composites.", Plastic, Vol.20, pp:19-21
  13. Wei, P., Wang, J.Q., 2003, "The TGA/XPS study on the synergy of 4A zeolites in the intumescent flame retardant APP /PER.", Polymeric materials science and engineering, Vol.12, pp:179-181
  14. Reti, C.,Casetta, M., 2008,"Flammability properties of intumescent PLA including starch and lignin.", Polym Adv Tech, Vol.19, pp:628-635
  15. Li, S.M., Yuan, H., 2009, "Flame retardancy and anti-dripping effects of intumescent flame retardant incorporating mont-morillomite on poly(1actic acid).", Polym Adv Tech,Vol.20, pp:1114-1120
  16. Xu,J.Y., Guo,S.Y., 2006, "Studies on fire-retardant and smoke-suppressant effect of zeolites on PVC.", Polyvinyl chloride, Vol.6, pp:22 -25
  17. Yang, Y.F., Liu, M.J., Tian,L.B., 2003,"Study on PE/Graphite flame retardation composites.", China plastics,Vol.17, pp:43-45
  18. Ling, Q.F., Li, X.G., 2013,"Study on properties of PLA/BF/ATH flame retardant composites.", Plastics science and technology, Vol.41, pp:80-84 19. Jiang, S.J., Shao, J., Li, Z.Z., 2005, "Investigation of hemp's properties and organisms enzyme degumming process.", Journal of Lanzhou University of Technology, Vol.31, pp:69-72 20. He, X., Wang, D.F., 2015, "Tensile property of corn stalk rind based on analysis of fiber morphology.", Transactions of the Chinese Society of Agricultural Engineering, Vol.31, pp:92-98
  19. Tan, Z.H., Wu, F., 2001, "Effects of Blowing Agents on Adsorption Performance of Zeolite", Materials Review, Vol.15, pp:66-68
  20. Ren, Z.J., Gu. M.D., 2005, "Comprehensive utilization of crop straw and circular economy.", Journal of Anhui agricultural science, Vol. 33, pp: 2105- 2106
  21. Liang, C.Q., Li, L.,2003, "Preparation of carboxymethyl cellulose with shuck of corn.", Technology and development of chemical industry, Vol.32, pp:8-9
  22. Hu,Y.B., Wang, Z., 2006, "Effects of different bio-preparations on the composition and functional properties of corn bran dietary fibers.", Food science, Vol.27, pp:96-99
  23. Cui,L.F., Wang, S., 2002, "Corn skin pigment extraction and its stability study.", Food science, Vol.23, pp:66-70
  24. Ma, B.X., 2003, "Fabrication of carpet made by corn husk.", Popular business, Vol.6, pp:49
  25. Xue, Z.Y., 2003, "Starch extraction of corn byproducts.", Farm products prcessing, Vol.8, pp:19
  26. Zhao, J.Q., 2011,"The study of the cellulose fiber extracted from corn husk.", Journal of textile dyeing and finishing, Vol.2, pp:12-16
  27. Wang, S.Y., 2004,"The development trend of comprehensive utilization of maize straw.", Jilin Journal of animal husbandry and veterinary medicine, Vol.1, pp:26-27
  28. Zhang, M., Cui, C.N., 2008,"Analysis of the factors influencing degradability and degradation mechanism of polylactic acid.", Packaging engineering, Vol.29, pp:16-46
  29. Zhang, J., Li, G.P., 2006,"Research on manufacturing environmentally friendly and fire-retardant medium-density fiberboard.", China wood-based panels, Vol.13, pp:26-28
  30. Feng,X.W., Wu, X.Q., Qiu, G.X., 2002,"Research on the shaping process and flame retardant property of the recycled waste textile material.", Journal of Tianjin institute of textile science and technology, Vol.21, pp:18-21
  31. Liang, S.J., Xu, H.S., 2009,"Halogen-free flame retardant polypropylene composites.", Plastic, Vol.20, pp:19-21
  32. Wei, P., Wang, J.Q., 2003, "The TGA/XPS study on the synergy of 4A zeolites in the intumescent flame retardant APP /PER.", Polymeric materials science and engineering, Vol.12, pp:179-181
  33. Reti, C.,Casetta, M., 2008,"Flammability properties of intumescent PLA including starch and lignin.", Polym Adv Tech, Vol.19, pp:628-635
  34. Li, S.M., Yuan, H., 2009, "Flame retardancy and anti-dripping effects of intumescent flame retardant incorporating mont-morillomite on poly(1actic acid).", Polym Adv Tech,Vol.20, pp:1114-1120
  35. Xu,J.Y., Guo,S.Y., 2006, "Studies on fire-retardant and smoke-suppressant effect of zeolites on PVC.", Polyvinyl chloride, Vol.6, pp:22 -25
  36. Yang, Y.F., Liu, M.J., Tian,L.B., 2003,"Study on PE/Graphite flame retardation composites.", China plastics,Vol.17, pp:43-45
  37. Ling, Q.F., Li, X.G., 2013,"Study on properties of PLA/BF/ATH flame retardant composites.", Plastics science and technology, Vol.41, pp:80-84 19. Jiang, S.J., Shao, J., Li, Z.Z., 2005, "Investigation of hemp's properties and organisms enzyme degumming process.", Journal of Lanzhou University of Technology, Vol.31, pp:69-72 20. He, X., Wang, D.F., 2015, "Tensile property of corn stalk rind based on analysis of fiber morphology.", Transactions of the Chinese Society of Agricultural Engineering, Vol.31, pp:92-98
  38. Tan, Z.H., Wu, F., 2001, "Effects of Blowing Agents on Adsorption Performance of Zeolite", Materials Review, Vol.15, pp:66-68.