Journals / Engineering Sciences / 2011 / Cilt: 6 Sayı: 4

KÜKÜRT ATIKLARI (FGD)YLE HAZIRLANAN ÇYMENTO HAMURUNUN POROZYTE VE BO?LUK ORANI DE?ERLERY ÜZERYNE ETKYLERY

INFLUENCE OF INCORPORATING FLUE GAS DESULPHURISATION (FGD) RESIDUES ON POROSITY AND PORE SIZE DISTRIBUTION OF CEMENT PASTE

Pages
1676–1682
Publication Date
2011-05-01
🏛️Bibliographic metadata and full text access for this article are provided via DergiPark.
DergiPark Record ↗
✨

AI Summary & Key Takeaways

AI Insight
⚡ TL;DR(Too Long; Didn't Read)

Increasing the amount of gypsum up does not change the pore volume, however, there is tendency of obtaining coarser pore structure in the presence of gypsum.

📌 3 Key Takeaways

🎯
Objective & Hypothesis:This paper reports results on the porosity and pore size distribution of cement paste containing varying amounts of simulated desulphurised waste (SDW).
📊
Key Findings & Data:The water to binder ratio was 0.5.
💡
Conclusion & Impact:Increasing the amount of gypsum up does not change the pore volume, however, there is tendency of obtaining coarser pore structure in the presence of gypsum.
🔬Design:Research Article
📍Scope:Comprehensive Sample
⚙️Variables:Desulphurised Waste · FGD Waste · Fly Ash

Abstract

This paper reports results on the porosity and pore size distribution of cement paste containing varying amounts of simulated desulphurised waste (SDW). The water to binder ratio was 0.5. The binder consists of cement and SDW. The SDW is a combination of fly ash and gypsum ranging from 0-100%. Cement in the pastes was partially replaced with 25% SDW (by weight). The porosity and pore size distribution of cement pastes at 90 days of curing is reported. Increasing the amount of gypsum up does not change the pore volume, however, there is tendency of obtaining coarser pore structure in the presence of gypsum.

Özet

This paper reports results on the porosity and pore size distribution of cement paste containing varying amounts of simulated desulphurised waste (SDW). The water to binder ratio was 0.5. The binder consists of cement and SDW. The SDW is a combination of fly ash and gypsum ranging from 0-100%. Cement in the pastes was partially replaced with 25% SDW (by weight). The porosity and pore size distribution of cement pastes at 90 days of curing is reported. Increasing the amount of gypsum up does not change the pore volume, however, there is tendency of obtaining coarser pore structure in the presence of gypsum.

🔖

Cite This Article

Khatib, J. M., Wright, L., Mangat, P. S. (2011). KÜKÜRT ATIKLARI (FGD)YLE HAZIRLANAN ÇYMENTO HAMURUNUN POROZYTE VE BO?LUK ORANI DE?ERLERY ÜZERYNE ETKYLERY. Engineering Sciences, Cilt: 6 Sayı: 4, 1676–1682. https://doi.org/10.12739/nwsaes.v6i4.5000066977

📄 Full Text PDF Viewer

📄

PDF görüntüleyici hazırlanıyor...