Journals / Konya Journal of Engineering Sciences / 2021 / Cilt: 9 Sayı: 4

Production and Characterization of UHMWPE - HAp Composites for HIP Prosthesis

KALÇA PROTEZİ İÇİN UHMWPE – HAp KOMPOZİTLERİNİN ÜRETİMİ VE KARAKTERİZASYONU

Pages
1013–1024
Publication Date
2021-12-04
DOI
—
🏛️Bibliographic metadata and full text access for this article are provided via DergiPark.
DergiPark Record ↗
✨

AI Summary & Key Takeaways

AI Insight
⚡ TL;DR(Too Long; Didn't Read)

The melting temperatures of both the UHMWPE and the UHMWPE-HAp composites were determined to be approximately 140 °C by DSC analysis.

📌 3 Key Takeaways

🎯
Objective & Hypothesis:Most of the wear problems occur in hip prostheses because of long-term use in the liner (socket) part.
📊
Key Findings & Data:For this purpose, UHMWPE-HAp (hydroxyapatite) composites have been developed by reinforcing UHMWPE, which is used as hip prosthesis acetabular liner, by biomimetic HAp powders at a ratio of 1, 2, and 3% by weight.
💡
Conclusion & Impact:The melting temperatures of both the UHMWPE and the UHMWPE-HAp composites were determined to be approximately 140 °C by DSC analysis.
🔬Design:Research Article
📍Scope:Comprehensive Sample
⚙️Variables:UHMWPE – HAp Kompozitleri · Sertlik · DSC

Abstract

Most of the wear problems occur in hip prostheses because of long-term use in the liner (socket) part. In this study, the aim was to develop the acetabular liner part of total hip replacement implants. For this purpose, UHMWPE-HAp (hydroxyapatite) composites have been developed by reinforcing UHMWPE, which is used as hip prosthesis acetabular liner, by biomimetic HAp powders at a ratio of 1, 2, and 3% by weight. The morphology of the samples was examined by SEM. SEM-EDS was used for elemental analysis. Phase analysis was carried out by XRD technique. According to the experimental results, HAp addition was detected when the reinforcement level was at least 2%. Hardness analyses were performed by Vickers indentation technique, and the highest hardness value of 5.28HV was obtained at 2% HAp reinforcement. All additive levels contributed positively to hardness values. The melting temperatures of both the UHMWPE and the UHMWPE-HAp composites were determined to be approximately 140 °C by DSC analysis.

Özet

Uzun süreli kullanım sonucunda kalça protezlerinde meydana gelen aşınma problemlerinin çoğu liner (yuva) kısmında gerçekleşmektedir. Bu çalışmada total kalça protez implantlarının asetabuler liner parçasının (kalça eklemi yuvası) geliştirilmesi hedeflenmiştir. Bu amaçla kalça protezi asetabuler liner olarak kullanılan Ultra Yüksek Molekül Ağırlıklı Polietilene (UHMWPE) ağırlıkça %1, 2 ve 3 oranında hidroksiapatit (HAp) tozları ilave edilerek UHMWPE-HAp toz karışımları hazırlanmıştır. Hazırlanan toz karışımları 200 °C’de 30 dakika boyunca 1 ton yük altında sıcak preslenerek UHMWPE-HAp kompozitleri üretilmiştir. Kompozit numunelerin morfolojisi SEM ile incelenmiş, elementel analiz için SEM-EDS kullanılmıştır. Faz analizi XRD ile gerçekleştirilmiştir. XRD analiz sonuçlarına göre takviye artışının %2’ye ulaşması ile HAp takviyesinin varlığı belirlenmiştir. Kompozitlerin kırık yüzey incelemelerinde HAp partiküllerinin matris içerisinde homojen olarak dağıldığı görülmüştür. Sertlik analizleri Vickers indentasyon tekniği ile gerçekleştirilmiş olup; en yüksek sertlik değeri %2 HAp takviyeli UHMWPE-HAp kompozitinde 5,28HV olarak elde edilmiştir. Tüm katkı oranları, kompozitin sertlik değerlerinde artışa neden olmuştur. DSC analizi ile hem UHMWPE numunesinin hem de UHMWPE kompozitlerinin ergime sıcaklıkları yaklaşık 140 C olarak belirlenmiştir.

🔖

Cite This Article

EFE, G., YENER, T. (2021). Production and Characterization of UHMWPE - HAp Composites for HIP Prosthesis. Konya Journal of Engineering Sciences, Cilt: 9 Sayı: 4, 1013–1024. https://ajindex.com/articles/909056

📄 Full Text PDF Viewer

📄

PDF görüntüleyici hazırlanıyor...

References (10)

  1. Annas B., A.,et al. 2018, “Tribological investigations of UHMWPE nanocomposites reinforced with three different organo-modified clays”. Polymer Composites, Vol. 39, No: 7, pp. 2224–31. Antônio E., C., M., et al. 2016, “Calcium carbonate hybrid coating promotes the formation of biomimetic hydroxyapatite on titanium surfaces”. Applied Surface Science, Vol. 370, pp. 459–68.
  2. Balani, K., et al. 2014, “Biosurfaces: Amaterials Science and Engineering Perspective”, http://www.ncbi.nlm.nih.gov/pubmed/17343486.
  3. Balasundaram, G., et al. 2006,“ Using hydroxyapatite nanoparticles and decreased crystallinity to promote osteoblast adhesion similar to functionalizing with RGD”. Biomaterials, Vol 27, No: 14, pp. 2798–805.
  4. Çelebi Efe, G., et al. 2021, “Characterization of UHMWPE- HAp coating produced by dip coating method on Ti6Al4V alloy”. Surface and Coatings Technology, Vol. 418, pp. 127091. Dastjerdi, R., ve Montazer, M., 2010, “Colloids and Surfaces B: Biointerfaces A review on the application of inorganic nano-structured materials in the modification of textiles: Focus on anti-microbial properties”. Colloids and Surfaces B: Biointerfaces, Vol. 79, No: 1, pp. 5–18.
  5. Demirel, B., et al. 2011, “Crystallization Behavior of PET Materials”. BAÜ Fen Bil. Enst. Dergisi Cilt, Vol. 13, No:1, pp. 26–35.
  6. Edward, B., et al. 2020, “Threshold for Computer- and Robot-Assisted Knee and Hip Replacements in the English National Health Service”. Value in Health, Vol. 23, No:6, pp. 719–26.
  7. Gaot, P., Mackley M. R., 1992, Surface treatment of ultra high molecular weight polyethylene to enhance adhesion and conductivity properties*. Vol. 33, No: 19, pp. 4075–80.
  8. Gong, S., et.al., 2008, “Zirconium complexes with versatile b -diketiminate ligands: Synthesis, structure, and ethylene polymerization”. Journal of Organometallic Chemistry, Vol. 693, No:23, pp. 3509–18.
  9. Hussain, O., 2021, “Tribological performance of biomedical grade UHMWPE/nano-Al2O3/Vitamin-C hybrid composite for cartilage replacements”. Materials Letters, Vol. 291, Elsevier B.V., pp. 129515. Kang, X.,, 2016, “Mechanical properties study of micro- and nano-hydroxyapatite reinforced ultrahigh molecular weight polyethylene composites”. Journal of Applied Polymer Science, Vol. 133, No:3, Kilgour, Ã, A., Elfick, A., 2009, “Tribology International Influence of crosslinked polyethylene structure on wear of joint replacements”. Tribiology International, Vol. 42, No:11–12, Elsevier, pp. 1582–94.
  10. Kong, Y., Hay, J. N., 2002, The measur