FARKLI HASSASİYET GİDERİCİ AJANLARIN TEK AŞAMALI BİR SELF-ETCH ADEZİV SİSTEMİN DENTİNE MAKASLAMA BAĞLANMA DAYANIMINA ETKİSİ

Pages
213–219
Publication Date
2019-03-22
DOI
—
🏛️Bibliographic metadata and full text access for this article are provided via DergiPark.
DergiPark Record ↗
✨

AI Summary & Key Takeaways

AI Insight
⚡ TL;DR(Too Long; Didn't Read)

Conclusion: Considering the all-in-one adhesive system used in this study, it can be concluded that, the desensitizers used in this study have no negative effect on shear bonding strength to dentin.

📌 3 Key Takeaways

🎯
Objective & Hypothesis:Amaç: Bu çalışmanın amacı, üç farklı hassasiyet giderici uygulamasını takiben tek aşamalı self-etch adeziv sistemin, dentine bağlanmada makaslama dayanımı üzerine etkisinin karşılaştırılmasıdır.
📊
Key Findings & Data:Gereç ve Yöntem: Bu çalışmada 40 adet çekilmiş, sağlam, insan küçük azı dişi kullanılmıştır.
💡
Conclusion & Impact:Conclusion: Considering the all-in-one adhesive system used in this study, it can be concluded that, the desensitizers used in this study have no negative effect on shear bonding strength to dentin.
🔬Design:Research Article
📍Scope:40 adet
⚙️Variables:Dentin hassasiyeti giderici ajan · makaslama dayanımı · Adeziv Sistem

Özet

Amaç: Bu çalışmanın amacı, üç farklı hassasiyet giderici uygulamasını takiben tek aşamalı self-etch adeziv sistemin, dentine bağlanmada makaslama dayanımı üzerine etkisinin karşılaştırılmasıdır. Gereç ve Yöntem: Bu çalışmada 40 adet çekilmiş, sağlam, insan küçük azı dişi kullanılmıştır. Dişlerin okluzal yüzeyleri dentin tamamen ortaya çıkacak şekilde uzaklaştırılmış ve her örnekten 2 mm kalınlığında okluzal kesitler elde edilmiştir. Tüm örnekler özel olarak hazırlanmış akrilik bloklara gömüldükten sonra, yüzeyleri sırasıyla 320, 600, 800, 1200 gren kalınlığında silikon karbid zımparalar ile parlatılmıştır. Örnekler rasgele 4 gruba ayrılmıştır (n=10). Kontrol grubu dışında, tüm gruplarda hassasiyet gidericiler üretici firmaların talimatları doğrultusunda uygulanmıştır. Grup 1: Bifluorid 12 (Voco GmbH, Cuxhaven, Almanya); Grup 2: Desen (Spident Co., LTD. Incheon, Kore); Grup 3: Gluma (Heraeus Kulzer GmbH, Hanau, Almanya); Grup 4: Kontrol. Kontrol grubuna herhangi bir hassasiyet giderici ajan uygulanmamıştır. Tüm gruplara adeziv ajan olarak Clearfil S3 (Kuraray Noritake Dental Inc. Okayama, Japonya) uygulanmış ve daha sonra 2 mm çap ve 3 mm yüksekliğinde polietilen tüpler yardımıyla kompozit rezin dolgu (3M ESPE FiltekTM Z250 St. Paul, MN, ABD) yapılmıştır. Örnekler 37°C’de, %100 nemlilikte, 24 saat bekletilmiştir. Makaslama dayanım testi universal test cihazı (Shimadzu Autograph, AGS-J 5kN, Shimadzu Corporation, Tokyo, Japonya) kullanılarak 1mm/dak çapraz hızda gerçekleştirilmiştir. İstatistiksel analizler için Tek Yönlü Varyans Analizi kullanılmıştır. Bulgular: Grup 1 ve kontrol grubu en yüksel makaslama dayanım değerleri göstermesine rağmen gruplar arasında anlamlı bir fark bulunamamıştır (p>0.05). Sonuç: Kullanılan tek aşamalı adeziv sistem göz önünde bulundurulduğunda, bu çalışmada kullanılan hassasiyet gidericilerin dentine olan bağlanmada makaslama dayanımı üzerinde negatif bir etkisinin bulunmadığı sonucuna varılabilir. Anahtar Kelimeler: Dentin hassasiyeti giderici ajan, makaslama dayanımı, Adeziv Sistem, Dentin. The Effect of Different desensitizing Agents on the Shear Bond Strength of a one-step Self-etch Adhesive System to dentin Aim: The purpose of this study was to compare the effect of a one-step self-etch adhesive system on the shear bond strength of dentin following three different dentin desensitizers’ applications. Materials and Methods: Forty extracted intact human premolars were used in this study. Occlusal surfaces of the teeth were removed so that the dentin was completely exposed and 2 mm thick occlusal slices were obtained from each sample. After all specimens were embedded in specially prepared acrylic blocks, surface polishing was carried out with silicon carbide papers at 320, 600, 800, 1200 grit, respectively. Specimens were divided randomly into 4 groups (n=10). Except the control group, in all groups the desensitizers were applied in accordance with the instructions of the manufacturer instructions. Group 1: Bifluorid 12 (Voco GmbH, Cuxhaven, Germany); Group 2: Desen (Spident Co., LTD. Incheon, Korea); Group 3: Gluma (Heraeus Kulzer GmbH, Hanau, Germany); Group 4: Control. No desensitizer was applied to the control group. All groups were treated with Clearfil S3 (Kuraray Noritake Dental Inc. Okayama, Japan) as an adhesive agent and then composite resin filler (3M ESPE Filtek Z250 St. Paul, MN, USA) with the help of 2 mm diameter and 3 mm height polyethylene tubing. The samples were incubated at 37 C°, 100% humidity for 24 hours. The shear bond strength test was performed at a cross speed of 1 mm/min using a universal testing machine (Shimadzu Autograph, AGS-J 5kN, Shimadzu Corporation, Tokyo, Japan). One way ANOVA was used for statistical analysis. Results: Although Group 1 and control group showed the highest shear bond strength values, no significant difference was found between the groups (p>0.05). Conclusion: Considering the all-in-one adhesive system used in this study, it can be concluded that, the desensitizers used in this study have no negative effect on shear bonding strength to dentin. Key Words: Dentin desensitizing agent; shear bond strength; Clearfil S3 Bond; Dentin bonding agents.

🔖

Cite This Article

OLCAY, K., EYÜBOĞLU, T. F. (2019). FARKLI HASSASİYET GİDERİCİ AJANLARIN TEK AŞAMALI BİR SELF-ETCH ADEZİV SİSTEMİN DENTİNE MAKASLAMA BAĞLANMA DAYANIMINA ETKİSİ. Current Research in Dental Sciences, Cilt: 29 Sayı: 2, 213–219. https://ajindex.com/articles/901034

📄 Full Text PDF Viewer

📄

PDF görüntüleyici hazırlanıyor...

References (16)

  1. Davari A, Ataei E, Assarzadeh H. [Dentin hypersensitivity: etiology, diagnosis and treatment; a literature review]. J Dent (Shiraz) 2013;14(3):136-45
  2. Gillam DG, Bulman JS, Eijkman MA, Newman HN. [Dentists’ perceptions of dentine hypersensitivity and knowledge of its treatment]. J Oral Rehabil 2002;29(3):219-25
  3. Yang H, Pei D, Chen Z, Lei J, Zhou L, Huang C. [Effects of the application sequence of calcium-containing desensitising pastes during etch-and-rinse adhesive restoration]. J Dent 2014;42(9):1115-23
  4. Brännström M, Åström A. [A study on the mechanism of pain elicited from the dentin]. J Dent Res 1964; Jul-Aug;43:619-25
  5. Ling TY, Gillam DG. [The effectiveness of desensitizing agents for the treatment of cervical dentine sensitivity (CDS)—a review]. J West Soc Periodontol Periodontal Abstr 1996;44(1):5-12
  6. Perdigao J, Lopes M. [Dentin bonding-Questions for the new millennium]. J Adhes Dent 1999;1(3):191-209
  7. Rosenthal MW. [Historic review of the management of tooth hypersensitivity]. Dent Clin North Am 1990;34(3):403-27
  8. Renton-Harper P, Midda M. [Nd:YAG laser treatment of dentinal hypersensitivity]. Br Dent J 1992;172(1):13-6
  9. Pashley EL, Tao L, Pashley DH. [Effects of oxalate on dentin bonding]. Am J Dent 1993;6(3):116-8
  10. Perdigao J, Van Meerbeek B, Lopes MM,Ambrose WW. [The effect of a re-wetting agent on dentin bonding]. Dent Mater 1999;15(4):282-95
  11. Xu J, Stangel I, Butler IS, & Gilson DF. [An FT-Raman spectroscopic investigation of dentin and collagen surfaces modified by 2-hydroxyethylmethacrylate]. J Dent Res 1997;76(1):596-601
  12. Van Meerbeek B, Yoshida Y, Lambrechts P, Vanherle G, Duke ES, Eick JD, et al. [A TEM study of two water-based adhesive systems bonded to dry and wet dentin]. J Dent Res 1998;77(1):50-9
  13. Sarac D, Kulunk S, Sarac YS, & Karakas O. [Effect of fluoride-containing desensitizing agents on the bond strength of resin-based cements to dentin]. J Appl Oral Sci 2009;17(5):495-500
  14. Itota T, Torii Y, Nakabo S, & Yoshiyama M. [Effect of fluoride application on tensile bond strength of selfetching adhesive systems to demineralized dentin]. J Prosthet Dent 2002;88(5):503-10
  15. Soeno K, Taira Y, Matsumura H, & Atsuta M. [Effect of desensitizers on bond strength of adhesive luting agents to dentin]. J Oral Rehabil 2001;28(12):1122-8
  16. Qin C, Xu J, & Zhang Y. [Spectroscopic investigation of the function of aqueous 2-hydroxyethylmethacrylate/ glutaraldehyde solution as a dentin desensitize