Journals / İleri Teknoloji Bilimleri Dergisi / 2017 / Cilt: 6 - Sayı: 3

EFFECT OF HEAT TREATMENT ON THE MECHANICAL PROPERTIES AND DIMENSIONAL STABILITY OF BEECH WOOD

ISIL İŞLEMİN KAYIN ODUNUN MEKANİK ÖZELLİKLERİ VE BOYUTSAL KARARLILIĞI ÜZERİNE ETKİSİ

Pages
820–830
Publication Date
2017-12-15
DOI
—
🏛️Bibliographic metadata and full text access for this article are provided via DergiPark.
DergiPark Record ↗
✨

AI Summary & Key Takeaways

AI Insight
⚡ TL;DR(Too Long; Didn't Read)

It was seen that a significant increase of dimensional stability and besides the color of samples was darken uniformly.

📌 3 Key Takeaways

🎯
Objective & Hypothesis:Thermal modification at different temperatures especially at high temperatures is an effective method to change chemical, physical, and mechanical properties of wood.
📊
Key Findings & Data:In this study, some mechanical and physical properties of heat treated beech (Fagus orientalis) wood at temperatures 170, 180, 190, and 212oC for 2 h with ThermoWood method were investigated.
💡
Conclusion & Impact:It was seen that a significant increase of dimensional stability and besides the color of samples was darken uniformly.
🔬Design:Research Article
📍Scope:Comprehensive Sample
⚙️Variables:Mekanik özellikler · Isıl işlem · Renk

Abstract

Thermal modification at different temperatures especially at high temperatures is an effective method to change chemical, physical, and mechanical properties of wood. In this study, some mechanical and physical properties of heat treated beech (Fagus orientalis) wood at temperatures 170, 180, 190, and 212oC for 2 h with ThermoWood method were investigated. The results were compared with oven-dried reference samples. Consequently, depending on the increase of heat treatment temperature, the bending strength was decreasing, the compression strength parallel to the grain and modulus of elasticity increased. Also, when the treatment temperature increased, equilibrium moisture content decreased. It was seen that a significant increase of dimensional stability and besides the color of samples was darken uniformly.

Özet

Farklı sıcaklıklarda özellikle yüksek sıcaklıklardaki termal modifikasyon odunun kimyasal, fiziksel ve mekanik özelliklerini değiştirmede etkili bir metottur. Bu çalışmada, ThermoWood metoduyla 170, 180, 190, ve 212 oC sıcaklıkta 2 saat süre ile ısıl işlem görmüş kayın odununun bazı mekanik ve fiziksel özellikleri araştırılmıştır. Sonuçlar tam kuru referans örnekler ile karşılaştırılmıştır. Sonuç olarak, ısıl işlem sıcaklığının artmasına bağlı olarak, eğilme direnci azalırken, liflere paralel basınç direnci ve elastikiyet modülü artmıştır. Ayrıca, işlem sıcaklığı yükseldikçe, denge rutubet miktarı azalmıştır. Boyutsal stabilizasyonda önemli ölçüde artış görülmüş ve bunun yanında odun örneklerinin rengi yeknesak bir şekilde koyulaşmıştır.

🔖

Cite This Article

KOL, H. Ş., KESKİN, S. A., VAYDOĞAN, K. G. (2017). EFFECT OF HEAT TREATMENT ON THE MECHANICAL PROPERTIES AND DIMENSIONAL STABILITY OF BEECH WOOD. İleri Teknoloji Bilimleri Dergisi, Cilt: 6 - Sayı: 3, 820–830. https://ajindex.com/articles/833781

📄 Full Text PDF Viewer

📄

PDF görüntüleyici hazırlanıyor...

References (16)

  1. Akyildiz, M. H., Ates, S., and Özdemir, H. (2009). Technological and chemical properties of heat-treated Anatolian black pine wood. African Journal of Biotechnology, 8(11)
  2. Bekhta, P., and Niemz, P. (2003). Effect of high temperature on the change in color, dimensional stability and mechanical properties of spruce wood.Holzforschung, 57(5), 539-546
  3. Bhuiyan, T. R., and Hirai, N. (2005). Study of crystalline behavior of heat-treated wood cellulose during treatments in water. Journal of Wood Science, 51(1), 42-47
  4. Boonstra, M. (2008). A two-stage thermal modification of wood. Ph.D. Thesis in Applied Biological Sciences: Soil and Forest management. Henry Poincare university- Nancy, France
  5. Boonstra, M. J., and Tjeerdsma, B. (2006). Chemical analysis of heat treated softwoods. Holz als Roh-und Werkstoff, 64(3), 204-211
  6. Boonstra, M. J., Van Acker, J., Tjeerdsma, B. F., and Kegel, E. V. (2007). Strength properties of thermally modified softwoods and its relation to polymeric structural wood constituents. Annals of forest science, 64(7), 679-690
  7. Burmester, A. (1975). The dimentional stabilization of wood. Holz als Roh-und Werkstoff. 33 (9), 333-335
  8. Cao, Y., Lu, J., Huang, R., and Jiang, J. (2012). Increased dimensional stability of Chinese through steam-heat treatment. European Journal of Wood and Wood Products, 70(4), 441-444
  9. Chang, C. I., and Keith, C. T. (1978). Properties of heat-darkened wood: II. Mechanical properties and gluability
  10. Esteves, B., Domingos, I., and Pereira, H. (2008). Pine wood modification by heat treatment in air. BioResources, 3(1), 142-154
  11. Esteves, B., Marques, A. V., Domingos, I., and Pereira, H. (2007b). Influence of steam heating on the properties of pine (Pinus pinaster) and eucalypt (Eucalyptus globulus) wood. Wood Science and Technology, 41(3), 193-207
  12. Feist, W. C., and Sell, J. (1987). Weathering behaviour of dimensionally stabilized wood treated by heating under pressure of nitrogen gas. Wood Fiber Sci, 19(2), 183-195
  13. Fengel, D. (1966). On the changes of the wood and its components within the temperature range up to 200 °C-Part III: Thermally and mechanically caused structural changes in spruce wood. Holz als Roh-und Werkstoff, 24(11). 529-536
  14. Fengel, D., and Wegener, G. (Eds.). (1983). Wood: chemistry, ultrastructure, reactions. Walter de Gruyter
  15. Finnish Thermo Wood Association. (2003).Thermo Wood Handbook. Helsinki, Finland
  16. Hill, C. A. (2007). Wood modification: