Journals / Turkish Journal of Physics / 2013 / Cilt: 37 - Sayı: 2

Effect of stepwise replacement of LiF by ZnO on structural and optical properties of LiF.B2O3 glasses

Pages
229–236
Publication Date
2013-02-01
DOI
—
🏛️Bibliographic metadata and full text access for this article are provided via DergiPark.
DergiPark Record ↗
✨

AI Summary & Key Takeaways

AI Insight
⚡ TL;DR(Too Long; Didn't Read)

A UV-visible study was carried out to calculate the optical band gap energy, EgIt was found that Egdecreased with increase in concentration of ZnO up to x = 15 and increased slightly for x 20 with the stepwise replacement of a nonoxide group (LiF) by an oxide group (ZnO).

📌 3 Key Takeaways

🎯
Objective & Hypothesis:Zinc fluoroborate glasses with compositions xZnO.(40 - x) LiF.60B2O3 (x = 0, 5, 10, 15, and 20) were synthesized by the melt-quench method.
📊
Key Findings & Data:A UV-visible study was carried out to calculate the optical band gap energy, EgIt was found that Egdecreased with increase in concentration of ZnO up to x = 15 and increased slightly for x 20 with the stepwise replacement of a nonoxide group (LiF) by an oxide group (ZnO).
💡
Conclusion & Impact:Theoretical optical basicity, Lambdath, decreased with decrease in concentration of LiF.
🔬Design:Research Article
📍Scope:Comprehensive Sample
⚙️Variables:Fluoroborate glasses · XRD · FTIR

Abstract

Zinc fluoroborate glasses with compositions xZnO.(40 - x) LiF.60B2O3 (x = 0, 5, 10, 15, and 20) were synthesized by the melt-quench method. The amorphous nature of the glassy samples was confirmed by XRD analysis. The nature of the bonds formed and the role of various species in the composition of the glasses were examined using FTIR spectroscopy. FTIR analysis showed shifting of an absorption band with the addition of ZnO. A UV-visible study was carried out to calculate the optical band gap energy, EgIt was found that Egdecreased with increase in concentration of ZnO up to x = 15 and increased slightly for x 20 with the stepwise replacement of a nonoxide group (LiF) by an oxide group (ZnO). Urbach tail energy, EU, was found to increase from x = 0 to x = 15 and then decreased slightly for x = 20}. Theoretical optical basicity, Lambdath, decreased with decrease in concentration of LiF.

Özet

Zinc fluoroborate glasses with compositions xZnO.(40 - x) LiF.60B2O3 (x = 0, 5, 10, 15, and 20) were synthesized by the melt-quench method. The amorphous nature of the glassy samples was confirmed by XRD analysis. The nature of the bonds formed and the role of various species in the composition of the glasses were examined using FTIR spectroscopy. FTIR analysis showed shifting of an absorption band with the addition of ZnO. A UV-visible study was carried out to calculate the optical band gap energy, EgIt was found that Egdecreased with increase in concentration of ZnO up to x = 15 and increased slightly for x 20 with the stepwise replacement of a nonoxide group (LiF) by an oxide group (ZnO). Urbach tail energy, EU, was found to increase from x = 0 to x = 15 and then decreased slightly for x = 20}. Theoretical optical basicity, Lambdath, decreased with decrease in concentration of LiF.

🔖

Cite This Article

ARORA, S., KUNDU, V., GOYAL, D. R., MAAN, A. S. (2013). Effect of stepwise replacement of LiF by ZnO on structural and optical properties of LiF.B2O3 glasses. Turkish Journal of Physics, Cilt: 37 - Sayı: 2, 229–236. https://ajindex.com/articles/724004

📄 Full Text PDF Viewer

📄

PDF görüntüleyici hazırlanıyor...

References (5)

  1. V. R. Kumar, B. Apparao and N. Veeraiah, Bull. Mater. Sci., 21, (1998), 341. I. Z. Hager, J. Phys. Chem. Solids, 70, (2009), 210. S. Arora, V. Kundu, D. R. Goyal, and A. S. Maan, ISRN Spectroscopy, 2012, (2012), 896492(1-5).
  2. S. Arora, V. Kundu, D. R. Goyal, and A. S. Maan, ISRN Optics, 2012, (2012), 193185(1-7).
  3. A. Sasaki, W. Hara, A. Matsuda, N. Tateda, S. Otaka, S. Akiba, K. Saito, T. Yodo, M. Yoshimoto, Appl. Phys. Lett,. 86, (2005), 231911.
  4. S. Fujihara, C. Sasaki and T. Kimura, Key Eng. Mater., 181, (2000), 109. L. Baja, R. Stefan, W. Kiefer and S. Simon, J. Raman Spectrosc., 36, (2005), 262. P. Pa¸scut¸˘ a, M. Bo¸sca, S. Rada, M. Culea, I. Bratu and E. Culea, J. Optoelectron. Adv. M., 10, (2008), 2416. V. Kundu, R. L. Dhiman, D. R. Goyal and A. S. Maan, J. Optoelectron. Adv. M., 10, (2008), 2765. E. I. Kamitsos, M. A. Karakassides and G. D. Chryssikos, J. Phys. Chem., 91, (1987), 1073. C. Feifei, D. Shixun, N. Qiuhua, X. Tiefeng, S. Xiang and W. Xunsi, J. Wuhan University of Tech.-Mater. Sci., 24, (2009), 716. I. Ardelean and S. Cora, J Mater Sci. - Mater Electron, 19, (2008), 584. J. N. Ayuni, M. K. Halimah, Z. A. Talib, H. A. A. Sidek, W. M. Daud, A. W. Zaidan and A. M. Khamirul, IOP Conference Series: Materials Science and Engineering, 17, (2001), 012027.
  5. E. A. Devis and N. F. Mott, Phil. Magn., 22, (1970), 903. F. Urbach, Phys. Rev., 92, (1953), 1324. A. A. Kutub, A. E. Mohamed-Osman, and C. A. Hogarth, J. Mater. Sci. 21, (1986), 3517. C. Dayanand, G. Bhikshamaiah, and M. Salagram, Mater. Lett., 23, (1995), 309. K. L. Chopra and S. K. Bahl, Thin Solid Films, 11, (1972), 377. J. A. Duffy and M. D. Ingram, J. Inorg. Nucl. Chem., 37, (1975), 1203.