Journals / Turkish Journal of Chemistry / 2016 / Cilt: 40 - Sayı: 2

Investigation of long-term water absorption behavior of carbon fabric reinforcedepoxy composites containing hydrophobic nanosilica

Pages
321–331
Publication Date
2022-11-03
DOI
—
🏛️Bibliographic metadata and full text access for this article are provided via DergiPark.
DergiPark Record ↗
✨

AI Summary & Key Takeaways

AI Insight
⚡ TL;DR(Too Long; Didn't Read)

The results revealed that ller addition lowers the damage created by distilled water a considerableamount and addition of hydrophobic llers to epoxy matrix composites can be especially bene cial for applicationswhere long-term water exposure is desired.

📌 3 Key Takeaways

🎯
Objective & Hypothesis:The effect of water absorption on the chemical and mechanical properties of hydrophobic ller containingepoxy matrix composites was investigated by keeping them in distilled water for 9 months.
📊
Key Findings & Data:Aerosil R812 (8 nm) andAerosil R972 (12 nm) were utilized at 3% and 5% w/w ller to resin ratio and the resin/ ller mixture was combined with12-ply carbon fabric to get 15 15 cm samples.
💡
Conclusion & Impact:The results revealed that ller addition lowers the damage created by distilled water a considerableamount and addition of hydrophobic llers to epoxy matrix composites can be especially bene cial for applicationswhere long-term water exposure is desired.
🔬Design:Research Article
📍Scope:Comprehensive Sample
⚙️Variables:Domain Parameters

Abstract

The effect of water absorption on the chemical and mechanical properties of hydrophobic ller containingepoxy matrix composites was investigated by keeping them in distilled water for 9 months. Aerosil R812 (8 nm) andAerosil R972 (12 nm) were utilized at 3% and 5% w/w ller to resin ratio and the resin/ ller mixture was combined with12-ply carbon fabric to get 15 15 cm samples. Samples were molded under a hot press and for each sample 50 testsamples obtained by cutting them with a water jet. The obtained samples were characterized by TG, FTIR, and SEM.The effect of water absorption was evaluated by measuring percentage water absorption and exural strength of samplesover 9 months. The results revealed that ller addition lowers the damage created by distilled water a considerableamount and addition of hydrophobic llers to epoxy matrix composites can be especially bene cial for applicationswhere long-term water exposure is desired.

🔖

Cite This Article

İÇDUYGU, M. G., GÜLTEK, A., EKİN, N. (2022). Investigation of long-term water absorption behavior of carbon fabric reinforcedepoxy composites containing hydrophobic nanosilica. Turkish Journal of Chemistry, Cilt: 40 - Sayı: 2, 321–331. https://ajindex.com/articles/602012

📄 Full Text PDF Viewer

📄

PDF görüntüleyici hazırlanıyor...

References (1)

  1. Bai, J.Advanced Fibre-Reinforced Polymer (FRP) Composites for Structural Applications; Woodhead Publishing:Oxford, UK, 2013. 2.Roderick, H. M.Composite Materials: Fatigue and Fracture; American Society for Testing and Materials: WestConshohocken, PA, USA, 1995. 3.Robinson, P.; Greenhalgh, E. S.; Pinho, S.Failure Mechanisms in Polymer Matrix Composites: Criteria, Testingand Industrial Applications; Woodhead Publishing: Oxford, UK, 2012. 4.Thompson, D. O.; Chimenti, D. E.Review of Progress in Quantitative Nondestructive Evaluation; Plenum Press:New York, NY, USA, 1991. 5.Tomoko, S.; Srivatsan, T. S.Advanced Composites for Aerospace, Marine, and Land Applications II; John Willey& Sons, Inc.: Hoboken, NJ, USA, 2015. 6.Hong, S. C.Abrasion Resistant Coatings.United States Patent Application 20100249295, 2010. 7.Ramamoorthi, R.; Sampath, P.S.International Journal of ChemTech Research2015,8, 52-57. 8.Ahmed, Z.; Ansell, M. P.; Smedley, D.IOP Conf. Series: Materials Science and Engineering2011,17, 1-15. 9.Dinh Van Chau, A.Journal of Applied Science2012,12, 1939-1945. 10.Chow, W. S.eXPRESS Polymer Letters2007,1, 104-108. 11.Kalil, A.International Journal of Application or Innovation in Engineering & Management2013,2, 131-136. 12.Hardinnawirda, K.; Aisha, I. S.Journal of Mechanical Engineering and Sciences2012,2, 181-186. 13.Ashbee, K. H. G.; Wyatt, R. C.Proc. Roy. Soc. A1969,312, 553-564. 14.Ashbee, K. H. G.; Frank, F. C.; Wyatt, R. C.Proc. Roy. Soc. A1967,300, 415-419. 15.Castaing, Ph.; Lemoine, L.Polym. Composite.1995,16, 349-356. 16.Schutte, C. L.Mater. Sci. Eng.1994,13, 265-324. 17.Chu, W.; Wu, L.; Karbhari, V. M.J. Appl. Polym. Sci.2006,99, 1405-1414. 18.Strait, L. H.; Karasek, M. L.; Amateau, M. F.J. Compos. Mater.1992,26, 2118-2133. 19.Kinlock, A. J.Structural Adhesives: Developments in Resins and Primers; Elsevier Applied Science Publishers:London, UK, 1986. 20.Karbhari, V. M.Journal of Composites for Construction2004, 148-156. 21.Suh, D.; Ku, M.; Nam, J.; Kim, B.; Yoon, S.J. Compos. Mater.2001,35, 264-278. 22.Swei, G. S.; Rushkin, I. L.; House, D. W.; Czubarow, P. Patent 0224366, 2008. 23.Girase, R.; Jaiswal, R.; Chaudhari, L.; Bhattacharya, S.; D'Melo, D.J. Vinyl Addit. Techn.2012,18, 46-51. 24.Curtis, A. R.; Shortall, A. C.; Marquis, P. M.; Palin, W. M.J. Dent.2008,36, 186-193. 25.Kontou, E.; Georgiopoulos, P.; Niaounakis, M.Polym. Composite.2012,33, 282-294. 26.Markos, J.Mass Transfer in Chemical Engineering Processes; InTech: Rijeak, Croatia, 2011. 27.