Journals / Bilimsel Madencilik Dergisi / 1987 / Cilt: 26 - Sayı: 3

Investigation of Flotation Possibilities of The Jig and First Flotation Tailings of The Balikesir-Balya Lead Mine's Old Processing Plant

Balıkesir-Balya Kurşun-Çinko Sahasındaki Jig ve Birinci Flotasyon Artıklarının Teknolojik Değerlendirilmesi

Pages
5–13
Publication Date
1987-09-01
DOI
—
🏛️Bibliographic metadata and full text access for this article are provided via DergiPark.
DergiPark Record ↗
✨

AI Summary & Key Takeaways

AI Insight
⚡ TL;DR(Too Long; Didn't Read)

In the flotation tests, the oxide lead minerals were tried to be floated by sulfidizing the surfaces.

📌 3 Key Takeaways

🎯
Objective & Hypothesis:The jig and first flotation tailings of the old processing plant of Balya Lead Mine contain 6.0% Pb, 7.0% Zn and 10.5% Fe, and 7.05% Pb, 9.7% Zn and 12.8% respectively.
📊
Key Findings & Data:In the laboratory studies, flotation tests were performed to float Pb and Zn selectively on the one hand and on the other hand, the adequate flotation canditions to obtain a bulk Pb and Zn concentrate were also investigated.
💡
Conclusion & Impact:In the flotation tests, the oxide lead minerals were tried to be floated by sulfidizing the surfaces.
🔬Design:Research Article
📍Scope:Comprehensive Sample
⚙️Variables:Domain Parameters

Abstract

The jig and first flotation tailings of the old processing plant of Balya Lead Mine contain 6.0% Pb, 7.0% Zn and 10.5% Fe, and 7.05% Pb, 9.7% Zn and 12.8% respectively. The main valuable minerals found in both tailings are galena, sphalerite and pyrite as sulfide minerals; lead oxide, carbonate and sulphate, and zinc oxide as oxide minerals. In the laboratory studies, flotation tests were performed to float Pb and Zn selectively on the one hand and on the other hand, the adequate flotation canditions to obtain a bulk Pb and Zn concentrate were also investigated. In the flotation tests, the oxide lead minerals were tried to be floated by sulfidizing the surfaces.

Özet

Balya Kurşun Sahası'nda bulunan eski işletme artıklarından jig artıkları % 6.0 Pb, % 7.0 Zn ve % 103 Fe, birinci flotasyon artıkları ise % 7.05 Pb, % 9.7 Zn ve % 12.8 Fe içermektedir. Artıklarda genel olarak sülfiirlü minerallerden galen, sfalerit ve pirit, oksitli minerallerden kurşun oksit, karbonat ve sülfatlar ile çinko oksitler bulunmaktadır. Değerlendirme çalışmalarında öncelikle seçimli kurşun ve çinko yüzdürmesi üzerinde durulmuş, bunun yanında uygun toplu yüzdürme koşulları da araştırılmıştır. Ayrı­ ca oksitli kurşun mineralleri sülfürlenerek kazanılmaya çalışılmıştır.

🔖

Cite This Article

UÇURUM, M., ULU, E. (1987). Investigation of Flotation Possibilities of The Jig and First Flotation Tailings of The Balikesir-Balya Lead Mine's Old Processing Plant. Bilimsel Madencilik Dergisi, Cilt: 26 - Sayı: 3, 5–13. https://ajindex.com/articles/58999

📄 Full Text PDF Viewer

📄

PDF görüntüleyici hazırlanıyor...