Journals / Research on Engineering Structures and Materials / 2022 / Cilt: 8 - Sayı: 2

The freeze-thaw durability of concrete containing the rubber aggregate of tire waste

Pages
253–264
Publication Date
2022-10-19
DOI
—
🏛️Bibliographic metadata and full text access for this article are provided via DergiPark.
DergiPark Record ↗
✨

AI Summary & Key Takeaways

AI Insight
⚡ TL;DR(Too Long; Didn't Read)

Our results indicate that the inclusion of RATW increasing entrappedair and the interfacial transition zone (ITZ) between cement matrix - rubber is weak and porous.

📌 3 Key Takeaways

🎯
Objective & Hypothesis:The influence of rubber aggregate of tire waste (RATW) under cyclic freezethaw attack of concrete was studied.
📊
Key Findings & Data:Various concrete mixes were prepared: a plain concrete (PC) produced with natural sand and rubber concretes (CRATW) included the RATW ratios of 5, 10, and 15 % such as a partial replacement with the natural sand aggregate (NSA).
💡
Conclusion & Impact:Our results indicate that the inclusion of RATW increasing entrappedair and the interfacial transition zone (ITZ) between cement matrix - rubber is weak and porous.
🔬Design:Research Article
📍Scope:Comprehensive Sample
⚙️Variables:Domain Parameters

Abstract

The influence of rubber aggregate of tire waste (RATW) under cyclic freezethaw attack of concrete was studied. Various concrete mixes were prepared: a plain concrete (PC) produced with natural sand and rubber concretes (CRATW) included the RATW ratios of 5, 10, and 15 % such as a partial replacement with the natural sand aggregate (NSA). After the samples exposed to the different freeze-thaw cycles (120, 240, 340), their following properties were evaluated: visual observations, mass loss, dynamic modulus of elasticity and compressive strength. Our results indicate that the inclusion of RATW increasing entrappedair and the interfacial transition zone (ITZ) between cement matrix - rubber is weak and porous. In addition, the rubber concretes have higher resistance to freeze-thaw attack compared to plain concrete. This innovative trend could be extending the concrete structures’ life in a cold climate. This clean practice of reusing RATW with cement based materials will reduce their stock in the landfills and eliminates their pollution on the environment.

🔖

Cite This Article

GUELMINE, L. (2022). The freeze-thaw durability of concrete containing the rubber aggregate of tire waste. Research on Engineering Structures and Materials, Cilt: 8 - Sayı: 2, 253–264. https://ajindex.com/articles/588818

📄 Full Text PDF Viewer

📄

PDF görüntüleyici hazırlanıyor...

References (11)

  1. Rashad MA. Comprehensive overview about recycling rubber as fine aggregate replacement in traditional cementitious materials. Int. J. Sustainable Built Environ, June 2016; 5: 46-82.
  2. Arunkumar K, Muthukannan M, Suresh Kumar A, Chithambar Ganesh A. Mitigation of waste rubber tire and waste wood ash by the production of rubberized low calcium waste wood ash based geopolymer concrete and influence of waste rubber fibre in setting properties and mechanical behavior. Environmental Research, March 2021; 194: 110661.
  3. Arunkumar K, Muthukannan M, Suresh kumar A, Chithambar Ganesh A, Kanniga Devi R. Hybrid fibre reinforced eco-friendly geopolymer concrete made with waste wood ash: A mechanical characterization study. Engineering and Applied Science Research, 2022; 49: 235-247.
  4. Arunkumar K, Muthukannan M, Suresh kumar A, Chithambar Ganesh A, Kanniga Devi R. Mechanical and durability characterization of hybrid fibre reinforced green geopolymer concrete. Research on Engineering Structures and Materials.
  5. Yuan W, Yang R, Yu J, Zhou S,Cui S, Kang J, Yao Z. Preparation and Propertiers Study of Cementitious Grouts Containing Crumb Rubber. Building, 2021; 11: 555.
  6. Li Q, Xu F, Zheng H, Shi J, Zhang J. Experimental Study on Freeze –thaw Effects on Greep Characteristics of Rubber Concrete. Advances in Materials Sciences and Enginneering, 2022:1-14.
  7. Alsaif A,Bernal SA, Guadagnini M, Pilakoutas K. Durability of steel fibre reinforced rubberised concrete exposed to chlorides, Constr. Build. Mater,10 November 2018; 188: 130–142.
  8. Pigeon M, Marchand J, Pleau R. Frost resistant concrete, Cons. Build. Mater, July 1996; 10: 339 –348.
  9. Alsaif A, Bernal SA, Guadagnini M, Pilakoutas K. Freeze-thaw resistance of steel fibre reinforced rubberised concrete. Constr. Build. Mater, 20 January 2019; 95: 450–458.
  10. Pedro D, de Brito J, Veiga R. Mortars made with fine granulates from shredded tires, J. Mater. Civ. Eng. ASCE, April 2013; 25: 519– 529.
  11. Guelmine L, Hadjab H, Benazzouk A. Effect of elevated temperature