Feldspar Production from Bursa-Orhaneli Syenites

BURSA-ORHANELİ SİYENİTLERİNDEN FELDİSPAT ÜRETİMİ

Pages
17–28
Publication Date
2004-12-01
DOI
—
🏛️Bibliographic metadata and full text access for this article are provided via DergiPark.
DergiPark Record ↗
✨

AI Summary & Key Takeaways

AI Insight
⚡ TL;DR(Too Long; Didn't Read)

Although the concentrate provides white firing color, due to the removal of 43.37% of the feed as tails and K20:Na20 ratio being low (i.e., 1.77), an investment on a beneficiation plant for Bursa-Orhaneli syenites can be stated as "risky" in terms of today's market conditions.

📌 3 Key Takeaways

🎯
Objective & Hypothesis:In this study, the possibility of obtaining high quality feldspar concentrate from syenite samples of Bursa-Orhaneli district is investigated.
📊
Key Findings & Data:Following the mineralogical characterization, the sample is subjected to high intensity dry magnetic separation at -300|j.m; high intensity wet magnetic separation at -212, -106 and -74jim; flotation at -106 and -74)o,m; flotation+wet magnetic separation at -106 and - 74(j,m for the removal of coloring impurities.
💡
Conclusion & Impact:Although the concentrate provides white firing color, due to the removal of 43.37% of the feed as tails and K20:Na20 ratio being low (i.e., 1.77), an investment on a beneficiation plant for Bursa-Orhaneli syenites can be stated as "risky" in terms of today's market conditions.
🔬Design:Research Article
📍Scope:Comprehensive Sample
⚙️Variables:Siyenit · Feldispat · Manyetik Ayırma

Abstract

In this study, the possibility of obtaining high quality feldspar concentrate from syenite samples of Bursa-Orhaneli district is investigated. Following the mineralogical characterization, the sample is subjected to high intensity dry magnetic separation at -300|j.m; high intensity wet magnetic separation at -212, -106 and -74jim; flotation at -106 and -74)o,m; flotation+wet magnetic separation at -106 and - 74(j,m for the removal of coloring impurities. The best results are obtained by flotation followed by high intensity wet magnetic separation of -106 (im size fraction. Although the concentrate provides white firing color, due to the removal of 43.37% of the feed as tails and K20:Na20 ratio being low (i.e., 1.77), an investment on a beneficiation plant for Bursa-Orhaneli syenites can be stated as "risky" in terms of today's market conditions.

Özet

Bu çalışmada, Bursa-Orhaneli bölgesinden alınan siyenit numunelerinden kaliteli feldispat konsantresi elde edilebilirliği araştırılmıştır. Numunenin mineralojik karakterizasyonunun ardından, renk verici safsızlıkların ayrılması amacıyla, -300^m tane boyutunda yüksek alan şiddetli kuru manyetik ayırma; - 212, -106 ve -74p,m tane boyutlarında yüksek alan şiddetli yaş manyetik ayırma; -106 ve -74(xm tane boyutlarında flotasyon; -106 ve -74 um tane boyutlarında flotasyon + yaş manyetik ayırma testleri uygulanmıştır. En iyi sonuçlar -106 |im tane boyutunda flotasyon ve flotasyon konsantresinin yüksek alan şiddetli yaş manyetik ayırıcıdan geçirilmesi ile elde edilmektedir. Elde edilen konsantrenin beyaz pişme rengi vermesine karşın, malzemenin toplam %43,37'sinin atılması ve elde edilen konsantre K20:Na20 oranının 1,77 gibi görece düşük değerlerde kalması nedenleriyle söz konusu cevherin zenginleştirilmesi amacıyla kurulacak bir tesisin günümüz pazar koşullarında "riskli" sayılabilecek bir yatırım olacağı düşünülmektedir.

🔖