Optimization of process parameters of medium carbon steel joints joined by MIG welding using Taguchi method

Pages
17–26
Publication Date
2022-10-12
DOI
—
🏛️Bibliographic metadata and full text access for this article are provided via DergiPark.
DergiPark Record ↗
✨

AI Summary & Key Takeaways

AI Insight
⚡ TL;DR(Too Long; Didn't Read)

The results showed that the highest tensile strength as 597.963 MPa was obtained at groove angle 90ᵒ, current 120 A and voltage 30 V, the lowest tensile strength was obtained as 395.125 MPa.

📌 3 Key Takeaways

🎯
Objective & Hypothesis:In this study, related to getting better obtain to the mechanical properties of medium carbon steel joints joined by MIG welding method using the Taguchi method welding groove were optimized.
📊
Key Findings & Data:Grove angle (60ᵒ, 75ᵒ and 90ᵒ), current (100 A, 110 A and 120 A) and voltage (25 V, 30 V and 35 V) were used as welding parameters.
💡
Conclusion & Impact:The results showed that the highest tensile strength as 597.963 MPa was obtained at groove angle 90ᵒ, current 120 A and voltage 30 V, the lowest tensile strength was obtained as 395.125 MPa.
🔬Design:Research Article
📍Scope:Comprehensive Sample
⚙️Variables:Optimization · Taguchi method · ANOVA

Abstract

In this study, related to getting better obtain to the mechanical properties of medium carbon steel joints joined by MIG welding method using the Taguchi method welding groove were optimized. Grove angle (60ᵒ, 75ᵒ and 90ᵒ), current (100 A, 110 A and 120 A) and voltage (25 V, 30 V and 35 V) were used as welding parameters. The results showed that the highest tensile strength as 597.963 MPa was obtained at groove angle 90ᵒ, current 120 A and voltage 30 V, the lowest tensile strength was obtained as 395.125 MPa. The highest elongation as 11.551% was obtained at groove angle 90ᵒ, current 120 A and voltage 30 V, the lowest elongation was obtained as 8.354%. In addition, it was observed that the changes in current and voltage values significantly affect the tensile strength and elongation values of the joints. According to ANOVA analyses, the most effective parameter on average tensile strength and elongation were determined to be groove angle (62.75% and 75.58%, respectively). Based on S/N ratios, the optimal parameters for average tensile strength and elongation were determined A3B3C2 factors.

🔖

Cite This Article

İŞCAN, B., ADİN, M. Ş. (2022). Optimization of process parameters of medium carbon steel joints joined by MIG welding using Taguchi method. European Mechanical Science, Cilt: 6 - Sayı: 1, 17–26. https://ajindex.com/articles/512366

📄 Full Text PDF Viewer

📄

PDF görüntüleyici hazırlanıyor...

References (14)

  1. Kah, P., Suoranta, R., Martikainen, J., (2013). Advanced gas metal arc welding processes. The International Journal of Advanced Manufacturing Technology, vol. 67, no. 1, pp. 655-674
  2. Kalpakjian, S., Schmid, S.R., (2013). Manufacturing Engineering and Technology, Seventh ed. Pearson Prentice-Hall, Hoboken, NJ, USA
  3. MillerWelds, (2014). Welding Process Training Series: Introduction to Welding. Miller Electric Mfg. Co., Appleton, Wisconsin, USA
  4. Ramarao, M., King, M.F.L., Sivakumar, A., Manikandan, V., Vijayakumar, M., Subbiah, R., (2021). Optimizing GMAW parameters to achieve high impact strength of the dissimilar weld joints using Taguchi approach. Materials Today: Proceedings, pp. 1-6
  5. Cary, H.B., Helzer, S.C., (2005). Modern welding technology, 6th ed. Pearson Prentice-Hall, Upper Saddle River, New Jersey, Ohio, USA
  6. Kou, S., (2003). Welding metallurgy 2nd edition ed. A John Wiley & Sons Inc., New Jersey, USA
  7. Althouse, A.D., Turnquist, C.H., Bowditch, W.A., Bowditch, K.E., Bowditch, M.A., (2020). Modern welding, 12th ed. The Goodheart-Wilcox Company, Inc
  8. Jeffus, L., (2020). Welding: principles and applications, 9th ed. Cengage, 200 Pier 4 Boulevard Boston, MA, USA
  9. Kishore, K., Krishna, P.G., Veladri, K., Ali, S.Q., (2010). Analysis of defects in gas shielded arc welding of AISI1040 steel using Taguchi method. ARPN Journal of Engineering and Applied Sciences, vol. 5, no. 1, pp. 37-41
  10. Patel, R.B.P.D.B., Patel, T.M., (2013). A Review on Experimental Investigation of GMAW for AISI 1045 by using Taguchi Method. International Journal for Scientific Research & Development, vol. 1, pp. 1679-1682
  11. Wang, D., Yao, D., Gao, Z., Wang, Q., Zhang, Z., Li, X., (2021). Fatigue mechanism of medium-carbon steel welded joint: Competitive impacts of various defects. International Journal of Fatigue, p. 106363
  12. Pal, A., (2015). MIG welding parametric optimisation using taguchi's orthogonal array and analysis of variance. International Journal of Research Review in Engineering Science & technology vol. 4, no. 1, pp. 211-217
  13. Utkarsh, S., Neel, P., Mahajan, M.T., Jignesh, P., Prajapati, R., (2014). Experimental investigation of MIG welding for ST-37 using design of experiment. International Journal of Scientific and Research Publications, vol. 4, no. 5, pp. 402-405
  14. Narwadkar, A., Bhosle, S., (2016). Optimization of MIG welding parameters to control the angular distortion in Fe410WA steel. Materials and Manufacturi