⚡ TL;DR(Too Long; Didn't Read)

The highest strength and fullness properties were found to be achieved in the samples which were processed with the combination of 15 % hydrolysate and 6 % oxazolidine.

📌 3 Key Takeaways

🎯
Objective & Hypothesis:In this study, it is aimed to find out usability of collagen hydrolysate along with oxazolidine in retanning process to achieve an enhanced over all strength and fullness properties of leathers and to reuse hazardous chromed shaving wastes from leather industry as well.
📊
Key Findings & Data:Strength and fullness properties of leathers were evaluated after applying varying ratios of collagen hydrolysates (7.5 -10.0-12.5-15.0 %) along with oxazolidines (4-6 -8%).
💡
Conclusion & Impact:The highest strength and fullness properties were found to be achieved in the samples which were processed with the combination of 15 % hydrolysate and 6 % oxazolidine.
🔬Design:Research Article
📍Scope:Comprehensive Sample
⚙️Variables:Domain Parameters

Abstract

In this study, it is aimed to find out usability of collagen hydrolysate along with oxazolidine in retanning process to achieve an enhanced over all strength and fullness properties of leathers and to reuse hazardous chromed shaving wastes from leather industry as well. Those wastes were hydrolyzed with commercial enzyme preparation in an alkali medium. This collagen hydrolysate was used along with oxazolidine in retanning process. Strength and fullness properties of leathers were evaluated after applying varying ratios of collagen hydrolysates (7.5 -10.0-12.5-15.0 %) along with oxazolidines (4-6 -8%). As a result it is determined that all applied combinations had enhanced expected properties of leather. The highest strength and fullness properties were found to be achieved in the samples which were processed with the combination of 15 % hydrolysate and 6 % oxazolidine.

Özet

Bu projede, derilerin dayanım ve dolgunluk özelliklerini geliştirmek için retenaj prosesinde kollagen hidrolizatı ile oksazolidinin birlikte kullanım ve deri endüstrisinin zararlı tıraş atıklarını değerlendirme olanakları araştırılmıştır. Bu atıklar, alkali bir ortamda ticari bir enzim preperatı ile hidrolize edilmiştir. Elde edilen kollagen hidrolizat, oksazolidin ile birlikte retenaj işleminde kullanılmıştır. Farklı oranlarda uygulanan kollagen hidrolizatı (% 7.5, 10.0, 12.5 ve 15.0) ile oksazolidinin (% 4.0, 6.0 ve 8.0) deriye verdiği dayanım ve dolgunluk özellikleri tespit edilmiştir. Sonuçta, uygulanan tüm kombinasyonların deride istenilen özellikleri geliştirdiği saptanmıştır. En iyi değerler ise % 15 hidrolizat ve%6 oksazolidin kullanılması ile elde edilmiştir.

🔖

Cite This Article

OCAK, B., AFŞAR, A., ASLAN, A., GÜLÜMSER, G. (2022). Kollagen hidrolizatları ile oksazolidinin deri işletisinde birlikte kullanılabilirliği üzerine bir araştırma. DERİ BİLİM, Cilt: 5 - Sayı: 2, 9–14. https://ajindex.com/articles/487170

📄 Full Text PDF Viewer

📄

PDF görüntüleyici hazırlanıyor...

References (1)

  1. A. Püntener, "The Ecological Challenge of Producing Leather", J. Am. Leather Chem. Soc., 90, pp. 206-219, 1995. 2. B. Buljan, G. Reich, J. Ludwig, "Mass Balance in Leather Processing", World Leather, 12, pp. 34-46, 1999. 3. M.M. Taylor, E.J. Diefendorf, C.J. Thompson, E.M. Brown, W.N. Marmer, L.F. Cabeza, "Extraction of Value by Products from the Treatment of Chromium Containing Collagenous Leather Industry Waste", J. Soc. Leather Technol. Chem., 81, pp. 5-13, 1997. 4. V.J. Sundar, J.R. Rao, C. Muradlidharan,, "Cleaner Chrome Tanning-Emerging Options", J. Clean Prod, 10, pp. 69-74,2002. 5. M.M. Taylor, E.J. Diefendorf, G.C. Na, "Enzymic Treatment of Chrome Shavings", J. Am. Leather Chem. Assoc., 85, pp. 264-275, 1990. 6. Z. Bajza, V. Vrcek, 'Thermal and Enzymatic Recovering of Proteins from Untanned Leather Waste", Waste Management, 21, pp. 79-84, 2001. 7. K. Kolomaznik, F. Lanmaier, M. Mladek, M. Taylor, "Industrial Treatment of Chrome Tanned Solid Waste", International Union of Leather Technologists and Chemists Societies Centenary Congress, London. 238 p., 1997. 8. V. Trandafir, T.M. Cioroianu, V. Bratulescu, C. Sarbu, A. Madalina, "Use of Collagen Hydrolysate As Active Biologic Component for Biofertilisiers", Poster presentation, International Union of Leather Technologists and Chemists Societies, XXVIII Congress, Cancun, Mexico, 2003. 9. A. Przepiorkowska, K. Chronska, M. Zaborski, "Chrome-Tanned Leather Shavings as A Filler of Butadiene-Acrylonitrile Rubber", J. Hazard. Mater., 141, pp. 252-257,2007. 10. M. Kishibe, S. Arima, M. Sugita, "Novel Noncatalytic Graft-Copolymerization Methyl Methacrylate onto Collagen", The lllrd Asian International Conference of Leather Science and Technology, Himeji City, Japan, pp. 319-326, 1996. 11.Vdeselnicu. M.D. Bucevschi, M. Colt, "Polymer-Collagen Composite Materials Used in Leather Finishing", Poster Presentation International Union of Leather Technologists and Chemists Societies, XXVI Congress, Cape Town, South Africa, 2001. 12. J. Kanagaraj, K.C. Velappan and N.K.C. Babu, "Solid Wastes Generation in the Leather Industry and Its Utilization for Cleaner Environment-A Review"., Sci. Ind. Res. 65:541-548, 2006. 13. F. Langmaier, P. Mokrejs, K. Kolomaznik, M. Mladek, R. Karnas, "Cross-Linking Epoxide Resins with Hydrolysates of Chrome-Tanned Leather Waste", J. Therm. Anal. Caiorim. 88, pp. 857-862, 2007. 14. J. Kanagaraj, N. Samivelu, A.M.D. Rafiuddun, R. Jayakumar, "High Exhaust Chrome Tanning Using Fleshing Hydr