Effect of tungsten disilicide addition on tungsten boride based composites produced by milling-assisted pressureless sintering

Pages
42–50
Publication Date
2022-10-11
DOI
—
🏛️Bibliographic metadata and full text access for this article are provided via DergiPark.
DergiPark Record ↗
✨

AI Summary & Key Takeaways

AI Insight
⚡ TL;DR(Too Long; Didn't Read)

The results showed that the highest density, microhardness and oxidationstability values amongst the fabricated composites were obtained for the dry milled andsintered WB-20 wt.% WSi2 sample.

📌 3 Key Takeaways

🎯
Objective & Hypothesis:In this study, tungsten boride (WB and W2B) based composites with various amounts oftungsten disilicide (WSi2) addition were fabricated by using a combined method of mechanicalmilling (MM), cold isostatic pressing (CIP) and pressureless sintering (PS).
📊
Key Findings & Data:MMwas conducted for 4 h in ethanol (wet milling) and Argon atmosphere (dry milling) using ahigh-energy ball mill.
💡
Conclusion & Impact:The results showed that the highest density, microhardness and oxidationstability values amongst the fabricated composites were obtained for the dry milled andsintered WB-20 wt.% WSi2 sample.
🔬Design:Research Article
📍Scope:2 sample
⚙️Variables:Domain Parameters

Abstract

In this study, tungsten boride (WB and W2B) based composites with various amounts oftungsten disilicide (WSi2) addition were fabricated by using a combined method of mechanicalmilling (MM), cold isostatic pressing (CIP) and pressureless sintering (PS). MMwas conducted for 4 h in ethanol (wet milling) and Argon atmosphere (dry milling) using ahigh-energy ball mill. WSi2 was used with different amounts (0, 5, 10 and 20 wt.%) in orderto investigate its effect on the resultant products. MM’d powders were compacted usingCIP under a pressure of 450 MPa, and were consecutively sintered at 1600 °C for 2 h and1770 °C for 2 h under Ar atmosphere. Compositional, physical and microstructural characterizationsof the samples were performed using stereo and optical microscopes, X-raydiffractometer, TOPAS software, scanning electron microscope coupled with an energy-dispersivespectrometer, particle size analyzer and gas pycnometer. Sintered products werealso characterized in terms of Archimedes density and Vickers microhardness. Moreover,the oxidation studies of the samples were performed at 500 and 1000 °C via thermogravimetricanalyzer. The results showed that the highest density, microhardness and oxidationstability values amongst the fabricated composites were obtained for the dry milled andsintered WB-20 wt.% WSi2 sample.

🔖

Cite This Article

OVALI, D., AĞAOĞULLARI, D., ÖVEÇOĞLU, M. L., GÖKÇE, H. (2022). Effect of tungsten disilicide addition on tungsten boride based composites produced by milling-assisted pressureless sintering. Bor Dergisi, Cilt: 3 - Sayı: 1, 42–50. https://ajindex.com/articles/467448

📄 Full Text PDF Viewer

📄

PDF görüntüleyici hazırlanıyor...

References (16)

  1. Weimer A. W., ed., Carbide, Nitride and Boride Materials Synthesis and Processing, 1st edition, Chapman & Hall, London, 1996.
  2. Ramberg C. E., Beatrice P., Kurokawa K., Worrell W. K., High temperature oxidation behavior of structural silicides, 21st Annual Cocoa Beach Conference And Exposition on Composites, Advanced Ceramics, Materials and Structures, 12-16 January, 1993.
  3. Suryanarayana C., Mechanical alloying and milling, Prog. Mater. Sci., 46, 1–184, 2001.
  4. Guo S. Q., Densification of ZrB2-based composites and their mechanical and physical properties: A review, J. Eur. Ceram. Soc., 29, 995–1011, 2009.
  5. Murthy T. S. R. C., Sonber J. K., Sairam K., Bedse R. D., Chakarvartty J.K., Development of refractory and rare earth metal borides & carbides for high temperature applications, Mater. Today Proc., 3, 3104–3113, 2016.
  6. Kainer K. U., High temperature ceramic matrix composites, 1st edition, Wiley-VCH Verlag GmbH & Co. KGaA, Weinheim, 2006.
  7. Silvestroni L., Meriggi G., Sciti D., Oxidation behavior of ZrB2 composites doped with various transition metal silicides, Corros. Sci., 83, 281–291, 2014.
  8. Predel B., B-W (Boron-Tungsten), B-Ba–C-Zr, Springer- Verlag, Berlin/Heidelberg, 1992.
  9. Itoh H., Matsudaira T., Naka S., Hamamoto H., Obayashi M., Formation process of tungsten borides by solid state reaction between tungsten and amorphous boron, J. Mater. Sci., 22, 2811–2815, 1987.
  10. Li Q., Zhou D., Zheng W., Ma Y., Chen C., Global structural optimization of tungsten borides, Phys. Rev. Lett., 110, 136-403, 2013.
  11. Kiessling R., The borides of some transition elements, J. Electrochem. Soc., 98 166–170, 1951.
  12. Brewer L., Sawyer D. L., Templeton D. H., Dauben C. H., A study of the refractory borides, J. Am. Ceram. Soc., 34 173–179, 1951.
  13. Barış M., Şimşek T., Gökmeşe H., Akkurt A., Characterization of W2B nanocrystals synthesized by mechanochemical method, J. Boron., 1, 45–51, 2016.
  14. Petrovic J. J., High temperature structural silicides, 21st Annual Cocoa Beach Conference and Exposition on Composites, Advanced Ceramics, Materials and Structures, 12-16 January, 1993.
  15. Murthy T. S. R. C., Sonber J., Subramanian C., Hubli R., Suri A., Densification, characterization and oxidation studies of TiB2–WSi2 composite, Int. J. Refract. Met. Hard Mater., 33, 10–21, 2012.
  16. Silvestroni L., Sciti D., Balat-Pichelin M., Charpentier L., Zirconium carbide doped with tantalum silicide: microstructure, mechanical properties and high temperature oxidation, Mater. Chem. Phys., 143, 407–415, 2013. Sciti D.,