Journals / Bor Dergisi / 2019 / Cilt: 4 - Sayı: 1

Surface modification of anhydrous borax powders with stearic acid via mechanical dry powder coating

Pages
7–15
Publication Date
2022-10-11
DOI
—
🏛️Bibliographic metadata and full text access for this article are provided via DergiPark.
DergiPark Record ↗
✨

AI Summary & Key Takeaways

AI Insight
⚡ TL;DR(Too Long; Didn't Read)

Results indicate that anhydrous borax surface couldbe switched from hydrophilic to hydrophobic with changing contact angle from wetting(17o) to non-wetting (99o).

📌 3 Key Takeaways

🎯
Objective & Hypothesis:Surface modification of anhydrous borax powders with stearic acid in the laboratoryscale planetary ball mill via mechanical dry powder coating approach was investigated.The alteration of hydrophilic surface properties of anhydrous borax with stearic acidwas optimized by modifier amount and activation time.
📊
Key Findings & Data:The cohesion mechanisms ofpowders, which processed at conditions of 0.5, 1 and 2 wt.% stearic acid amount withthe function of 30, 60 and 120 minute activation time, were evaluated in terms of thesolubility test, contact angle measurements, particle size distributions, and scanningelectron microscopy (SEM) analysis.
💡
Conclusion & Impact:Results indicate that anhydrous borax surface couldbe switched from hydrophilic to hydrophobic with changing contact angle from wetting(17o) to non-wetting (99o).
🔬Design:Research Article
📍Scope:Comprehensive Sample
⚙️Variables:Domain Parameters

Abstract

Surface modification of anhydrous borax powders with stearic acid in the laboratoryscale planetary ball mill via mechanical dry powder coating approach was investigated.The alteration of hydrophilic surface properties of anhydrous borax with stearic acidwas optimized by modifier amount and activation time. The cohesion mechanisms ofpowders, which processed at conditions of 0.5, 1 and 2 wt.% stearic acid amount withthe function of 30, 60 and 120 minute activation time, were evaluated in terms of thesolubility test, contact angle measurements, particle size distributions, and scanningelectron microscopy (SEM) analysis. Results indicate that anhydrous borax surface couldbe switched from hydrophilic to hydrophobic with changing contact angle from wetting(17o) to non-wetting (99o). Water-insoluble amount of anhydrous borax powders, as acoating efficiency indicator, was increased from 73% to 91% by coating with 1 wt.%stearic acid for 60 min. Furthermore, SEM analysis results demonstrate that stearic acidwas discretely coated over the anhydrous borax surface. As a conclusion, an effectivemechanical dry coating processing by a one-step coating approach could be applied toobtain a modified anhydrous borax surface, which offers controlled solubility behaviour inwater-based suspensions.

🔖

Cite This Article

Arsoy, Z., Akpınar, S., Şenol, R. S. (2022). Surface modification of anhydrous borax powders with stearic acid via mechanical dry powder coating. Bor Dergisi, Cilt: 4 - Sayı: 1, 7–15. https://ajindex.com/articles/467414

📄 Full Text PDF Viewer

📄

PDF görüntüleyici hazırlanıyor...

References (15)

  1. McMillian P. W., Glass-Ceramics, 2nd Edition, Academic Press, New York, 1979
  2. Kingery W. D., Bowen H. K., Uhlmann, D. R., Introduction to Ceramics, John Wiley and Sons, New York, 1976
  3. Hawthorne F. C., Burns P. C., Grice J. D., The crystal chemistry of boron. In Boron Mineralogy, Petrology and Geology (E. S. Grew and L. M. Anevitz, Eds.), Mineral Society American, MSA Reviews in Mineralogy, 33 (2), 41-116, 1996
  4. Helvaci C. Borates, in Encyclopedia of Geology, (Selley R.C., Cocks, L.R.M and Plimer, I.R., eds.), Elsevier, (3), 510-522, 2005
  5. Kirk-Othmer, Encyclopedia of Chemical Technology, Ch.4, 5th Edition, 241-294, 2004
  6. Akpinar S., Yazici Z.O., Can M.F., Investigation of surface-modified anhydrous borax utilisation in raw glazes, Ceram. Int 44, 18344–18351, 2018 [7] ECETOC Technical Report No. 63, Reproductive and General Toxicology of Some Inorganic Borates and Risks Assessment for Human Beings, European Centre for Ecotoxicology and Toxicology of Chemicals (ECETOC), Brussels, Belgium, 3, 1995
  7. Kaplan J., Zamek J., A substitute for gerstley borate, Ceramics Technical, 32, 24-29, 2011
  8. Otles M. S., Modification of surface properties of biopowders by dry particle coating, Ph.D. Thesis, Université de Toulouse, National Institute of Posts and Telecommunications, Rabat, 2008
  9. Pfeffer R., Dave R. N., Dongguang W., Ramlakhan M., Synthesis of engineered particulates with tailored properties using dry particle coating, Powder Technol., 117, pp.40-67, 2001
  10. Yoshihara I., Pieper W., Hybridization–technology for surface modification of powders without binders, Swiss Pharma 6, 21, 1999
  11. Ouabbas Y., Chamayou A., Galet L., Baron M., Thomas G., Grosseau P., Guilhot B., Surface modification of silica particles by dry coating: Characterization and powder ageing, Powder Technol., 190a, 200-209, 2009
  12. Lefebvre G., Galet L., Chamayou A., Dry coating of talc particles: Effect of material and process modifications on their wettability and dispersibility, AIChE Journal, 57 (1), 79-86, 2011
  13. Sonoda R., Horibe M., Oshima T., Iwasaki T., Watano S., Improvement of dissolution property of poorly water-soluble drug by novel dry coating method using planetary ball mill, Chem. Pharm. Bull. 56 (9),1243-7, 2008
  14. Tsai W. T., Microstructural characterization of calcitebased powder materials prepared by planetary ball milling, Materials, 6, 3361-3372, 2013
  15. Suryanarayana C., Mechanical alloying and milling, Prog. Mater Sci.,