Journals / Tekstil ve Konfeksiyon / 2015 / Cilt: 25 - Sayı: 1

EFFECTS OF SOLVENT MIXTURES ON THE MORPHOLOGY OF ELECTROSPUN THERMOPLASTIC POLYURETHANE NANOFIBRES

ÇÖZGEN KARIŞIMLARININ ELEKTROLİF ÇEKİM YÖNTEMİ İLE ÜRETİLMİŞ TERMOPLASTİK POLİÜRETAN NANOLİFLERİNİN MORFOLOJİSİNE ETKİSİ

Pages
38–46
Publication Date
2015-06-01
DOI
—
🏛️Bibliographic metadata and full text access for this article are provided via DergiPark.
DergiPark Record ↗
✨

AI Summary & Key Takeaways

AI Insight
⚡ TL;DR(Too Long; Didn't Read)

Therefore, diluting TPU solutions with 10 or 20 % of EA had positive effect on electrospun nanofibres

📌 3 Key Takeaways

🎯
Objective & Hypothesis:The effects of solvent mixtures on the electro-spinnability of the thermoplastic polyurethane (TPU) solutions and the morphological appearance of the electrospun thermoplastic polyurethane nanofibres were investigated qualitatively by means of a scanning electron microscope (SEM).
📊
Key Findings & Data:Fibre diameters increased with the increasing THF volume fraction.
💡
Conclusion & Impact:Therefore, diluting TPU solutions with 10 or 20 % of EA had positive effect on electrospun nanofibres
🔬Design:Research Article
📍Scope:Comprehensive Sample
⚙️Variables:Termoplastik poliüretan · elektrolif çekimi · nanolifler

Abstract

The effects of solvent mixtures on the electro-spinnability of the thermoplastic polyurethane (TPU) solutions and the morphological appearance of the electrospun thermoplastic polyurethane nanofibres were investigated qualitatively by means of a scanning electron microscope (SEM). N,N-dimethylformamide (DMF), tetrahydrofuran (THF) and ethylacetate (EA) were used as solvents. TPUDMF/THF and TPU-DMF/EA solutions and the resultant nanofibres were compared to those produced by TPU-DMF system. Fibre diameters increased with the increasing THF volume fraction. At 50/50 and 40/60 DMF/THF mixtures fibres were fused to adjacent fibres and electrospinning is restricted due to low conductivity and low boiling point of the THF, and the high viscosity of the prepared solution. On the other hand, 90/10 and 80/20 DMF/EA solutions led to lower nanofibre diameters. Therefore, diluting TPU solutions with 10 or 20 % of EA had positive effect on electrospun nanofibres

Özet

Termoplastik poliüretan (TPU) çözeltilerinin elektrolif çekim yöntemine göre çekilebilirliklerine ve elde edilen termoplastik poliüretan nanoliflerinin morfolojik görünümlerine çözgen karışımlarının etkileri taramalı electron mikroskopu (SEM) ile nitel olarak incelenmiştir. Çözgen olarak N,N-dimetilformamid (DMF), tetrahidrofuran (THF) ve etilasetat (EA) kullanılmıştır. TPU-DMF/THF ve TPU-DMF/EA çözeltileri ve elde edilen nanolifler, TPU-DMF sistemi ile elde edilen nanolifler ile karşılaştırılmıştır. Lif çapları artan THF hacim oranı ile artmıştır. 50/50 ve 40/60 DMF/THF karışımlarında lifler birbirlerie yapışmıştır ve elektrolif çekimi THF’nin düşük iletkenliği ve kaynama noktası ve hazırlanan çözeltilerin yüksek viskozitelerine bağlı olarak zorlaşmıştır. Diğer taraftan, 90/10 ve 80/20 DMF/EA ile hazırlanan çözeltilerden daha ince lif çapı olan nanolifler elde edilmiştir. Bu nedenle TPU çözeltilerini %10 veya %20 EA ile seyreltmek elektrolif çekim yöntemine gore elde edilen nanolifler üzerine olumlu etki yapmaktadır

🔖

Cite This Article

ÇAY, A., KUMBASAR, E. P. A., AKDUMAN, Ç. (2015). EFFECTS OF SOLVENT MIXTURES ON THE MORPHOLOGY OF ELECTROSPUN THERMOPLASTIC POLYURETHANE NANOFIBRES. Tekstil ve Konfeksiyon, Cilt: 25 - Sayı: 1, 38–46. https://ajindex.com/articles/46198

📄 Full Text PDF Viewer

📄

PDF görüntüleyici hazırlanıyor...

References (13)

  1. Gopa, R., Kaur, S., Maa, Z., Chanc, C., Ramakrishna, S., Matsuura, T., 2006, “Electrospun nanofibrous filtration membrane”, Journal of Membrane Science, 281, 581-586
  2. Qin, X., Wang, S., 2006, “Filtration properties of electrospinning nanofibers”, Journal of Applied Polymer Science, 102, 1285-1290
  3. Yun, K.M., Hogan Jr., C.J., Matsubayashi, Y., Kawabe, M., Iskandar, F., Okuyama, K., 2007, “Nanoparticle filtration by electrospun polymer fibers”, Chemical Engineering Science, 62, 4751-4759
  4. Uyar, T., Havelund, R., Nur, Y., Hacaloglu, J., Besenbacher, F., Kingshott, P., 2009, “Molecular filters based on cyclodextrin functionalized electrospun fibers”, Journal of Membrane Science, 332, 129-137
  5. Chunder, A., Sarkar, S., Yu, Y., Zhai, L., 2007, “Fabrication of ultrathin polyelectrolyte fibers and their controlled release properties”, Colloids and Surfaces B: Biointerfaces, 58, 172-179
  6. Dotti, F., Varesano, A., Montarsolo, A., Aluigi, A., Tonin, C., Mazzuchetti, G., 2007, “Electrospun porous mats for high efficiency filtration”, Journal of Industrial Textiles, 37, 151-162
  7. Qin, X., Wang, S., 2008, “Electrospun nanofibers from crosslinked poly(vinyl alcohol) and its filtration efficiency”, Journal of Applied Polymer Science, 109, 951-956
  8. Sill, T.J., von Recum, H.A., 2008, “Electrospinning: Applications in drug delivery and tissue engineering”, Biomaterials, 29, 1989-2006
  9. Menga, Z.X., Zhenga, W., Lia, L., Zheng, Y.F., 2011, “Fabrication, characterization and in vitro drug release behavior of electrospun PLGA/chitosan nanofibrous scaffold”, Materials Chemistry and Physics, 125, 606-611
  10. Liang, D., Hsiao, B.S., Chu, B., 2007, “Functional electrospun nanofibrous scaffolds for biomedical applications”, Advanced Drug Delivery Reviews, 59, 1392-1412
  11. Verreck, G., Chun, I., Rosenblatt, J., Peeters, J., Dijck A.V., Mensch, J., Noppe, M., Brewster, M.E., 2003, “Incorporation of drugs in an amorphous state into electrospun nanofibers composed of a water-insoluble, nonbiodegradable polymer”, Journal of Controlled Release, 92, 349- 360
  12. Kim, K., Luu, Y.K., Chang, C., Fang, D., Hsiao, B.S., Chu, B., Hadjiargyrou, M., 2004, “Incorporation and controlled release of a hydrophilic antibiotic using poly(lactide-co-glycolide)-based electrospun nanofibrous scaffolds”, Journal of Controlled Release, 98, 47- 56
  13. Kenawy, E., Bowlin, G.L., Mansfield, K., Layman, J., Simpson, D. G., Sanders, E. H., Wnek, G. E., 2002, “Release of tetracycline hydr