Journals / Annals of Medical Research / 2020 / Cilt: 27 - Sayı: 10

Long-term monomer elution from bulk-fill composite resins

Pages
2731–2736
Publication Date
2022-10-12
DOI
—
🏛️Bibliographic metadata and full text access for this article are provided via DergiPark.
DergiPark Record ↗
✨

AI Summary & Key Takeaways

AI Insight
⚡ TL;DR(Too Long; Didn't Read)

At the end of 3 months, a statistically significant increase was observed in the amount of almost all monomers released from bulk-fill composites (P

📌 3 Key Takeaways

🎯
Objective & Hypothesis:Aim: The aim of this study was to investigate the long-term elution of unreacted monomers from bulk-fill composite resins.
📊
Key Findings & Data:Material and Methods: Four different restorative bulk-fill composite resins (Filtek Bulk Fill, 3M ESPE; X-tra fil, VOCO; SonicFill, Kerr; and Tetric EvoCeram Bulk Fill, Ivoclar Vivadent) were used.
💡
Conclusion & Impact:At the end of 3 months, a statistically significant increase was observed in the amount of almost all monomers released from bulk-fill composites (P
🔬Design:Research Article
📍Scope:15 samples
⚙️Variables:Domain Parameters

Abstract

Aim: The aim of this study was to investigate the long-term elution of unreacted monomers from bulk-fill composite resins. Material and Methods: Four different restorative bulk-fill composite resins (Filtek Bulk Fill, 3M ESPE; X-tra fil, VOCO; SonicFill, Kerr; and Tetric EvoCeram Bulk Fill, Ivoclar Vivadent) were used. A total of 15 samples per group (5 x 5 x 4 mm) were polymerized with light as a single layer (4 mm). Then the samples were put into 75/25% ethanol/water mixture. Evaluation of monomer release was performed by using High-Performance Liquid Chromatography device. This process was repeated after one hour, 24 hours, and 3 months. One-way analysis of variance was used to determine the differences in monomer release between groups, while the Tukey HSD test was used for multiple comparisons. The paired sample t-test was used to determine the time-dependent changes of the same material. (P < .05).Results: Monomer release was observed in all groups. At the end of 3 months, a statistically significant increase was observed in the amount of almost all monomers released from bulk-fill composites (P

🔖

Cite This Article

DÜNDAR, A., BARUTCUGİL, Ç., GÜÇLÜER, Ö., BATMAZ, S. G., YILDIRIM, K. (2022). Long-term monomer elution from bulk-fill composite resins. Annals of Medical Research, Cilt: 27 - Sayı: 10, 2731–2736. https://ajindex.com/articles/446088

📄 Full Text PDF Viewer

📄

PDF görüntüleyici hazırlanıyor...

References (16)

  1. Demirci M, Tuncer S, Yuceokur AA. Prevalence of caries on individual tooth surfaces and its distribution by age and gender in university clinic patients. Eur J Dent 2010;4:270-9
  2. Spahl W, Budzikiewicz H, Geurtsen W. Determination of leachable components from four commercial dental composites by gas and liquid chromatography/mass spectrometry. J Dent 1998;26:137-45
  3. Ortengren U, Wellendorf H, Karlsson S, et al. Water sorption and solubility of dental composites and identification of monomers released in an aqueous environment. J Oral Rehabil 2001;28:106-15
  4. Zhu S, Platt J. Curing efficiency of three different curing modes at different distances for four composites. Oper Dent 2011;36:362-71
  5. Ferracane JL. Elution of leachable components from composites. J Oral Rehabil 1994;21:441-52
  6. Ferracane JL. Hygroscopic and hydrolytic effects in dental polymer networks. Dent Mater 2006;22:211-22
  7. Tadin A, Marovic D, Galic N, et al. Composite-induced toxicity in human gingival and pulp fibroblast cells. Acta Odontol Scand 2014;72:304-11
  8. Schweikl H, Schmalz G. Triethylene glycol dimethacrylate induces large deletions in the hprt gene of V79 cells. Mutat Res. 1999;438:71-8
  9. Visalli G, Baluce B, La Maestra S, et al. Genotoxic damage in the oral mucosa cells of subjects carrying restorative dental fillings. Arch Toxicol 2013:87:179- 87
  10. Darmani H, Al-Hiyasat AS. The effects of BIS-GMA and TEG-DMA on female mouse fertility. Dent Mater 2006;22:353-8
  11. Teti G, Mazzotti G, Zago M, et al. HEMA downregulates procollagen alpha1 type I in human gingival fibroblasts. J Biomed Mater Res A 2009;90:256-62
  12. Blomgren J, Axell T, Sandahl O, et al. Adverse reactions in the oral mucosa associated with anterior composite restorations. J Oral Pathol Med 1996;25:311-3
  13. Lai YL, Chen YT, Lee SY, et al. Cytotoxic effects of dental resin liquids on primary gingival fibroblasts and periodontal ligament cells in vitro. J Oral Rehabil 2004;31:1165-72
  14. Cebe MA, Cebe F, Cengiz MF, et al. Elution of monomer from different bulk fill dental composite resins. Dent Mater 2015;31:141-9
  15. Alshali RZ, Salim NA, Sung R, et al. Analysis of longterm monomer elution from bulk-fill and conventional resin-composites using high performance liquid chromatography. Dent Mater 2015;31:1587-98
  16. Mazzaoui SA, Burrow MF, Tyas MJ, et al. Long-term quantification of the release of monomers from dental resin composites and a resin-modified glass ionomer cement. J Biomed Mate