Journals / An International Journal of Optimization and Control: Theories & Applications (IJOCTA) / 2021 / Cilt: 11 - Sayı: 2

Taguchi’s method of optimization of fracture toughness parameters of $Al SiC_p$ composite using compact tension specimens

Pages
152–157
Publication Date
2022-10-11
DOI
—
🏛️Bibliographic metadata and full text access for this article are provided via DergiPark.
DergiPark Record ↗
✨

AI Summary & Key Takeaways

AI Insight
⚡ TL;DR(Too Long; Didn't Read)

From the ANOVAoutcomes it is clear that the composition and a/W ratio of the geometry has moreinfluence on the fracture toughness than the grain size of reinforcement.

📌 3 Key Takeaways

🎯
Objective & Hypothesis:The objective of this work is to investigate the process parameters which influencethe fracture toughness of aluminum-silicon carbide particulate composite preparedusing the stir casting technique.
📊
Key Findings & Data:From the Taguchi’s analysis, on compacttension specimens, aluminum 6061 reinforced with 9 wt% of the silicon carbideparticles composite and a/W ratio of 0.45 are considered to be optimizedparameters.
💡
Conclusion & Impact:From the ANOVAoutcomes it is clear that the composition and a/W ratio of the geometry has moreinfluence on the fracture toughness than the grain size of reinforcement.
🔬Design:Research Article
📍Scope:Comprehensive Sample
⚙️Variables:Domain Parameters

Abstract

The objective of this work is to investigate the process parameters which influencethe fracture toughness of aluminum-silicon carbide particulate composite preparedusing the stir casting technique. The Taguchi’s design of experiments is conductedto analyze the process parameters. Three parameters considered are compositionof material, grain size and a/W ratio. From the Taguchi’s analysis, on compacttension specimens, aluminum 6061 reinforced with 9 wt% of the silicon carbideparticles composite and a/W ratio of 0.45 are considered to be optimizedparameters. Taguchi's technique result shows that the increment in the a/W ratiocauses decrement in the load carrying capacity of the composite. Whereas the finegrain size of silicon carbide have better toughness values. From the ANOVAoutcomes it is clear that the composition and a/W ratio of the geometry has moreinfluence on the fracture toughness than the grain size of reinforcement.

🔖

Cite This Article

GUDDHUR, H., NAGANNA, C., DODDAMANI, S. (2022). Taguchi’s method of optimization of fracture toughness parameters of $Al SiC_p$ composite using compact tension specimens. An International Journal of Optimization and Control: Theories & Applications (IJOCTA), Cilt: 11 - Sayı: 2, 152–157. https://ajindex.com/articles/440545

📄 Full Text PDF Viewer

📄

PDF görüntüleyici hazırlanıyor...

References (1)

  1. Anderson, T.L. (2013). Fracture MechanicsFundamentals and Applications. 3rd Edition, Taylor & Francis Group, New York, [2] Zhu, X.K. Joyce, J.A. (2012). Review of Fracture Toughness (G, K, J, CTOD, CTOA) Testing and Standardization, Engineering Fracture Mechanics, Elsevier, 85, 1–46. [3] ASTM Standards. (2017). Standard Test Method for Plane-Strain Fracture Toughness of Metallic Materials. ASTM International, E 399-17. [4] ASM Handbook. (2001). Composites. 21. ASM International. [5] Alaneme, K.K., Aluko, A.O. (2012). Fracture toughness (K1C) and tensile properties of as-cast and age-hardened aluminium (6063)–silicon carbide particulate composites. Scientia Iranica A, 19(4), 992–996. [6] Doddamani, S., Kaleemulla, M., Begum, Y. (2015). Experimental Investigation on Tensile Properties of Al6061-Graphite Particulate Composites. International Journal of Composite Material and Matrices, 1(2), 1-8. [7] Taj, A., Doddamani, S., Vijaykumar, T.N. (2017). Vibrational Analysis of Aluminium Graphite Metal Matrix Composite, International Journal of Engineering Research & Technology (IJERT), 6(4), 1072-1078. http://dx.doi.org/10.17577/IJERTV6IS040720. [8] Rajesh A M, Mohammed Kaleemulla, Saleemsab Doddamani. (2019). Material characterization of SiC and Al2O3 reinforced hybrid aluminum metal matrix composites on wear behavior”, Advanced Composite Letters, SAGE, 28, 1-10. DOI: 10.1177/0963693519856356. [9] Rajesh, A.M, Kaleemulla, M., Doddamani, S. (2019). Effect of heat treatment on wear behavior of hybrid aluminum metal matrix composites, Tribology in Industry, 41(3), 344-354. DOI: 10.24874/ti.2019.41.03.04. [10] Rajesh, A.M, Kaleemulla, M., Doddamani, S. (2019). Generation of Mechanically Mixed Layer (MML) in Hybrid Aluminum Metal Matrix Composites under As-cast and Age Hardened Conditions. SN Aplied Science, Springer, 1(8). DOI:10.1007/s42452-019-0906-5. [11] Doddamani, S., Kaleemulla, M. (2015). Review of experimental fracture toughness (KIc) of aluminium alloy and aluminium MMCs. International Journal of Fracture and Damage Mechanics, 1(2), 38-51. [12] Doddamani, S., Kaleemulla, M. (2016). Indentation Fracture Toughness of Alumnum6061-Graphite Composites, International Journal of Fracture and Damage Mechanics, 1(1), 40-46. [13] Doddamani, S., Kaleemulla, M. (2017). Experimental investigation on fracture toughness of Al6061–graphite by using Circumferential Notched Tensile Specimens. Frattura ed Integrità Strutturale, 11(39), 274-281. DOI: 10.3221/IGFESIS.39.25.