Journals / Turkish Journal of Engineering and Environmental Sciences / 2010 / Cilt: 34 - Sayı: 4

Production of submicron sized boric acid particles by wet milling

Pages
271–274
DOI
—
🏛️Bibliographic metadata and full text access for this article are provided via DergiPark.
DergiPark Record ↗
✨

AI Summary & Key Takeaways

AI Insight
⚡ TL;DR(Too Long; Didn't Read)

Moreover, it appeared that thermal decomposition temperatures were not size dependent.

📌 3 Key Takeaways

🎯
Objective & Hypothesis:Submicron sized boric acid particles are used in traditional lubrication oils as they provide a low friction coefficient and they are friendly to the environment.
📊
Key Findings & Data:In the present study, size and structure changes in high energy ball wet milled boric acid particles were investigated and characterized by X-ray diffraction (XRD), BET, and thermo-gravimetric/differential thermal analysis (TG-DTA).
💡
Conclusion & Impact:Moreover, it appeared that thermal decomposition temperatures were not size dependent.
🔬Design:Research Article
📍Scope:Comprehensive Sample
⚙️Variables:Boric acid · nanoparticle · wet milling

Abstract

Submicron sized boric acid particles are used in traditional lubrication oils as they provide a low friction coefficient and they are friendly to the environment. In the present study, size and structure changes in high energy ball wet milled boric acid particles were investigated and characterized by X-ray diffraction (XRD), BET, and thermo-gravimetric/differential thermal analysis (TG-DTA). It was seen that increasing time of milling resulted in smaller particle formation and a larger specific surface area. Moreover, it appeared that thermal decomposition temperatures were not size dependent.

Özet

Submicron sized boric acid particles are used in traditional lubrication oils as they provide a low friction coefficient and they are friendly to the environment. In the present study, size and structure changes in high energy ball wet milled boric acid particles were investigated and characterized by X-ray diffraction (XRD), BET, and thermo-gravimetric/differential thermal analysis (TG-DTA). It was seen that increasing time of milling resulted in smaller particle formation and a larger specific surface area. Moreover, it appeared that thermal decomposition temperatures were not size dependent.

🔖

Cite This Article