Journals / Research on Engineering Structures and Materials / 2021 / Cilt: 7 - Sayı: 2

Performance evaluation of geopolymer concrete using E-waste and M-sand

Pages
183–198
DOI
—
🏛️Bibliographic metadata and full text access for this article are provided via DergiPark.
DergiPark Record ↗
✨

AI Summary & Key Takeaways

AI Insight
⚡ TL;DR(Too Long; Didn't Read)

The results of this experimental study very well match with Indian standards of concrete.

📌 3 Key Takeaways

🎯
Objective & Hypothesis:This study has been conducted to diminish the carbon footprint of concrete and to assess the performance of geopolymer concrete by completely replacing river sand with Manufactured sand (M-Sand) and Electronic Waste (E-waste).
📊
Key Findings & Data:The characteristic strength of geopolymer concrete is obtained by completely replacing fine aggregate with E-waste and M-sand with different percentages.
💡
Conclusion & Impact:The results of this experimental study very well match with Indian standards of concrete.
🔬Design:Research Article
📍Scope:Comprehensive Sample
⚙️Variables:Domain Parameters

Özet

This study has been conducted to diminish the carbon footprint of concrete and to assess the performance of geopolymer concrete by completely replacing river sand with Manufactured sand (M-Sand) and Electronic Waste (E-waste). Fly ash and Ground Granulated Blast Furnace Slag (GGBFS) are used in various combinations as a cementitious material in geopolymer concrete. The characteristic strength of geopolymer concrete is obtained by completely replacing fine aggregate with E-waste and M-sand with different percentages. An optimum percentage replacement is arrived at by studying the physical, chemical, and mechanical characteristics. The sizes of the E-waste particles used in this research are between 0.3mm and 0.15 mm and it has a deep colour with a specific gravity of 2.68. Maximum compressive strength of 35.8 N/$mm^2$ on 28 days is achieved for the optimal mix proportion of 80% fly ash, 20% GGBFS, 80% M-sand, and 20% E-waste as fine aggregate. Maximum flexural strength obtained is 6.54 N/$mm^2$ for mix proportion 1 and split tensile strength is 4.75 N/$mm^2$ resulted in mix proportion 2. The use of fly ash, E-waste, and M-sand in geopolymer concrete reduce the environmental pollution and depletion of natural river sand. The results of this experimental study very well match with Indian standards of concrete.

🔖

Cite This Article

PARTHEEBAN, P., KALAIYARRASI, A. R. R., NARAYANAN, L. (2021). Performance evaluation of geopolymer concrete using E-waste and M-sand. Research on Engineering Structures and Materials, Cilt: 7 - Sayı: 2, 183–198. https://ajindex.com/articles/316799

📄 Full Text PDF Viewer

📄

PDF görüntüleyici hazırlanıyor...

References (13)

  1. Dahl R. Who pays for e-junk? Environ Health Perspect. 2002;110:A196-9. [PMCID: PMC1240811] [PubMed: 11940446]
  2. Koehnken L, Rintoul MS, Goichot M, Tickner D, Loftus AC, Acreman MC. Impacts of riverine sand mining on freshwater ecosystems: A review of the scientific evidence and guidance for future research, River Res Applic. 2020;36:362-370.
  3. Davidovits J. Le Livre de la Pierre - Que le Dieu Khnoum Protégé Kheops, Consteur de Pyramide. Saint-Quentin, 1978
  4. Palomo A, Grutzeck MW, Blanco M.T. Alkali-activated fly ashes-A cement for the future. Cement and Concrete Research, 29, 1999, pp. 1323-1329.
  5. Van Jaarsveld, JGS, Van Deventer JSJ, Lukey GC The characterisation of source materials in fly ash-based geopolymers, Materials Letters, 57, 2003, pp. 1272- 1280.
  6. Barbosa, VFF, Mackenzie KJF, Thaumaturgo C. Synthesis and Characterisation of Materials Based on Inorganic Polymers of Alumina and Silica: Sodium Polyciliate Polymers, International Journal of Inorganic Materials, 2(4), 2000, pp. 309-317.
  7. Lenin Sundar M, Raj S, Vadivel M. Experimental Investigation of Geopolymer Concrete with E-Waste, International Journal of Emerging Science and Engineering, 9(3), 2016, pp. 491-496
  8. Basha M, Reddy B, Vasugi K. Research on Strength behaviour of geopolymer concrete replacing fine aggregates by M- sand and E-waste, International Journal of Engineering Research & Technology, 40(7), 2016, pp. 401-407.
  9. Gayathri G, Ramya VS, Yasotha T. Experimental Investigation on Geopolymer Concrete with E-Waste, International Journal of Recent Research and Applied Studies, 8(2), 2016, pp. 280-291
  10. Balasubramanian B, Gopal Krishna GVT, Saraswathy V. Investigation on Partial Replacement of Coarse Aggregate using E-Waste in Concrete, International Journal of Emerging Science and Engineering, 9(3), 2016, pp. 285-288
  11. Kale SP, Pathan HI. Recycling of Demolished Concrete and E-waste, International Journal of Science and Research, 4(1), 2015, pp. 789-792
  12. Krishna Prasanna P, Kanta Rao M. Strength. Variations in Concrete by Using E-Waste as Coarse Aggregate, International Journal of Education and Applied Research, 4(spl2), 2014, pp. 82-84
  13. Kr. Das S, Kr. Mohapatra A, Rath AK. Geo-polymer Concrete