Journals / Politeknik Dergisi / 2018 / Cilt: 21 - Sayı: 4

The Effects of Wood Preservatives on the Combustion Characteristics of Sessile Oak (Quercus Petreae L.)

Pages
805–811
DOI
—
🏛️Bibliographic metadata and full text access for this article are provided via DergiPark.
DergiPark Record ↗
✨

AI Summary & Key Takeaways

AI Insight
⚡ TL;DR(Too Long; Didn't Read)

In CWF stage, the highest temperature was obtained in water-based varnished samples (490 °C), the lowest in non-varnished samples (458 °C); in CWOF stage the highest temperature in water-based varnished samples (572 °C), the lowest in synthetic varnished samples (544 °C); and in ECP stage the highest temperature in non-varnished samples (306.5 °C), the lowest in the samples with the synthetic varnished (262.7 °C).

📌 3 Key Takeaways

🎯
Objective & Hypothesis:This study carried out to determine the combustion properties of the sessile oak wood (Quercus petraea L.) which impregnated with wood preservative and subjected to surface treatments.
📊
Key Findings & Data:For this purpose, the samples, which were prepared from sessile oak wood according to ASTM–E 160-50 combustion principles, impregnated with wolmanit-CB (WC) and tanalith-E (T) in accordance with ASTM-D 1413-76 and then synthetic (St) and Water-based (wb) varnishes were applied according to ASTM-D 3023.
💡
Conclusion & Impact:In CWF stage, the highest temperature was obtained in water-based varnished samples (490 °C), the lowest in non-varnished samples (458 °C); in CWOF stage the highest temperature in water-based varnished samples (572 °C), the lowest in synthetic varnished samples (544 °C); and in ECP stage the highest temperature in non-varnished samples (306.5 °C), the lowest in the samples with the synthetic varnished (262.7 °C).
🔬Design:Research Article
📍Scope:Comprehensive Sample
⚙️Variables:Combustion · wood · impregnation

Abstract

This study carried out to determine the combustion properties of the sessile oak wood (Quercus petraea L.) which impregnated with wood preservative and subjected to surface treatments. For this purpose, the samples, which were prepared from sessile oak wood according to ASTM–E 160-50 combustion principles, impregnated with wolmanit-CB (WC) and tanalith-E (T) in accordance with ASTM-D 1413-76 and then synthetic (St) and Water-based (wb) varnishes were applied according to ASTM-D 3023. The combustion test was carried out in 3 stages, combustion with flame (CWF), self-combustion without flame source (CWOF) and ember combustion stage (ECP). It was aimed to determine the combustion temperature values in CWF, CWOF and ECP stage, weight loss, total combustion time and demolition time. As a result, impregnation applications have increased the total combustion time to between 15-18% and reduced the demolition period. The exact opposite results were obtained for the varnish types, the total combustion time was reduced by 19-21% and the demolition time increased by 10-22%. In CWF stage, the highest temperature was obtained in water-based varnished samples (490 °C), the lowest in non-varnished samples (458 °C); in CWOF stage the highest temperature in water-based varnished samples (572 °C), the lowest in synthetic varnished samples (544 °C); and in ECP stage the highest temperature in non-varnished samples (306.5 °C), the lowest in the samples with the synthetic varnished (262.7 °C).

Özet

This study carried out to determine the combustion properties of the sessile oak wood (Quercus petraea L.) which impregnated with wood preservative and subjected to surface treatments. For this purpose, the samples, which were prepared from sessile oak wood according to ASTM–E 160-50 combustion principles, impregnated with wolmanit-CB (WC) and tanalith-E (T) in accordance with ASTM-D 1413-76 and then synthetic (St) and Water-based (wb) varnishes were applied according to ASTM-D 3023. The combustion test was carried out in 3 stages, combustion with flame (CWF), self-combustion without flame source (CWOF) and ember combustion stage (ECP). It was aimed to determine the combustion temperature values in CWF, CWOF and ECP stage, weight loss, total combustion time and demolition time. As a result, impregnation applications have increased the total combustion time to between 15-18% and reduced the demolition period. The exact opposite results were obtained for the varnish types, the total combustion time was reduced by 19-21% and the demolition time increased by 10-22%. In CWF stage, the highest temperature was obtained in water-based varnished samples (490 °C), the lowest in non-varnished samples (458 °C); in CWOF stage the highest temperature in water-based varnished samples (572 °C), the lowest in synthetic varnished samples (544 °C); and in ECP stage the highest temperature in non-varnished samples (306.5 °C), the lowest in the samples with the synthetic varnished (262.7 °C).

🔖

Cite This Article

YAŞAR, Ş. Ş., ATAR, M. (2018). The Effects of Wood Preservatives on the Combustion Characteristics of Sessile Oak (Quercus Petreae L.). Politeknik Dergisi, Cilt: 21 - Sayı: 4, 805–811. https://ajindex.com/articles/307158

📄 Full Text PDF Viewer

📄

PDF görüntüleyici hazırlanıyor...

References (16)

  1. Archer K. Lebow S., “Wood preservation,” Prim. Wood Process. Princ. Pract., 297–338, (2006)
  2. Keskin H. and Dağlıoğlu N., “Effects of impregnation with Tanalith-E on the compression strength of some woods”, Journal of Polytechnic, 20(3): 711-716, (2017)
  3. Yasar ŞŞ., Fidan MS., Yaşar M., Atar M., Alkan E., “Combustion properties of impregnated spruce ( Picea orientalis L.) wood. Construction and Building Materials, 143: 574–579. https://doi.org/10.1016/j.conbuildmat.2017.03.141, (2017)
  4. Fidan MS., Yaşar ŞŞ., Yaşar M., Atar M., Alkan E., “Characterization of the Combustion Parameters of Impregnated and Varnished Cedar Wood ( Cedrus libani )”, Forest Products Journal, 66(5–6): 290–299, (2016)
  5. Yasar ŞŞ., Fidan MS., Yaşar M., Atar M., “Influences of Seasonal Alterations on The Burning Characteristics of Impregnated and Surface Treated Chestnut (Castanea Sativa Mill) Wood”, Wood Research, 61: 399–412, (2016)
  6. Fidan MS., Yaşar ŞŞ., Yaşar M., Atar M., Alkan E., “Effect of seasonal changes on the combustion characteristics of impregnated cedar (Cedrus libani A. Rich.) wood”. Construction and Building Materials, 106: 711–720, (2016)
  7. Ibach RE., “Biological Properties of Wood” Handb. Wood Chem. Wood Compos., 5: 99–126, (2013)
  8. US EPA, O. (n.d.). "Overview of Wood Preservative Chemicals". website. [Online]: Access, URL: https://www.epa.gov/ingredients-used-pesticide-products/overview-wood-preservative-chemicals, (2017)
  9. Browne F., “Theories of the combustion of wood and its control,” Collections, (2136): 72, (1958)
  10. Ibach R.E., “Biological Properties of Wood”. Handbook of Wood Chemistry and Wood Composites, 5: 99–126, (2013)
  11. McIntyre C.R., Burley J., Evans J., Youngquist J., (Eds.), “Protection from Fire” in Encyclopedia of Forest Science, Academic Press, San Diego, CA, 1283–1288, (2004)
  12. Jiang J., Li J., Gao Q., “Effect of flame retardant treatment on dimensional stability and thermal degradation of wood”. Construction and Building Materials, 75: 74–81, (2015)
  13. Bozkurt A., Göker Y., Erdin N., “Emprenye Tekniği”, Istanbul University,. Faculty of Forestry, 3779/425, 429 s, (1993)
  14. Lee HL., Chen GC., Rowell RM., “Thermal properties of wood reacted with a phosphorus pentoxide–amine system”, J. Appl. Polym. Sci. 91: 2465–2481, (2004)
  15. Lee HL., Chen GC., Rowell RM., “Fungal decay resistance of wood reacted with phosphorus pentoxide–amine system”, Holzforchung 58, 311–315, (2004)
  16. Keskin H., Atar M., Izc