Journals / Bilecik Şeyh Edebali Üniversitesi Fen Bilimleri Dergisi / 2019 / Cilt: 6 - Sayı: 2

Improvement of Surface Properties via an Electroless Ni-B Coating for Commercial Purity Titanium

Ticari Saflıkta Titanyumun Akımsız Ni-B Kaplaması ile Yüzey Özelliklerinin Geliştirilmesi

Pages
99–105
Publication Date
2019-09-30
DOI
—
🏛️Bibliographic metadata and full text access for this article are provided via DergiPark.
DergiPark Record ↗
✨

AI Summary & Key Takeaways

AI Insight
⚡ TL;DR(Too Long; Didn't Read)

The superior wear resistance of Ni-B coating on the CP-Ti is dealt with the combination of its high hardness and self-lubricating property.

📌 3 Key Takeaways

🎯
Objective & Hypothesis:In the present study, the surface of commercial pure titanium (CP-Ti) was coated with electroless Ni–B.
📊
Key Findings & Data:The obtained Ni-B coating demonstrated significantly lower wear rate and stable friction coefficient compared to bare CP-Ti.
💡
Conclusion & Impact:The superior wear resistance of Ni-B coating on the CP-Ti is dealt with the combination of its high hardness and self-lubricating property.
🔬Design:Research Article
📍Scope:Comprehensive Sample
⚙️Variables:Wear resistance · friction · electroless Ni-B

Abstract

In the present study, the surface of commercial pure titanium (CP-Ti) was coated with electroless Ni–B. The surface morphology, microstructure and phase identification were analyzed by Scanning Electron Microscope (SEM) and X-Ray Diffraction (XRD). The obtained Ni-B coating demonstrated significantly lower wear rate and stable friction coefficient compared to bare CP-Ti. The superior wear resistance of Ni-B coating on the CP-Ti is dealt with the combination of its high hardness and self-lubricating property.

Özet

Bu çalışmada, ticari saf titanyumun (CP-Ti) yüzeyi akımsız Ni-B ile kaplandı. Yüzey morfolojisi, mikroyapı ve faz analizi, Taramalı Elektron Mikroskobu (SEM) ve X-Işınları Difraksiyonu (XRD) ile analiz edildi. Elde edilen Ni-B kaplama, işlem görmemiş CP-Ti'ye kıyasla önemli ölçüde daha düşük aşınma hızı ve kararlı sürtünme katsayısı sergilemiştir. CP-Ti yüzeyine oluşturulan Ni-B kaplamanın üstün aşınma direnci sergilemesi, oluşturulan kaplamanın yüksek sertlik ve kendinden yağlama özelliğinden kaynaklanmaktadır.

🔖

Cite This Article

MİNDİVAN, F., MİNDİVAN, H. (2019). Improvement of Surface Properties via an Electroless Ni-B Coating for Commercial Purity Titanium. Bilecik Şeyh Edebali Üniversitesi Fen Bilimleri Dergisi, Cilt: 6 - Sayı: 2, 99–105. https://ajindex.com/articles/251516

📄 Full Text PDF Viewer

📄

PDF görüntüleyici hazırlanıyor...

References (12)

  1. Kazemzadeh-Narbat M., Lai B. F.L., Ding C., Kizhakkedathu J.N., Hancock R. E.W., Wang R. (2013). Multilayered coating on titanium for controlled release of antimicrobial peptides for the prevention of implant-associated infections. Biomaterials, 34, 5969-5977
  2. Caroline R. (2016). Innovative surface treatments of titanium alloys for biomedical applications. Materials Science Forum, 879, 1570-1575
  3. Annamalai V.E., Kavitha S., Ramji S. A. (2014). Enhancing the properties of Ti6Al4V as a biomedical material: a review. The Open Materials Science Journal, 8, 1-17
  4. Revathi A., Magesh S., Balla V.K., Das M., Manivasagam G. (2016). Current advances in enhancement of wear and corrosion resistance of titanium alloys –a review. Materials Technology: Advanced Performance Materials, 1-9
  5. Marques I.S.V., Alfaro M.F., Saito M. T., Saito M.T., Takoudis C., Landers R., Mesquita M.F., Junior F. H. N., Mathew M.T., Sukotjo C., Baraok V. A. R. (2016). Biomimetic coatings enhance tribocorrosion behavior and cell responses of commercially pure titanium surfaces. Biointerphases, 11, 1-14
  6. Zhecheva A., Sha W., Malinov S., Long A. (2005). Enhancing the microstructure and properties of titanium alloys through nitriding and other surface engineering methods. Surface & Coatings Technology, 200, 2192-2207
  7. Stratton P., Graf M. (2009). Thermochemical surface treatment of titanium. International Heat Treatment and Surface Engineering, 3, 26-29
  8. Kikuchi S., Takebe J. (2010). Characterization of the surface deposition on anodized-hydrothermally treated commercially pure titanium after immersion in simulated body fluid. Journal of Prosthodontic Research, 54, 70-77
  9. Richard C., Kowandy C., Landoulsi J., Geetha M., Ramasawmy H. (2010). Corrosion and wear behavior of thermally sprayed nano ceramic coatings on commercially pure Titanium and Ti-13Nb-13Zr substrates. International Journal of Refractory Metals & Hard Materials, 28, 115-123
  10. Ipekci M., Siyahjani F., Cimenoglu H. (2013). Thermochemical nitriding of commercial purity titanium. Defect and Diffusion Forum, 334-335, 117-121
  11. Vora H. D., Rajamure R.S., Dahotre S. N., Ho Y.H., Banerjee R., Dahotre N.B. (2015). Integrated experimental and theoretical approach for corrosion and wear evaluation of laser surface nitrided, Ti-6Al-4V biomaterial in physiological solution. Journal of The Mechanical Behavior of Biomedical Materials, 37, 153-164
  12. Teker D., Muhaffel F., Menekse M., Karaguler N. G.,