Journals / Current Research in Dental Sciences / 2026 / Cilt: 29 Sayı: 3

THE EVALUATION OF BOND STRENGTH BETWEEN DENTAL CERAMIC AND BASE METAL ALLOYS FABRICATED BY CASTING AND LASER SINTERING

Pages
455–460
Publication Date
2019-07-16
🏛️Bibliographic metadata and full text access for this article are provided via DergiPark.
DergiPark Record ↗
✨

AI Summary & Key Takeaways

AI Insight
⚡ TL;DR(Too Long; Didn't Read)

Conclusion: Within the limitations of this study, it can be concluded that laser sintered Co-Cr frameworks establish a strong bond with porcelain.

📌 3 Key Takeaways

🎯
Objective & Hypothesis:Amaç: Bu çalışmanın amacı lazer sinterize Co-Cr ve döküm yöntemi ile elde edilen Ni-Cr ve Co-Cr alaşımlarının porselen ile bağlantısını 3-nokta-bükme testi (3-Point-Bending; 3PB) kullanarak değerlendirmektir.
📊
Key Findings & Data:Gereç-Yöntem: Çalışmada metal altyapı olarak 3 farklı grup kullanılmıştır: lazer sinterize Co-Cr, döküm Co-Cr ve döküm Ni-Cr.
💡
Conclusion & Impact:Conclusion: Within the limitations of this study, it can be concluded that laser sintered Co-Cr frameworks establish a strong bond with porcelain.
🔬Design:Araştırma Makalesi
📍Scope:15 örnek
⚙️Variables:Hızlı Üretim · CAD/CAM · Lazer Sinterleme

Özet

Amaç: Bu çalışmanın amacı lazer sinterize Co-Cr ve döküm yöntemi ile elde edilen Ni-Cr ve Co-Cr alaşımlarının porselen ile bağlantısını 3-nokta-bükme testi (3-Point-Bending; 3PB) kullanarak değerlendirmektir. Gereç-Yöntem: Çalışmada metal altyapı olarak 3 farklı grup kullanılmıştır: lazer sinterize Co-Cr, döküm Co-Cr ve döküm Ni-Cr. Her grup için 15 örnek ISO 9693(1999) standartlarına uygun olarak hazırlanmış ve 3PB testi kullanılarak bağlanma dayanımı değerlendirilmiştir. Veriler ANOVA ve sonrasında Tukey çok yönlü karşılaştırma testi kullanılarak değerlendirilmiştir (α=0,05). Bulgular: Bükülme modülü ve ortalama en yüksek bükme dayanımı değerleri karşılaştırıldığında her iki parametre için 3 grup arasında istatistiksel fark bulunmuştur (P=0,0001). En düşük ortalama bükülme modülü lazer sinterize grupta gözlenirken (77±6,5 GPa), en yüksek değer döküm Co-Cr grubunda (247±16 GPa) görülmüştür. İkili karşılaştırmalarda her 3 grup da birbirinden farklı bulunmuştur. Ortalama bükülme dayanımı değerleri karşılaştırıldığında ise en yüksek dayanım değeri lazer sinterize Co-Cr (87±9 MPa) grubunda bulunurken, döküm Co-Cr grubunun bükülme dayanımı (78±13 MPa) daha düşük olmakla birlikte aradaki farkın istatistiksel açıdan anlamlı olmadığı görülmüştür (P=0,094). Ancak döküm Ni-Cr grubunun ortalama bükülme dayanımı değeri (45±11 MPa) Co-Cr gruplarından anlamlı şekilde daha düşük bulunmuştur (P=0,0001). Sonuç: Bu çalışmanın sınırları dâhilinde lazer sinterize Co-Cr altyapılarının porselen ile güçlü bir bağlantı oluşturduğu sonucuna varılmıştır. Anahtar kelimeler: Hızlı Üretim, CAD/CAM, Lazer Sinterleme, Döküm, Bağlanma Dayanımı THE EVALUATION OF BOND STRENGTH BETWEEN DENTAL CERAMIC AND BASE METAL ALLOYS FABRICATED BY CASTING AND LASER SINTERING Abstract Aim: The aim of this study was to evaluate bond strength of laser sintered Co-Cr and cast Co-Cr and Ni-Cr alloys to porcelain using 3-point-bending test (3PB test). Material and Methods: 3 different metal frameworks were used in the current study: laser sintered Co-Cr, cast Co-Cr and cast Ni-Cr. Fifteen specimens per group were prepared according to ISO 9693 standard (1999) and tested using 3PB test. Results were analyzed using one-way ANOVA followed by Tukey multiple comparison test (α=0,05). Results: Mean bending modulus and flexural bending strength were statistically significantly different among 3 groups (P=0,0001). The lowest mean bending modulus was observed for laser sintered Co-Cr group (77±6,5 GPa) and the highest value was observed for cast Co-Cr group (247±16 GPa). Pairwise comparisons have shown statistically significant differences between all compared groups. When mean bending strength values were compared, the highest value was observed for laser sintered Co-Cr group (87±9 MPa). Although mean flexural strength value of cast Co-Cr group (78±13 MPa) was lower than the laser sintered one, the difference was not statistically significant (P=0,094). However, the mean bending strength of cast Ni-Cr (45±11 MPa) was significantly lower than the Co-Cr groups (P=0,0001). Conclusion: Within the limitations of this study, it can be concluded that laser sintered Co-Cr frameworks establish a strong bond with porcelain. Key Words: Rapid manufacturing, CAD/CAM, Laser Sintering, Casting, Bond Strength

🔖

Cite This Article

Uçar, Y., Koçak, E. F., Ekren, O. (2019). THE EVALUATION OF BOND STRENGTH BETWEEN DENTAL CERAMIC AND BASE METAL ALLOYS FABRICATED BY CASTING AND LASER SINTERING. Current Research in Dental Sciences, Cilt: 29 Sayı: 3, 455–460. https://doi.org/10.17567/ataunidfd.471522

📄 Full Text PDF Viewer

📄

PDF görüntüleyici hazırlanıyor...

References (20)

  1. Naylor PW. Introductıon to metal-ceramic technology, 3 rd ed. Berlin; Quintessence publishing Co Inc; 2017. p. 109.
  2. White SN, Ho L, Caputo AA, Goo E. Strength of porcelain fused to titanium beams. J Prosthet Dent. 1996;75:640-8.
  3. O’Brien WJ. Dental Materials and Their Selection. 4th ed. Chicago; Quintessence Publishing Co Inc; 2008; p. 531.
  4. Anusavice KJ, Shen C, Rawls RH. Phillips’ science of dental materials. 12th ed. St Louis; Elsevier Inc. Saunders; 2013. p. 418-73.
  5. Ucar Y, Aksahin Z, Kurtoglu C. Metal ceramic bond after multiple castings of base metal alloy. J Prosthet Dent. 2009;102:165-71.
  6. Naylor PW. Introductıon to metal-ceramic technology, 3 rd ed. Berlin; Quintessence publishing Co Inc; 2017. p. 18.
  7. Ekren O, Ozkomur A, Ucar Y. Effect of layered manufacturing techniques, alloy powders, and layer thickness on metal-ceramic bond strength. J Prosthet Dent. 2018;119:481-7.
  8. Uçar Y, Aysan Meriç I, Ekren O, Layered Manufacturing of Dental Ceramics: Fracture Mechanics, Microstructure, and Elemental Composition of Lithography-Sintered Ceramic. J Prosthodont. 2018 Feb 11. doi: 10.1111/jopr.12748
  9. Koutsoukis T, Zinelis S, Eliades G, Al-Wazzan K, Rifaiy MA, Al Jabbari YS. Selective Laser Melting Technique of Co-Cr Dental Alloys: A Review of Structure and Properties and Comparative Analysis with Other Available Techniques. J Prosthodont. 2015;24:303-12.
  10. Yıldırım MP, Bayındır F. Protetik diş tedavisinde hızlı prototip üretim teknolojileri Atatürk Üniv. Diş Hek. Fak. Derg 2013;25:430-35
  11. Mazzoli A. Selective laser sintering in biomedical engineering. Med Biol Eng Comput. 2013;51:245-56.
  12. Ren XW, Zeng L, Wei ZM, Xin XZ, Wei B. Effects of multiple firings on metal-ceramic bond strength of Co-Cr alloy fabricated by selective laser melting. J Prosthet Dent. 2016;115:109-14.
  13. Nesse H, Ulstein DM, Vaage MM, Øilo M. Internal and marginal fit of cobalt-chromium fixed dental prostheses fabricated with 3 different techniques. J Prosthet Dent. 2015;114:686-92.
  14. Naylor PW. Introductıon to metal-ceramic technology, 3 rd ed. Berlin; Quintessence publishing Co Inc; 2017. P. 53.
  15. Bae EJ, Kim JH, Kim WC, Kim HY. Bond and fracture strength of metal-ceramic restorations formed by selective laser sintering. J Adv Prosthodont. 2014;6:266-71.
  16. Li J, Chen C, Liao J, Liu L, Ye X, Lin S, Ye J. Bond strengths of porcelain to cobalt-chromium alloys made by casting, milling, and selective laser melting. J Prosthet Dent 2017;118:69-75.
  17. Dimitriadis K, Spyropoulos K, Papadopoulos T. Metal-ceramic bond strength between a feldspathic porcelain and a Co-Cr alloy fabricated with Direct Metal Laser Sintering technique. J Adv Prosthodont 2018;10:25-31.
  18. Kaleli N,Sarac D. Comparison of porcelain bond strength of different metal frameworks prepared by using conventional and recently introduced fabrication methods. J Prosthet Dent 2017;118:76-82.
  19. Akova T, Ucar Y, Tukay A, Balkaya MC, Brantley WA. Comparison of the bond strength of laser-sintered and cast base metal dental alloys to porcelain. Dent Mater 2008;24:1400-4.
  20. HammadIA,TalıcYF. Designs of bond strength tests for metalceramic complexes: review of the literature. J Prosthet Dent. 1996;75:602-8.